| 热处理对选区激光熔化镍基粉末高温合金组织与力学性能的影响 |
郝志博1, 葛昌纯1( ), 黎兴刚2, 田甜1, 贾崇林3 |
1 北京科技大学材料科学与工程学院 北京 100083 2 南方科技大学前沿与交叉科学研究院 深圳 518055 3 中国航发北京航空材料研究院先进高温结构材料重点实验室 北京 100095 |
|
| Effect of Heat Treatment on Microstructure and Mechanical Properties of Nickel-Based Powder Metallurgy Superalloy Processed by Selective Laser Melting |
HAO Zhibo1, GE Changchun1( ), LI Xinggang2, TIAN Tian1, JIA Chonglin3 |
1 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China 2 SUSTech Academy for Advanced Interdisciplinary Studies, Southern University of Science and Technology, Shenzhen 518055, China 3 Science and Technology on Advanced High Temperature Structural Materials Laboratory, Beijing Institute of Aeronautical Materials, Beijing 100095, China |
引用本文:
郝志博, 葛昌纯, 黎兴刚, 田甜, 贾崇林. 热处理对选区激光熔化镍基粉末高温合金组织与力学性能的影响[J]. 金属学报, 2020, 56(8): 1133-1143.
Zhibo HAO,
Changchun GE,
Xinggang LI,
Tian TIAN,
Chonglin JIA.
Effect of Heat Treatment on Microstructure and Mechanical Properties of Nickel-Based Powder Metallurgy Superalloy Processed by Selective Laser Melting[J]. Acta Metall Sin, 2020, 56(8): 1133-1143.
| [1] |
Tan L M, Jia J, Zhang Y W. Strengthening effect of alloying elements on powder metallurgical FGH97 superalloys [J]. Rare Met. Mater. Eng., 2017, 46: 1578
|
| [1] |
(谭黎明, 贾 建, 张义文. 合金元素对镍基粉末高温合金FGH97的强化作用 [J]. 稀有金属材料与工程, 2017, 46: 1578)
|
| [2] |
Tian T, Hao Z B, Jia C L, et al. Microstructure and properties of a new third generation powder metallurgy superalloy FGH100L [J]. Acta Metall. Sin., 2019, 55: 1260
doi: 10.11900/0412.1961.2018.00500
|
| [2] |
(田 甜, 郝志博, 贾崇林等. 新型第三代粉末高温合金FGH100L的显微组织与力学性能 [J]. 金属学报, 2019, 55: 1260)
doi: 10.11900/0412.1961.2018.00500
|
| [3] |
Liu Y H, Ning Y Q, Yao Z K, et al. Plastic deformation and dynamic recrystallization of a powder metallurgical nickel-based superalloy [J]. J. Alloys Compd., 2016, 675: 73
doi: 10.1016/j.jallcom.2016.03.093
|
| [4] |
Ning Y Q, Yao Z K, Yue T W, et al. Link microstructure of FGH4096 alloy [J]. Rare Met. Mater. Eng., 2009, 38: 1783
|
| [4] |
(宁永权, 姚泽坤, 岳太文等. FGH4096合金“项链”组织研究 [J]. 稀有金属材料与工程, 2009, 38: 1783)
|
| [5] |
Peng Z C, Tian G F, Jiang J, et al. Mechanistic behaviour and modelling of creep in powder metallurgy FGH96 nickel superalloy [J]. Mater. Sci. Eng., 2016, A676: 441
|
| [6] |
Liu C Z, Liu F, Huang L, et al. Effect of hot extrusion and heat treatment on microstructure of nickel-base superalloy [J]. Trans. Nonferrous Met. Soc. China, 2014, 24: 2544
doi: 10.1016/S1003-6326(14)63381-1
|
| [7] |
Chen Z, Xiang Y, Wei Z Y, et al. Thermal dynamic behavior during selective laser melting of K418 superalloy: Numerical simulation and experimental verification [J]. Appl. Phys., 2018, 124A: 313
|
| [8] |
Choi J P, Shin G H, Yang S S, et al. Densification and microstructural investigation of Inconel 718 parts fabricated by selective laser melting [J]. Powder Technol., 2017, 310: 60
doi: 10.1016/j.powtec.2017.01.030
|
| [9] |
Li J, Zhao Z Y, Bai P K, et al. Microstructural evolution and mechanical properties of IN718 alloy fabricated by selective laser melting following different heat treatments [J]. J. Alloys Compd., 2019, 772: 861
doi: 10.1016/j.jallcom.2018.09.200
|
| [10] |
Deng D Y, Peng R L, Brodin H, et al. Microstructure and mechanical properties of Inconel 718 produced by selective laser melting: Sample orientation dependence and effects of post heat treatments [J]. Mater. Sci. Eng., 2018, A713: 294
|
| [11] |
Strὂßner J, Terock M, Glatzel U. Mechanical and microstructural investigation of nickel-based superalloy IN718 manufactured by selective laser melting (SLM) [J]. Adv. Eng. Mater., 2015, 17: 1099
doi: 10.1002/adem.201500158
|
| [12] |
Nadammal N, Cabeza S, Mishurova T, et al. Effect of hatch length on the development of microstructure, texture and residual stresses in selective laser melted superalloy Inconel 718 [J]. Mater. Des., 2017, 134: 139
doi: 10.1016/j.matdes.2017.08.049
|
| [13] |
Hao Z B, Tian T, Li X G, et al. Microstructure and mechanical properties of powder metallurgy superalloy FGH4096 fabricated by selective laser melting [J]. Chin. J. Rare Met., 2020, 44: 476
|
| [13] |
(郝志博, 田 甜, 黎兴刚等. 选区激光熔化FGH4096高温合金的组织与性能 [J]. 稀有金属, 2020, 44: 476)
|
| [14] |
