|
|
|
| 丝材+电弧增材制造钛/铝异种金属反应层的研究 |
田银宝,申俊琦( ),胡绳荪,勾健 |
| 天津大学材料科学与工程学院天津市现代连接技术重点实验室 天津 300354 |
|
| Study of the Reaction Layer of Ti and Al Dissimilar Alloys by Wire and Arc Additive Manufacturing |
TIAN Yinbao,SHEN Junqi ( ),HU Shengsun,GOU Jian |
| Tianjin Key Laboratory of Advanced Joining Technology, School of Materials Science and Engineering, Tianjin University, Tianjin 300354, China |
引用本文:
田银宝, 申俊琦, 胡绳荪, 勾健. 丝材+电弧增材制造钛/铝异种金属反应层的研究[J]. 金属学报, 2019, 55(11): 1407-1416.
TIAN Yinbao,
SHEN Junqi,
HU Shengsun,
GOU Jian.
Study of the Reaction Layer of Ti and Al Dissimilar Alloys by Wire and Arc Additive Manufacturing[J]. Acta Metall Sin, 2019, 55(11): 1407-1416.
| [1] | LiN, HuangS, ZhangG D, et al. Progress in additive manufacturing on new materials: A review [J]. J. Mater. Sci. Technol., 2019, 35: 242 | | [2] | YuJ, WangJ J, NiD R, et al. Microstructure and mechanical properties of additive manufactured 2319 alloy by electron beam freeform fabrication [J]. Acta Metall. Sin., 2018, 54: 1725 | | [2] | 于 菁, 王继杰, 倪丁瑞等. 电子束熔丝沉积快速成形2319铝合金的微观组织与力学性能 [J]. 金属学报, 2018, 54: 1725 | | [3] | ZuoH S, LiH J, QiL H, et al. Influence of interfacial bonding between metal droplets on tensile properties of 7075 aluminum billets by additive manufacturing technique [J]. J. Mater. Sci. Technol., 2016, 32: 485 | | [4] | XiongJ, LiR, LeiY Y, et al. Heat propagation of circular thin-walled parts fabricated in additive manufacturing using gas metal arc welding [J]. J. Mater. Process. Technol., 2018, 251: 12 | | [5] | HorgarA, FostervollH, Nyhus, B, et al. Additive manufacturing using WAAM with AA5183 wire [J]. J. Mater. Process. Technol., 2018, 259: 68 | | [6] | HadenC V, ZengG, CarterIII F M, et al. Wire and arc additive manufactured steel: Tensile and wear properties [J]. Addit. Manuf., 2017, 16: 115 | | [7] | WuB T, DingD H, PanZ X, et al. Effects of heat accumulation on the arc characteristics and metal transfer behavior in wire arc additive manufacturing of Ti6Al4V [J]. J. Mater. Process. Technol., 2017, 250: 304 | | [8] | ZhangE L, WangX Y, HanY. Research status of biomedical porous Ti and its alloy in China [J]. Acta Metall. Sin., 2017, 53: 1555 | | [8] | 张二林, 王晓燕, 憨 勇. 医用多孔Ti及钛合金的国内研究现状 [J]. 金属学报, 2017, 53: 1555 | | [9] | JinP, SuiR, LiF X, et al. Reactive wetting of TC4 titanium alloy by molten 6061 Al and 4043 Al alloys [J]. Acta Metall. Sin., 2017, 53: 479 | | [9] | 靳 鹏, 隋 然, 李富祥等. 熔融6061/4043铝合金在TC4钛合金表面的反应润湿 [J]. 金属学报, 2017, 53: 479 | | [10] | QiZ W, CongB Q, QiB J, et al. Microstructure and mechanical properties of double-wire+arc additively manufactured Al-Cu-Mg alloys [J]. J. Mater. Process. Technol., 2018, 255: 347 | | [11] | WangY, WangJ. Microstructure and mechanical properties of TIG welded-brazed joint of dissimilar Al/Ti alloy [J]. Heat Treat. Met., 2017, 42(2): 44 | | [11] | 王 勇, 王 敬. Al/Ti异种金属TIG熔钎焊接头的显微组织及力学性能 [J]. 金属热处理, 2017, 42(2): 44 | | [12] | LiJ Z, SunQ J, LiuY B, et al. Cold metal transfer welding-brazing of pure titanium TA2 to aluminum alloy 6061-T6 [J]. Adv. Eng. Mater., 2017, 19: 1600494 | | [13] | FengJ C, ZhangH T, HeP. The CMT short-circuiting metal transfer process and its use in thin aluminium sheets welding [J]. Mater. Des., 2009, 30: 1850 | | [14] | ChenS J, WangX, YuanT, et al. Research on prediction method of liquation cracking susceptibility to magnesium alloy welds [J]. Acta Metall. Sin., 2018, 54: 1735 | | [14] | 陈树君, 王 宣, 袁 涛等. 镁合金焊缝液化裂纹敏感性及预测方法探究 [J]. 