NiTi-NbTi原位复合材料的Lüders带型变形和载荷转移行为 |
姜江1, 郝世杰2, 姜大强2, 郭方敏2, 任洋3, 崔立山2( ) |
1.江西省科学院 江西省铜钨新材料重点实验室 南昌 330096 2.中国石油大学(北京) 新能源与材料学院 北京 102249 3.X -ray Science Division, Argonne National Laboratory, Argonne, Illinois 60439, USA |
|
Lüders-Like Deformation and Stress Transfer Behavior in an In Situ NiTi-NbTi Composite |
JIANG Jiang1, HAO Shijie2, JIANG Daqiang2, GUO Fangmin2, REN Yang3, CUI Lishan2( ) |
1.Jiangxi Key Laboratory of Advanced Copper and Tungsten Materials, Jiangxi Academy of Sciences, Nanchang 330096, China 2.College of New Energy and Materials, China University of Petroleum-Beijing, Beijing 102249, China 3.X -ray Science Division, Argonne National Laboratory, Argonne, Illinois 60439, USA |
引用本文:
姜江, 郝世杰, 姜大强, 郭方敏, 任洋, 崔立山. NiTi-NbTi原位复合材料的Lüders带型变形和载荷转移行为[J]. 金属学报, 2021, 57(7): 921-927.
Jiang JIANG,
Shijie HAO,
Daqiang JIANG,
Fangmin GUO,
Yang REN,
Lishan CUI.
Lüders-Like Deformation and Stress Transfer Behavior in an In Situ NiTi-NbTi Composite[J]. Acta Metall Sin, 2021, 57(7): 921-927.
1 |
Niu J G, Xiao W. The lattice instability induced by Ti-site Ni in B2 austenite in TiNi alloy [J]. Acta Metall. Sin., 2019, 55: 267
|
1 |
牛建钢, 肖 伟. TiNi合金B2奥氏体中Ti位Ni诱导的晶格失稳 [J]. 金属学报, 2019, 55: 267
|
2 |
Zhao Y C, Sun H, Li C L, et al. High temperature deformation behavior of high strength and toughness Ti-Ni base bulk metallic glass composites [J]. Acta Metall. Sin., 2018, 54: 1818
|
2 |
赵燕春, 孙 浩, 李春玲等. 高强韧Ti-Ni基块体金属玻璃复合材料高温变形行为 [J]. 金属学报, 2018, 54: 1818
|
3 |
Wei Z Z, Ma X, Zhang X P. Topological modelling of the B2-B19' martensite transformation crystallography in NiTi alloy [J]. Acta Metall. Sin., 2018, 54: 1461
|
3 |
韦昭召, 马 骁, 张新平. NiTi合金B2-B19'马氏体相变晶体学的拓扑模拟研究 [J]. 金属学报, 2018, 54: 1461
|
4 |
He Z R, Wu P Z, Liu K K, et al. Microstructure, phase transformation and shape memory behavior of chilled Ti-47Ni alloy ribbons [J]. Acta Metall. Sin., 2018, 54: 1157
|
4 |
贺志荣, 吴佩泽, 刘康凯等. 激冷Ti-47Ni合金薄带的组织、相变和形状记忆行为 [J]. 金属学报, 2018, 54: 1157
|
5 |
Yang C G, Shan J G, Ren J L. Phase transformation temperature control of weld metal of laser welded TiNi shape memory alloy joint [J]. Acta Metall. Sin., 2013, 49: 199
|
5 |
杨成功, 单际国, 任家烈. TiNi形状记忆合金激光焊接焊缝金属相变温度的控制 [J]. 金属学报, 2013, 49: 199
|
6 |
Ke C B, Cao S S, Ma X, et al. Phase field simulation of auto-catalytic growth effect of coherent Ni4Ti3 precipitate in NiTi shape memory alloy [J]. Acta Metall. Sin., 2013, 49: 115
|
6 |
柯常波, 曹姗姗, 马 骁等. NiTi形状记忆合金中Ni4Ti3共格沉淀相自催化生长效应的相场模拟 [J]. 金属学报, 2013, 49: 115
|
7 |
Zhu Y G, Zhang Y, Zhao D. Micromechanical constitutive model for phase transformation of NiTi polycrystal SMA [J]. Acta Metall. Sin., 2013, 49: 123
|
7 |
朱祎国, 张 杨, 赵 聃. 多晶NiTi形状记忆合金相变的细观力学本构模型 [J]. 金属学报, 2013, 49: 123
|
8 |
