| 热等静压对铸态及固溶态第二代镍基单晶高温合金显微缺陷及持久性能的影响 |
和思亮1, 赵云松2, 鲁凡1, 张剑2, 李龙飞1( ), 冯强1 |
1 北京科技大学新金属材料国家重点实验室 北京材料基因工程高精尖创新中心 北京 100083 2 中国航发北京航空材料研究院先进高温结构材料重点实验室 北京 100095 |
|
| Effects of Hot Isostatic Pressure on Microdefects and Stress Rupture Life of Second-Generation Nickel-Based Single Crystal Superalloy in As-Cast and As-Solid-Solution States |
HE Siliang1, ZHAO Yunsong2, LU Fan1, ZHANG Jian2, LI Longfei1( ), FENG Qiang1 |
1 Beijing Innovation Center for Materials Genome Engineering, State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083, China 2 Science and Technology on Advanced High Temperature Structural Materials Laboratory, AECC Beijing Institute of Aeronautical Materials, Beijing 100095, China |
引用本文:
和思亮, 赵云松, 鲁凡, 张剑, 李龙飞, 冯强. 热等静压对铸态及固溶态第二代镍基单晶高温合金显微缺陷及持久性能的影响[J]. 金属学报, 2020, 56(9): 1195-1205.
Siliang HE,
Yunsong ZHAO,
Fan LU,
Jian ZHANG,
Longfei LI,
Qiang FENG.
Effects of Hot Isostatic Pressure on Microdefects and Stress Rupture Life of Second-Generation Nickel-Based Single Crystal Superalloy in As-Cast and As-Solid-Solution States[J]. Acta Metall Sin, 2020, 56(9): 1195-1205.
| [1] |
Zhao X B, Liu L, Yang C B, et al. Advance in research of casting defects of directionally solidified nickel-based single superalloys [J]. J. Mater. Eng., 2012, (1): 93
|
| [1] |
(赵新宝, 刘 林, 杨初斌等. 镍基单晶高温合金凝固缺陷研究进展 [J]. 材料工程, 2012, (1): 93)
|
| [2] |
Elliott A J, Pollock T M, Tin S, et al. Directional solidification of large superalloy castings with radiation and liquid-metal cooling: A comparative assessment [J]. Metall. Mater. Trans., 2004, 35A: 3221
|
| [3] |
Zhang J, Lou L H. Directional solidification assisted by liquid metal cooling [J]. J. Mater. Sci. Technol., 2007, 23: 289
|
| [4] |
Chen R Z. Development status of single crystal superalloys [J]. J. Mater. Eng., 1995, (8): 3
|
| [4] |
(陈荣章. 单晶高温合金发展现状 [J]. 材料工程, 1995, (8): 3)
|
| [5] |
Ma W Y, Li S S, Qiao M, et al. Effect of heat treatment on microstructure and stress rupture life of Ni-base single crystal superalloy [J]. Chin. J. Nonferrous Met., 2006, 16: 937
doi: 10.1016/S1003-6326(06)60355-5
|
| [5] |
(马文有, 李树索, 乔 敏等. 热处理对镍基单晶高温合金微观组织和高温持久性能的影响 [J]. 中国有色金属学报, 2006, 16: 937)
|
| [6] |
Danninger H, Weiss B. The influence of defects on high cycle fatigue of metallic materials [J]. J. Mater. Process. Technol., 2003, 143-144: 179
|
| [7] |
Murakami Y, Endo M. Effects of defects, inclusions and inhomogeneities on fatigue strength [J]. Int. J. Fatigue, 1994, 16: 163
|
| [8] |
Aldinger F. Materials by Powder Technology, PTM93 [M]. Obserusel, Germany: DGM Informationsgesellschaft, 1993: 247
|
| [9] |
Guo H M, Zhao Y S, Zheng S, et al. Effect of hot-isostatic pressing on microstructure and mechanical properties of second generation single crystal superalloy DD6 [J]. J. Mater. Eng., 2016, 44(10): 60
|
| [9] |
(郭会明, 赵云松, 郑 帅等. 热等静压对第二代单晶高温合金DD6显微组织和力学性能的影响 [J]. 材料工程, 2016, 44(10): 60)
|
| [10] |
Atkinson H V, Davies S. Fundamental aspects of hot isostatic pressing: An overview [J]. Metall. Mater. Trans., 2000, 31A: 2981
|
| [11] |
Bocanegra-Bernal M H. Hot isostatic pressing (HIP) technology and its applications to metals and ceramics [J]. J. Mater. Sci., 2004, 39: 6399
|
| [12] |
Ning Y Q, Yao Z K, Fu M W, et al. Recrystallization of the hot isostatic pressed nickel-base superalloy FGH4096: I. Microstructure and mechanism [J]. Mater. Sci. Eng., 2011, A528: 8065
|
| [13] |
Galante R, Figueiredo-Pina C G, Serro A P. Additive manufacturing of ceramics for dental applications: A review [J]. Dent. Mater., 2019, 35: 825
pmid: 30948230
|
| [14] |
Wei C N, Bor H Y, Chang L. Effect of hot isostatic pressing on microstructure and mechanical properties of CM-681LC nickel-base superalloy using microcast [J]. Mater. Trans., 2008, 49: 193
