| W含量对一种高W镍基高温合金显微组织的影响 |
华涵钰1,2,谢君1( ),舒德龙1,侯桂臣1,盛乃成1,于金江1,崔传勇1,孙晓峰1,周亦胄1 |
1. 中国科学院金属研究所 沈阳 110016 2. 东北大学冶金学院 沈阳 110819 |
|
| Influence of W Content on the Microstructure of Nickel Base Superalloy with High W Content |
HUA Hanyu1,2,XIE Jun1( ),SHU Delong1,HOU Guichen1,Naicheng SHENG1,YU Jinjiang1,CUI Chuanyong1,SUN Xiaofeng1,ZHOU Yizhou1 |
1. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2. School of Metallurgy, Northeastern University, Shenyang 110819, China |
引用本文:
华涵钰,谢君,舒德龙,侯桂臣,盛乃成,于金江,崔传勇,孙晓峰,周亦胄. W含量对一种高W镍基高温合金显微组织的影响[J]. 金属学报, 2020, 56(2): 161-170.
Hanyu HUA,
Jun XIE,
Delong SHU,
Guichen HOU,
SHENG Naicheng,
Jinjiang YU,
Chuanyong CUI,
Xiaofeng SUN,
Yizhou ZHOU.
Influence of W Content on the Microstructure of Nickel Base Superalloy with High W Content[J]. Acta Metall Sin, 2020, 56(2): 161-170.
| [1] | Shi C X, Zhong Z Y. Development and innovation of superalloy in China [J]. Acta Metall. Sin., 2010, 46: 1281 | | [1] | (师昌绪, 仲增墉. 我国高温合金的发展与创新 [J]. 金属学报, 2010, 46: 1281) | | [2] | Gao S, Zhou Y Z, Li C F, et al. Effects of platinum group metals addition on the precipitation of topologically close-packed phase in Ni-base single crystal superalloys [J]. J. Alloys Compd., 2016, 671: 458 | | [3] | Yin F S, Zheng Q, Sun X F, et al. Effect of melt treatment on carbides formation in a cast nickel-base superalloy M963 [J]. J. Mater. Process. Technol., 2007, 183: 440 | | [4] | Phillips P J, Unocic R R, Mills M J. Low cycle fatigue of a polycrystalline Ni-based superalloy: Deformation substructure analysis [J]. Int. J. Fatigue, 2013, 57: 50 | | [5] | Du B N, Yang J X, Cui C Y, et al. Effects of grain size on the high-cycle fatigue behavior of IN792 superalloy [J]. Mater. Des., 2015, 65: 57 | | [6] | Chiou M S, Jian S R, Yeh A C, et al. High temperature creep properties of directionally solidified CM-247LC Ni-based superalloy [J]. Mater. Sci. Eng., 2016, A655: 237 | | [7] | Zhang X B, Liu C S, Lv J Y, et al. Secondarily precipitated phases of a Ni-based superalloy during durable thermal treatment [J]. J. Northeastern Univ. (Nat. Sci.), 2005, 26: 355 | | [7] | (张小彬, 刘常升, 吕俊英等. 镍基高温合金长期时效过程中第二相的析出 [J]. 东北大学学报(自然科学版), 2005, 26: 355) | | [8] | Tian S G, Qian B J, Li T, et al. Precipitation behavior of TCP phase and its influence on stress rupture property of single crystal nickel-based superalloys [J]. Chin. J. Nonferrous Met., 2010, 20: 2154 | | [8] | (田素贵, 钱本江, 李 唐等. 镍基单晶合金中TCP相的析出行为及其对持久性能的影响 [J]. 中国有色金属学报, 2010, 20: 2154) | | [9] | Raju S V, Oni A A, Godwal B K, et al. Effect of B and Cr on elastic strength and crystal structure of Ni3Al alloys under high pressure [J]. J. Alloys Compd., 2015, 619: 616 | | [10] | Guo J T. Effects of several minor elements on superalloys and their mechanism [J]. Chin. J. Nonferrous Met., 2011, 21: 465 | | [10] | (郭建亭. 几种微量元素在高温合金中的作用与机理 [J]. 中国有色金属学报, 2011, 21: 465) | | [11] | Yu Z H, Zhang Y, Zhai Y N, et al. The research progress of the role of C, B and Hf in nickel-based superalloy [J]. Foundry, 2017, 66: 1076 | | [11] | (余竹焕, 张 洋, 翟娅楠等. C、B、Hf在镍基高温合金中作用的研究进展 [J]. 铸造, 2017, 66: 1076) | | [12] | Yen M K, Chen H Y. On the strengthening of nickel-base superalloys [J]. Acta Metall. Sin., 1964, 7: 307 | | [12] | (颜鸣皋, 陈学印. 镍基高温合金的强化 [J]. 金属学报, 1964, 7: 307) | | [13] | Zheng L. The effects of tantalum and ruthenium on the microstructures and properties of low chromium and high tungsten content cast nickel-base superalloys [D]. Xi'an: Xi'an University of Technology, 2004 | | [13] | (郑 亮. Ta和Ru对低Cr高W铸造镍基高温合金组织及性能的影响 [D]. 