Du H F, Zeng P, Zhao J Q, et al. In situ multi-fields investigation on instability and transformation localization of martensitic phase transformation in NiTi alloys [J]. Acta Metall. Sin., 2013, 49: 17
|
8 |
杜泓飞, 曾 攀, 赵加清等. NiTi合金中马氏体相变失稳与局部化的原位多场研究 [J]. 金属学报, 2013, 49: 17
|
9 |
Zhang H B, Jin W, Yang R. 3D finite element simulation of pull-out force of TiNiFe shape memory pipe coupling with inner convex [J]. Acta Metall. Sin., 2012, 48: 1520
|
9 |
张慧博, 金 伟, 杨 锐. 内脊型TiNiFe记忆合金管接头拉脱力的三维有限元模拟 [J]. 金属学报, 2012, 48: 1520
|
10 |
Yang C G, Shan J G, Ren J L. Study on shape recovery temperature of TiNi alloy laser weld joint [J]. Acta Metall. Sin., 2012, 48: 513
|
10 |
杨成功, 单际国, 任家烈. TiNi合金激光焊接接头形状恢复温度的研究 [J]. 金属学报, 2012, 48: 513
|
11 |
He Z R, Wang Q, Shao D W. Effect of aging on microstructure and superelasticity in Ti-50.8Ni-0.3Cr shape memory alloy [J]. Acta Metall. Sin., 2012, 48: 56
|
11 |
贺志荣, 王 启, 邵大伟. 时效对Ti-50.8Ni-0.3Cr形状记忆合金组织和超弹性的影响 [J]. 金属学报, 2012, 48: 56
|
12 |
Jiang H J, Ke C B, Cao S S, et al. Preparation of nano-sized SiC reinforced NiTi shape memory composites and their mechanical properties and damping behavior [J]. Acta Metall. Sin., 2011, 47: 1105
|
12 |
江鸿杰, 柯常波, 曹姗姗等. 纳米SiC颗粒增强NiTi形状记忆复合材料制备及其力学性能和阻尼行为 [J]. 金属学报, 2011, 47: 1105
|
13 |
Ke C B, Ma X, Zhang X P. Phase field simulation of effects of pores on B2-R phase transformation in NiTi shape memory alloy [J]. Acta Metall. Sin., 2011, 47: 129
|
13 |
柯常波, 马 骁, 张新平. 孔隙对NiTI形状记忆合金中B2-R相变影响的相场模拟 [J]. 金属学报, 2011, 47: 129
|
14 |
Yang J, He Z R, Wang F, et al. Effect of Cr addition on transformation and cyclic deformation characteristics of Ti-Ni shape memory alloy [J]. Acta Metall. Sin., 2011, 47: 157
|
14 |
杨 军, 贺志荣, 王 芳等. Cr掺杂对Ti-Ni形状记忆合金相变和循环形变特性的影响 [J]. 金属学报, 2011, 47: 157
|
15 |
Ke C B, Ma X, Zhang X P. Phase field simulation of the effect of applied external stress on growth kinetics of coherent Ni4Ti3 precipitate in NiTi alloy [J]. Acta Metall. Sin., 2010, 46: 921
|
15 |
柯常波, 马 骁, 张新平. 外应力对NiTi合金中共格Ni4Ti3沉淀相长大行为影响的相场法模拟 [J]. 金属学报, 2010, 46: 921
|
16 |
Wang Q, He Z R, Wang Y S, et al. Effects of annealing temperature and stress-strain cycle on superelasticity of Ti-Ni-Cr shape memory alloy [J]. Acta Metall. Sin., 2010, 46: 800
|
16 |
王 启, 贺志荣, 王永善等. 退火温度和应力-应变循环对Ti-Ni-Cr形状记忆合金超弹性的影响 [J]. 金属学报, 2010, 46: 800
|
17 |
Yamada Y, Taya M, Watanabe R. Strengthening of metal matrix composite by shape memory effect [J]. Mater. Trans., JIM, 1993, 34: 254
|
18 |
Mizuuchi K, Inoue K, Hamada K, et al. Processing of TiNi SMA fiber reinforced AZ31 Mg alloy matrix composite by pulsed current hot pressing [J]. Mater. Sci. Eng., 2004, A367: 343
|
19 |
Jang B K, Kishi T. Adhesive strength between TiNi fibers embedded in CFRP composites [J]. Mater. Lett., 2005, 59: 1338
|
20 |