|
| [15] |
Zhao X M, Lin X, Chen J, et al. The effect of hot isostatic pressing on crack healing, microstructure, mechanical properties of Rene88DT superalloy prepared by laser solid forming [J]. Mater. Sci. Eng., 2009, A504: 129
|
| [16] |
Cao L M, Liu L J, Chen J Y, et al. Effect of hot isostatic pressing temperature on the microstructure of a third generation single crystal superalloy DD10 [J]. J. Mater. Eng., 2013, (6): 1
|
| [16] |
(曹腊梅, 刘丽君, 陈晶阳等. 热等静压温度对第三代单晶高温合金DD10组织的影响 [J]. 材料工程, 2013, (6): 1)
|
| [17] |
Roncery L M, Lopez-Galilea I, Ruttert B, et al. Influence of temperature, pressure, and cooling rate during hot isostatic pressing on the microstructure of an SX Ni-base superalloy [J]. Mater. Des., 2016, 97: 544
|
| [18] |
Luo Y S, Guo H M, Zhao Y S, et al. Effect of hot isostatic pressing on high-temperature high cycle fatigue properties of a second generation single crystal superalloy DD6 [J]. Mater. Mech. Eng., 2016, 40(7): 51
|
| [18] |
(骆宇时, 郭会明, 赵云松等. 热等静压对第二代DD6单晶高温合金高温高周疲劳性能的影响 [J]. 机械工程材料, 2016, 40(7): 51)
|
| [19] |
Reed R C, Cox D C, Rae C M F. Damage accumulation during creep deformation of a single crystal superalloy at 1150 ℃ [J]. Mater. Sci. Eng., 2007, A448: 88
|
| [20] |
Chang J C, Choi C, Kim J C, et al. Development of microstructure and mechanical properties of a Ni-base single-crystal superalloy by hot-isostatic pressing [J]. J. Mater. Eng. Perform., 2003, 12: 420
|
| [21] |
Shi Q Y, Li X H, Zheng Y R, et al. Formation of solidification and homogenisation micropores in two single crystal superalloys produced by HRS and LMC processes [J]. Acta Metall. Sin., 2012, 48: 1237
doi: 10.3724/SP.J.1037.2012.00172
|
| [21] |
(石倩颖, 李相辉, 郑运荣等. HRS和LMC工艺制备的两种镍基单晶高温合金铸态及固溶微孔的形成 [J]. 金属学报, 2012, 48: 1237)
doi: 10.3724/SP.J.1037.2012.00172
|
| [22] |
Bokstein B S, Epishin A I, Link T, et al. Model for the porosity growth in single-crystal nickel-base superalloys during homogenization [J]. Scr. Mater., 2007, 57: 801
|
| [23] |
Li X W, Wang L, Dong J S, et al. Evolution of micro-pores in a single-crystal nickel-based superalloy during solution heat treatment [J]. Metall. Mater. Trans., 2017, 48A: 2682
|
| [24] |
Toloraya V N, Svetlov I L. Effect of conditions of directed crystallization and heat treatment on the porosity of single crystals of high-temperature nickel alloys [J]. Russ. Metall., 1991, 5: 70
|
| [25] |
Epishin A, Fedelich B, Link T, et al. Pore annihilation in a single-crystal nickel-base superalloy during hot isostatic pressing: Experiment and modelling [J]. Mater. Sci. Eng., 2013, A586: 342
|
| [26] |
Yan B C, Zhang J, Lou L H. Effect of boron additions on the microstructure and transverse properties of a directionally solidified superalloy [J]. Mater. Sci. Eng., 2008, A474: 39
|
| [27] |
Schmidt R, Feller-Kniepmeier M. Effect of heat treatments on phase chemistry of the nickel-base superalloy SRR 99 [J]. Metall. Trans., 1992, 23A: 745
|
| [28] |
Wilson B C, Cutler E R, Fuchs G E. Effect of solidification parameters on the microstructures and properties of CMSX-10 [J]. Mater. Sci. Eng., 2008, A479: 356
|
| [29] |
Yu Z, Rao S X, Zheng Z, et al. Interaction of hot isostatic pressing temperature and hydrostatic pressure on the healing of creep cavities in a nickel-based superalloy [J]. Mater. Des., 2013, 49: 25
doi: 10.1016/j.matdes.2013.01.055
|
| [30] |
Zhou Y, Zhang Z, Zhong Q P, et al. Model for healing of creep cavities in nickel-based superalloys under hot isostatic pressing [J]. Comput. Mater. Sci., 2012, 65: 320
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|