Please wait a minute...
金属学报  2020, Vol. 56 Issue (2): 249-256    DOI: 10.11900/0412.1961.2019.00203
  研究论文 本期目录 | 过刊浏览 |
金属Nb级联碰撞的分子动力学模拟
马小强1,2,杨坤杰3,徐喻琼1,2(),杜晓超1,2,周建军1,2,肖仁政1,2
1. 三峡大学机械与动力学院 宜昌 443002
2. 三峡大学水电机械设备设计与维护湖北省重点实验室 宜昌 443002
3. 烟台大学核装备与核工程学院 烟台 264005
Molecular Dynamics Simulation of DisplacementCascades in Nb
MA Xiaoqiang1,2,YANG Kunjie3,XU Yuqiong1,2(),DU Xiaochao1,2,ZHOU Jianjun1,2,XIAO Renzheng1,2
1. College of Mechanical and Power Engineering, China Three Gorges University, Yichang 443002, China
2. Hubei Key Laboratory of Hydroelectric Machinery Design & Maintenance, China Three Gorges University, Yichang 443002, China
3. College of Nuclear Equipment and Nuclear Engineering, Yantai University, Yantai 264005, China
引用本文:

马小强,杨坤杰,徐喻琼,杜晓超,周建军,肖仁政. 金属Nb级联碰撞的分子动力学模拟[J]. 金属学报, 2020, 56(2): 249-256.
Xiaoqiang MA, Kunjie YANG, Yuqiong XU, Xiaochao DU, Jianjun ZHOU, Renzheng XIAO. Molecular Dynamics Simulation of DisplacementCascades in Nb[J]. Acta Metall Sin, 2020, 56(2): 249-256.

全文: PDF(6060 KB)   HTML
摘要: 

运用分子动力学方法研究了bcc结构Nb在辐照损伤初期因辐照诱发位移损伤形成和演化的微观过程以及原子机制。选取初级离位原子(primary knock-on atom,PKA)能量5~50 keV,模拟温度300 K,研究了Nb中级联碰撞产生的缺陷数量及其分布随模拟时间的演化,PKA能量对稳定Frenkel缺陷数目的影响,缺陷团簇的分布等。研究结果显示,级联碰撞会在体系中产生辐照缺陷,Frenkel 缺陷对数目和不同的PKA能量区间(5~30 keV和30~50 keV)之间满足不同的幂函数关系,所形成的缺陷大多数以点缺陷的形式存在,空位团簇成团率17%~35%,间隙原子团簇成团率23%~40%,PKA能量越高,空位越容易形成较大的团簇;级联碰撞产生的间隙原子形成了大量的沿<110>方向的哑铃型结构;当PKA能量高于30 keV时,级联碰撞将产生1/2<111>间隙型位错环和<100>空位型位错环。

关键词 : Nb,  分子动力学,  位移级联,  Frenkel缺陷,  缺陷团簇    
Abstract:

Refractory metal Nb and its alloys are considered as promising materials in fusion reactor, where they are required to withstand a high neutron irradiation, because their excellent high temperature properties such as high temperature strength, good thermal conductivity and compatibility with most liquid metal coolants. The defects are created in atomic displacement cascade from the primary state of damage and subsequent evolution gives rise to important change in their microstructures and engineering properties. However, the evolution and aggregation of induced radiation defects in atomic level cannot be observed by experiment so far. In this work, molecular dynamics (MD) method is used to explore the microstructural formation and evolution of defects from the atomic displacement cascades in bcc-Nb. In the simulation, the energy range of primary knock-on atom (PKA) is chosen 5~50 keV and the simulation temperature 300 K. It is observed that the most of defects in bcc Nb are point defects at different PKA energies. The vacancy cluster rate varies from 17% to 35% and self-interstitial cluster rate varies from 23% to 40%. As the PKA energy increasing, vacancies usually tend to form larger clusters. The self-interstitial atoms form a dumbbell structure along the direction <110>. The 1/2<111> intermittent dislocation loop and <100> vacancy dislocation loop are produced when the PKA energy greater than 30 keV. The quantitative relationship between energy of PKA (EPKA) and number of survivals Frenkel pairs (NFP) is fitted by a power function with different parameters at low-energies (5~30 keV) and the high-energies (30~50 keV).