西安: 西安理工大学, 2004) | | [14] | Ritter N C, Sowa R, Schauer J C, et al. Effects of solid solution strengthening elements Mo, Re, Ru, and W on transition temperatures in nickel-based superalloys with high γ′-volume fraction: Comparison of experiment and CALPHAD calculations [J]. Metall. Mater. Trans., 2018, 49A: 3206 | | [15] | Zheng Y R. Development and application of low Cr and high W content cast nickel based superalloys in China [J]. J. Aeronaut. Mater., 2003, 23(Suppl.1): 227 | | [15] | (郑运荣. 我国低Cr高W系列铸造镍基高温合金的发展与应用 [J]. 航空材料学报, 2003, 23(增刊): 227) | | [16] | Xie J, Yu J J, Sun X F, et al. High-cycle fatigue behavior of K416B Ni-based casting superalloy at 700 ℃ [J]. Acta Metall. Sin., 2016, 52: 257 | | [16] | (谢 君, 于金江, 孙晓峰等. K416B镍基铸造高温合金的700 ℃高周疲劳行为 [J]. 金属学报, 2016, 52: 257) | | [17] | Ma Y H, Zhao K, Yang F X, et al. Precipitation of α-W phase in nickel base superalloys [J]. J. Chin. Electr. Microsc. Soc., 2005, 24: 297 | | [17] | (马永会, 赵 锴, 杨飞雪等. 镍基高温合金中α-W相的析出 [J]. 电子显微学报, 2005, 24: 297) | | [18] | Zheng L. Formation and transformation of α phase in Ta-containing low Cr and high W content cast Ni-base superalloys [J]. Chin. J. Nonferrous Met., 2005, 15: 1566 | | [18] | (郑 亮. 含Ta低Cr高W铸造镍基高温合金中α相的形成与转变 [J]. 中国有色金属学报, 2005, 15: 1566) | | [19] | Xie J, Yu J J, Sun X F, et al. Microstructure and creep behavior of Hf-containing K416B as-cast Ni-based superalloy with high W content [J]. Chin. J. Nonferrous Met., 2015, 25: 1490 | | [19] | (谢 君, 于金江, 孙晓峰等. 含铪高钨K416B镍基铸造高温合金的组织与蠕变行为 [J]. 中国有色金属学报, 2015, 25: 1490) | | [20] | Zhang L, Qi F, Zhang W H, et al. μ phase precipitation in a high W strengthening superalloy and its effect on tensile properties [J]. Rare Met. Mater. Eng., 2012, 41: 1965 | | [20] | (张 磊, 祁 峰, 张伟红等. 一种高W高温合金中μ相析出及其对拉伸性能的影响 [J]. 稀有金属材料与工程, 2012, 41: 1965) | | [21] | Tian S G, Xia D, Li T, et al. Influence of element W and microstructure evolution on lattice parameters and misfits of nickel base superalloys [J]. J. Aeronaut. Mater., 2008, 28(4): 12 | | [21] | (田素贵, 夏 丹, 李 唐等. W含量及组织状态对镍基高温合金晶格常数及错配度的影响 [J]. 航空材料学报, 2008, 28(4): 12) | | [22] | Miedema A R, De Chatel P F, De Boer F R. Cohesion in alloys—Fundamentals of a semi-empirical model [J]. Physica, 1980, 100B+C: 1 | | [23] | Lu G M, Yue Q Z, Cui J Z. Thermodynamic properties of binary alloys of Zn-Mn and Zn-Ti [J]. Chin. J. Nonferrous Met., 2001, 11: 99 | | [23] | (路贵民, 乐启炽, 崔建忠. Zn-Mn和Zn-Ti二元合金热力学性质 [J]. 中国有色金属学报, 2001, 11: 99) | | [24] | Wang W Y, Shang S L, Wang Y, et al. Impact of W on structural evolution and diffusivity of Ni-W melts: An ab initio molecular dynamics study [J]. J. Mater. Sci., 2015, 50: 1071 | | [25] | Haidemenopoulos G N. Physical Metallurgy [M]. London: Taylor and Francis, 2018: 189 | | [26] | Zhang Y F. The microstructure and mechanical properties of a superalloy strengthened by high W addition [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2009 | | [26] | (张艳峰. 一种高W强化高温合金的组织与性能 [D]. 沈阳: 中国科学院金属研究所, 2009) | | [27] | Wang W, Fu L M. Effect of the Inclusions/precipitates size on the intragranular ferrite nucleation [J]. Acta Metall. Sin., 2008, 44: 723 | | [27] | (王 巍, 付立铭. 夹杂物/析出相尺寸对晶内铁素体形核的影响 [J]. 金属学报, 2008, 44: 723) | | [28] | Wills V A, Mccartney D G. A comparative study of solidification features in nickel-base superalloys: Microstructural evolution and microsegregation [J]. Mater. Sci. Eng., 1991, A145: 223 | | [29] | Pan Z Y, Hu X B, Xie G, et al. Effects of W and Re on the recrystallization of Ni-based single crystal superalloys [J]. J. Chin. Electr. Microsc. Soc., 2014, 33: 197 | | [29] | (潘智毅, 胡肖兵, 谢 光等. 难熔元素W/Re对镍基单晶高温合金再结晶的影响 [J]. 电子显微学报, 2014, 33: 197) | | [30] | Zhang L, Qi F, Zhang W H, et al. Effect of Boron on solidification of high W nickel-base superalloy [J]. Hot Working Technol., 2011, 40(23): 33 | | [30] | (张 磊, 祁 峰, 张伟红等. B对高W镍基高温合金凝固行为的影响 [J]. 热加工工艺, 2011, 40(23): 33) |
|
|