Shimamoto A, Furuya Y, Abe H. Effect of fatigue crack propagation in the shape memory alloy fiber reinforced smart composite [J]. Key Eng. Mater., 2007, 334-335: 1093
|
21 |
Aoki T, Shimamoto A. Active vibration control using cantilever beam of smart matrix composite with embedded shape memory alloy [J]. Key Eng. Mater., 2004, 270-273: 2187
|
22 |
Zheng Y J, Cui L S, Schrooten J. Basic design guidelines for SMA/epoxy smart composites [J]. Mater. Sci. Eng., 2005, A390: 139
|
23 |
Jiang D Q, Cui L S, Zheng Y J, et al. Constrained martensitic transformation in an in situ lamella TiNi/NbTi shape memory composite [J]. Mater. Sci. Eng., 2009, A515: 131
|
24 |
Tsoi K A, Stalmans R, Schrooten J. Transformational behaviour of constrained shape memory alloys [J]. Acta Mater., 2002, 50: 3535
|
25 |
Piao M, Miyazaki S, Otsuka K, et al. Effects of Nb addition on the microstructure of Ti-Ni alloys [J]. Mater. Trans., JIM, 1992, 33: 337
|
26 |
Jiang D Q, Jiang J, Shi X B, et al. Constrained martensitic transformation in nanocrystalline TiNi/NbTi shape memory composites [J]. J. Alloys Compd., 2011, 577(suppl.1): S749
|
27 |
Hao S J, Cui L S, Wang Y D, et al. The ultrahigh mechanical energy-absorption capability evidenced in a high-strength NbTi/NiTi nanocomposite [J]. Appl. Phys. Lett., 2011, 99: 024102
|
28 |
Hao S J, Cui L S, Shao Y, et al. In situ X-ray diffraction study of deformation behavior in a Fe/NiTi composite [J]. Appl. Phys. Lett., 2012, 101: 221904.
|
29 |
Hao S J, Cui L S, Jiang D Q, et al. A transforming metal nanocomposite with large elastic strain, low modulus, and high strength [J]. Science, 2013, 339: 1191
|
30 |
Wang S, Cui L S, Hao S J, et al. Locality and rapidity of the ultra-large elastic deformation of Nb nanowires in a NiTi phase-transforming matrix [J]. Sci. Rep., 2014, 4: 6753
|
31 |
Liu Z Y, Cui L S, Liu Y N, et al. Influence of internal stress coupling on the deformation behavior of NiTi-Nb nanowire composites [J]. Scr. Mater., 2014, 77: 75
|
32 |
Liu Z Y, Liu Y N, Jiang D Q, et al. Local strain matching between Nb nanowires and a phase transforming NiTi matrix in an in-situ composite [J]. Mater. Sci. Eng., 2014, A610: 6
|
33 |
Cui L S, Jiang D Q. Progress in high performance nanocomposites based on a strategy of strain matching [J]. Acta Metall. Sin., 2019, 55: 45
|
33 |
崔立山, 姜大强. 基于应变匹配的高性能金属纳米复合材料研究进展 [J]. 金属学报, 2019, 55: 45
|
34 |
Zhang X D, Zong H X, Cui L S, et al. Origin of high strength, low modulus superelasticity in nanowire-shape memory alloy composites [J]. Sci. Rep., 2017, 7: 46360
|
35 |
Shaw J A, Kyriakides S. On the nucleation and propagation of phase transformation fronts in a NiTi alloy [J]. Acta Mater., 1997, 45: 683
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|