Key words: Nb    molecular dynamics (MD)    displacement cascade    Frenkel pair    defect cluster
收稿日期: 2019-06-20     
ZTFLH:  TG132  
基金资助:三峡大学人才专项经费项目(2016KJX03);水电机械设备设计与维护湖北省重点实验室开放基金项目(2019KJX08)
作者简介: 马小强,男,1976年生,讲师,博士
EPKA / keVCell sizeNumber of atomSimulation time / ps
520a×20a×20a1600020
1020a×20a×20a1600020
2030a×30a×30a5400025
3040a×40a×40a12800025
4060a×60a×60a43200030
5080a×80a×80a102400040
表1  不同PKA能量级联碰撞模拟盒子尺寸和原子数
图1  能量30 keV沿方向[235]的初级离位原子(PKA)产生的Frenkel缺陷对随时间的演化
图 2  能量30 keV、沿方向[235]运动的PKA级联碰撞过程产生的缺陷随时间演化过程可视化截图
图3  不同能量PKA级联碰撞过程中产生的缺陷数目随时间的演化
图4  存活Frenkel对数目和级联碰撞效率随PKA能量的变化
图 5  间隙原子和空位的成团率随EPKA的变化
图6  不同能量PKA间隙原子团簇和空位团簇的尺寸和数量分布
[1] Demkowicz M J, Misra A, Caro A. The role of interface structure in controlling high helium concentrations [J]. Curr. Opin.Solid State Mater. Sci., 2012, 16(3): 101
[2] Demkowicz M J, Hoagland R G, Hirth J P. Interface structure and radiation damage resistance in Cu-Nb multilayer nanocomposites [J]. Phys. Rev. Lett., 2008, 100: 136102
[3] Hattar K, Demkowicz M J, Misra A, et al. Arrest of He bubble growth in Cu-Nb multilayer nanocomposites [J]. Scr. Mater., 2008, 58: 541
[4] Allen T R, Stoller R E, Yamanaka S. Comprehensive Nuclear Materials [M]. Vol.4, Amsterdam: Elsevier Ltd., 2012: 182
[5] Buckman R W Jr. Nuclear space power systems materials requirements [A]. AIP Conference Proceedings [C]. Am. Inst. Phys., 2004, 699: 815
[6] Tavassoli A A F. Present limits and improvements of structural materials for fusion reactors—A review [J]. J. Nucl. Mater., 2002, 302(2-3): 73
[7] Goldberg D C, Dicker G, Worcester S A. Niobium and niobium alloys in nuclear power [J]. Nucl. Eng. Des., 1972, 22: 124
[8] Was G S. Fundamentals of Radiation Materials Science: Metals and Alloys [M]. 2nd Ed., New York: Springer, 2017: 167
[9] Ma X Q, Yuan D Q, Xia H H, et al. Molecular dynamics simulation of evolution of defect and temperature effect in irradiated 3C-SiC [J]. Atomic Energy Sci. Technol., 2016, 50: 219
[9] (马小强,袁大庆,夏海鸿,等. 3C-SiC辐照诱发缺陷演化及温度效应分子动力学模拟 [J]. 原子能科学技术, 2016, 50: 219)
[10] Ma-Thai C C, Bacon D J. Relaxed vacancy formation and surface energies in b.c.c transition metals [J]. Philos. Mag., 1985, 52A: 1
[11] Ackland G J, Thetford R. An improved N-body semi-empirical model for body-centred cubic transition metals [J]. Philos. Mag., 1987, 56A: 15
[12] Lee B J, Baskes M I, Kim H, et al. Second nearest-neighbor modified embedded atom method potentials for bcc transition metals [J]. Phys. Rev., 2001, 64B: 184102
[13] Plimpton S. Fast parallel algorithms for short-range molecular dynamics [J]. J. Comput. Phys., 1995, 117: 1
[14] Stukowski A. Visualization and analysis of atomistic simulation data with OVITO—The open visualization tool [J]. Model. Simul. Mater. Sci. Eng., 2010, 18: 015012
[15] Tikhonchev M, Svetukhin V, Kapustin P. Primary radiation damage of Zr-0.5%Nb binary alloy: Atomistic simulation by molecular dynamics method [J]. Model. Simul. Mater. Sci. Eng., 2017, 25: 065017
[16] Lin D Y, Wang S S, Peng D L, et al. An n-body potential for a Zr-Nb system based on the embedded-atom method [J]. J. Phys: Condens. Matter, 2013, 25: 105404
[17] Ziegler J F, Biersack J P, Ziegler M D. SRIM—The Stopping and Range of Ions in Matter [M]. Chester: SRIM Co., 2008: 2