Muñoz-Moreno R, Divya V D, Messé O M D M, et al. Effect of heat treatments on the microstructure and texture of CM247LC processed by selective laser melting [A]. Superalloys 2016: Proceedings of the 13th International Symposium on Superalloys [C]. Warrendale, PA: TMS, 2016: 375
|
| [15] |
Messé O M D M, Muñoz-Moreno R, Illston T, et al. Metastable carbides and their impact on recrystallisation in IN738LC processed by selective laser melting [J]. Addit. Manuf., 2018, 22: 394
|
| [16] |
Wang Z M, Guan K, Gao M, et al. The microstructure and mechanical properties of deposited-IN718 by selective laser melting [J]. J. Alloys Compd., 2012, 513: 518
doi: 10.1016/j.jallcom.2011.10.107
|
| [17] |
Divya V D, Muñoz-Moreno R, Messé O M D M, et al. Microstructure of selective laser melted CM247LC nickel-based superalloy and its evolution through heat treatment [J]. Mater. Charact., 2016, 114: 62
doi: 10.1016/j.matchar.2016.02.004
|
| [18] |
Holland S, Wang X Q, Chen J, et al. Multiscale characterization of microstructures and mechanical properties of Inconel 718 fabricated by selective laser melting [J]. J. Alloys Compd., 2019, 784: 182
doi: 10.1016/j.jallcom.2018.12.380
|
| [19] |
Li S, Wei Q S, Shi Y S, et al. Microstructure characteristics of Inconel 625 superalloy manufactured by selective laser melting [J]. J. Mater. Sci. Technol., 2015, 31: 946
doi: 10.1016/j.jmst.2014.09.020
|
| [20] |
Kunze K, Etter T, Grässlin J, et al. Texture, anisotropy in microstructure and mechanical properties of IN738LC alloy processed by selective laser melting (SLM) [J]. Mater. Sci. Eng., 2015, A620: 213
|
| [21] |
Davies S J, Jeffs S P, Coleman M P, et al. Effects of heat treatment on microstructure and creep properties of a laser powder bed fused nickel superalloy [J]. Mater. Des., 2018, 159: 39
doi: 10.1016/j.matdes.2018.08.039
|
| [22] |
Chlebus E, Gruber K, Kuźnicka K, et al. Effect of heat treatment on the microstructure and mechanical properties of Inconel 718 processed by selective laser melting [J]. Mater. Sci. Eng., 2015, A639: 647
|
| [23] |
Hirsch M, Catchpole-Smith S, Patel R, et al. Meso-scale defect evaluation of selective laser melting using spatially resolved acoustic spectroscopy [J]. Proc. R. Soc. London, 2017, 473A: 20170194
|
| [24] |
Marchese G, Lorusso M, Calignano F, et al. Inconel 625 by direct metal laser sintering: Effects of the process parameters and heat treatments on microstructure and hardness [A]. Superalloys 2016: Proceedings of the 13th International Symposium on Superalloys [C]. Warrendale, PA: TMS, 2016: 1013
|
| [25] |
Jia C L, Zhang F L, Li Y, et al. Investigation on microstructure evolution of a new disk superalloy under different hot process [J]. Met. Powder Rep., 2018, 73: 319
doi: 10.1016/j.mprp.2018.02.001
|
| [26] |
Hao Z B, Tian T, Yang Y, et al. Effect of post-treatments on microstructure and mechanical properties of a novel nickel-based powder metallurgy superalloy processed by selective laser melting [J]. Mater. Res. Express, 2019, DOI: 10.1088/2053-1591/ab4108
doi: 10.1088/2053-1591/3/9/094001
pmid: 32391160
|
| [27] |
Kanagarajah P, Brenne F, Niendorf T, et al. Inconel 939 processed by selective laser melting: Effect of microstructure and temperature on the mechanical properties under static and cyclic loading [J]. Mater. Sci. Eng., 2013, A588: 188
|
| [28] |
Tomus D, Tian Y, Rometsch P A, et al. Influence of post heat treatments on anisotropy of mechanical behaviour and microstructure of Hastelloy-X parts produced by selective laser melting [J]. Mater. Sci. Eng., 2016, A667: 42
|
| [29] |
Hao Z B, Tian T, Peng S Q, et al. Effect of heat treatment on microstructure and properties of FGH4096M superalloy processed by selective laser melting [J]. Met. Mater. Int., 2019, DOI: 10.1007/s12540-019-00467-0
|
| [30] |
Academic Committee of the Superalloys, CMS. China Superalloys Handbook (Book 2) [M]. Beijing: China Quality Inspection Press, Standards Press of China, 2012: 635
|
| [30] |
(中国金属学会高温材料分会. 中国高温合金手册(下卷) [M]. 北京: 中国质检出版社, 中国标准出版社, 2012: 635)
|
| [31] |
Dong K X, Yuan C, Gao S, et al. Creep properties of a powder metallurgy disk superalloy at 700 ℃ [J]. J. Mater. Res., 2017, 32: 624
doi: 10.1557/jmr.2016.510
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|