[18] Mendelev M I, Ackland G J. Development of an interatomic potential for the simulation of phase transformations in zirconium [J]. Philos. Mag. Lett., 2007, 87: 349
[19] Was G S. Fundamentals of Radiation Materials Science: Metals and Alloys [M]. 2nd Ed., New York: Springer, 2016: 127
[20] Cai J, Lu D G, Ma Y, et al.Structure evolution of defects in bcc iron by dislacement cascade: Molecular dynamics simulation [J]. Chin. J. Comput. Phys., 2011, 28: 915
[20] (蔡 军,陆道纲,马 雁等. 分子动力学模拟bcc铁中级联碰撞产生的缺陷结构及其演变 [J]. 计算物理, 2011, 28: 915)
[21] Chen W J, Lei J H. The molecular dynamics based research on the displacement cascades in zirconium [J]. J. Southwest Univ. Sci. Technol., 2017, 32(1): 101
[21] (陈文杰,雷洁红. 金属锆中离位级联碰撞的分子动力学模拟 [J]. 西南科技大学学报, 2017, 32(1): 101)
[22] Cao H, He X F, Wang D J, et al. Molecular dynamics simulation of displacement cascades in α-iron at different temperatures [J]. Atomic Energy Sci. Technol., 2019, 53: 487
[22] (曹 晗, 贺新福, 王东杰等. 不同温度下α-Fe中级联碰撞分子动力学模拟研究 [J]. 原子能科学技术, 2019, 53: 487)
[23] Yao M, Cui W, Wang X D, et al. Molecular dynamics simulation of initial radiation damage in tungsten [J]. Acta Metall., 2015, 51: 724
[23] (姚 曼, 崔 薇, 王旭东等. W辐照损伤初期的分子动力学研究 [J]. 金属学报, 2015, 51: 724)
[24] Bj?rkas C, Nordlund K, Dudarev S. Modelling radiation effects using the ab-initio based tungsten and vanadium potentials [J]. Nucl. Instrum. Methods Phys. Res., 2009, 267B: 3204
[25] Soneda N, Ishino S, de la Rubia T. Vacancy loop formation by ''cascade collapse'' in α-Fe: A molecular dynamics study of 50 keV cascades [J]. Philos. Mag. Lett., 2001, 81: 649
[26] Averback R S, de la Rubia T D, Benedek R. Dynamics and structure of energetic displacement cascades [J]. Nucl. Instrum.Methods Phys. Res., 1988, 33B: 693
[27] Norgett M J, Robinson M T, Torrens I M. A proposed method of calculating displacement dose rates [J]. Nucl. Eng. Des., 1975, 33: 50
[28] Li X Y, Xu Y C, Duan G H, et al. On the possibility of universal interstitial emission induced annihilation in metallic nanostructures [J]. J. Nucl. Mater., 2018, 500: 199
[29] Duan G H, Li X Y, Sun J J, et al. Surface-structure dependence of healing radiation-damage mechanism in nanoporous tungsten [J]. J. Nucl. Mater., 2018, 498: 362
[30] Bacon D J, Calder A F, Gao F, et al. Computer simulation of defect production by displacement cascades in metals [J]. Nucl. Instrum.Methods Phys. Res., 1995, 102B: 37
[31] Allen T R, Stoller R E, Yamanaka S. Comprehensive Nuclear Materials [M]. Vol.1, Amsterdam: Elsevier Ltd., 2012: 312
[32] Voskoboinikov R E, Osetsky Y N, Bacon D J. Computer simulation of primary damage creation in displacement cascades in copper. I. Defect creation and cluster statistics [J]. J. Nucl. Mater., 2008, 377: 385
[33] Gao F, Bacon D J, Howe L M, et al. Temperature-dependence of defect creation and clustering by displacement cascades in α-zirconium [J]. J. Nucl. Mater., 2001, 294: 288
[34] Selby A P, Xu D H, Juslin N, et al. Primary defect production by high energy displacement cascades in molybdenum [J]. J. Nucl. Mater., 2013, 437: 19
[35] Cerdeira M A, Palacios S L, González C, et al. Ab initio simulations of the structure, energetics and mobility of radiation-induced point defects in bcc Nb [J]. J. Nucl. Mater., 2016, 478: 185
[1] 刘兴军, 魏振帮, 卢勇, 韩佳甲, 施荣沛, 王翠萍. 新型钴基与Nb-Si基高温合金扩散动力学研究进展[J]. 金属学报, 2023, 59(8): 969-985.
[2] 冯艾寒, 陈强, 王剑, 王皞, 曲寿江, 陈道伦. 低密度Ti2AlNb基合金热轧板微观组织的热稳定性[J]. 金属学报, 2023, 59(6): 777-786.
[3] 姜江, 郝世杰, 姜大强, 郭方敏, 任洋, 崔立山. NiTi-Nb原位复合材料的准线性超弹性变形[J]. 金属学报, 2023, 59(11): 1419-1427.
[4] 梁琛, 王小娟, 王海鹏. 快速凝固Ti-Al-Nb合金B2相形成机制与显微力学性能[J]. 金属学报, 2022, 58(9): 1169-1178.
[5] 李亚敏, 张瑶瑶, 赵旺, 周生睿, 刘洪军. Cu对Inconel 718合金Nb偏析影响机理的第一性原理研究[J]. 金属学报, 2022, 58(2): 241-249.
[6] 李海勇, 李赛毅. 纯Al <111>对称倾斜晶界迁移行为温度相关性的分子动力学研究[J]. 金属学报, 2022, 58(2): 250-256.
[7] 陈瑞润, 陈德志, 王琪, 王墅, 周哲丞, 丁宏升, 傅恒志. Nb-Si基超高温合金及其定向凝固工艺的研究进展[J]. 金属学报, 2021, 57(9): 1141-1154.
[8] 姜江, 郝世杰, 姜大强, 郭方敏, 任洋, 崔立山. NiTi-NbTi原位复合材料的Lüders带型变形和载荷转移行为[J]. 金属学报, 2021, 57(7): 921-927.
[9] 王明康, 苑峻豪, 刘宇峰, 王清, 董闯, 张中伟. Ti对Zr-Nb二元合金β结构稳定性和力学性能的影响[J]. 金属学报, 2021, 57(1): 95-102.
[10] 梁晋洁, 高宁, 李玉红. 体心立方Fe中微裂纹与间隙型位错环相互作用的分子动力学模拟[J]. 金属学报, 2020, 56(9): 1286-1294.
[11] 吴贇, 刘雅辉, 康茂东, 高海燕, 王俊, 孙宝德. K4169合金循环加载过程中的微观组织演变[J]. 金属学报, 2020, 56(9): 1185-1194.
[12] 李美霖, 李赛毅. 金属Mg二阶锥面<c+a>刃位错运动特性的分子动力学模拟[J]. 金属学报, 2020, 56(5): 795-800.
[13] 李源才, 江五贵, 周宇. 温度对碳纳米管增强纳米蜂窝镍力学性能的影响[J]. 金属学报, 2020, 56(5): 785-794.
[14] 李源才, 江五贵, 周宇. 纳米孔洞对单晶/多晶Ni复合体拉伸性能的影响[J]. 金属学报, 2020, 56(5): 776-784.
[15] 钱月,孙蓉蓉,张文怀,姚美意,张金龙,周邦新,仇云龙,杨健,成国光,董建新. Nb对Fe22Cr5Al3Mo合金显微组织和耐腐蚀性能的影响[J]. 金属学报, 2020, 56(3): 321-332.