金属学报, 2018, 54: 1735 | | [15] | TianY B, ShenJ Q, HuS S, et al. Effects of ultrasonic peening treatment on surface quality of CMT-welds of Al alloys [J]. J. Mater. Process. Technol., 2018, 254: 193 | | [16] | XieC J, YangS L, LiuH B, et al. Microstructure and mechanical properties of robot cold metal transfer Al5.5Zn2.5Mg2.2Cu aluminium alloy joints [J]. J. Mater. Process. Technol., 2018, 255: 507 | | [17] | CongB Q, OuyangR J, QiB J, et al. Influence of cold metal transfer process and its heat input on weld bead geometry and porosity of aluminum-copper alloy welds [J]. Rare Met. Mater. Eng., 2016, 45: 606 | | [18] | TianY B, ShenJ Q, HuS S, et al. Effects of ultrasonic vibration in the CMT process on welded joints of Al alloy [J]. J. Mater. Process. Technol., 2018, 259: 282 | | [19] | PangJ, HuS S, ShenJ Q, et al. Arc characteristics and metal transfer behavior of CMT+P welding process [J]. J. Mater. Process. Technol., 2016, 238: 212 | | [20] | ChenM A, ZhangD, WuC S. Current waveform effects on CMT welding of mild steel [J]. J. Mater. Process. Technol., 2017, 243: 395 | | [21] | PickinC G, YoungK. Evaluation of cold metal transfer (CMT) process for welding aluminium alloy [J]. Sci. Technol. Weld. Joining, 2006, 11: 583 | | [22] | GungorB, KalucE, TabanE, et al. Mechanical and microstructural properties of robotic cold metal transfer (CMT) welded 5083-H111 and 6082-T651 aluminum alloys [J]. Mater. Des., 2014, 54: 207 | | [23] | CaoR, YuG, ChenJ H, et al. Cold metal transfer joining aluminum alloys-to-galvanized mild steel [J]. J. Mater. Process. Technol., 2013, 213: 1753 | | [24] | SunQ J, LiJ Z, LiuY B, et al. Microstructural characterization and mechanical properties of Al/Ti joint welded by CMT method-assisted hybrid magnetic field [J]. Mater. Des., 2017, 116: 316 | | [25] | JiH, DengY L, XuH Y, et al. The influence of welding line energy on the microstructure and property of CMT overlap joint of 5182-O and HC260YD+Z [J]. Acta Metall. Sin., 2019, 55: 376 | | [25] | 吉 华, 邓运来, 徐红勇等. 焊接线能量对5182-O/HC260YD+Z异种材料CMT搭接接头组织与性能的影响 [J]. 金属学报, 2019, 55: 376 | | [26] | ZhangC, LiY F, GaoM, et al. Wire arc additive manufacturing of Al-6Mg alloy using variable polarity cold metal transfer arc as power source [J]. Mater. Sci. Eng., 2018, A711: 415 | | [27] | GuJ L, DingJ L, WilliamsS W, et al. The effect of inter-layer cold working and post-deposition heat treatment on porosity in additively manufactured aluminum alloys [J]. J. Mater. Process. Technol., 2016, 230: 26 | | [28] | GuJ L, DingJ L, WilliamsS W, et al. The strengthening effect of inter-layer cold working and post-deposition heat treatment on the additively manufactured Al-6.3Cu alloy [J]. Mater. Sci. Eng., 2016, A651: 18 | | [29] | OnuikeB, BandyopadhyayA. Additive manufacturing of Inconel 718-Ti6Al4V bimetallic structures [J]. Addit. Manuf., 2018, 22: 844 | | [30] | HinojosA, MirelesJ, ReichardtA, et al. Joining of Inconel 718 and 316 stainless steel using electron beam melting additive manufacturing technology [J]. Mater. Des., 2016, 94: 17 | | [31] | CuiQ L. Microstructure and mechanical properties of TIG weldedbrazed joint of pre-coating titanium and aluminum alloy [J]. Trans. China Weld. Inst., 2016, 37(10): 125 | | [31] | 崔庆龙. 预镀层钛合金与铝合金电弧熔钎焊接头界面组织及力学性能分析 [J]. 焊接学报, 2016, 37(10): 125 | | [32] | WangP. Study on CMT welding process of Mg/Al dissimilar metals based on the control of energy input process [D]. Tianjin: Tianjin University, 2017 | | [32] | 王 鹏. 基于CMT焊接能量输入过程控制的镁/铝异种金属焊接研究 [D]. 天津: 天津大学, 2017 | | [33] | LüS X, YangT, HuangY X, et al. Interface characteristics and facture behavior of TIG arc welding-brazed Ti/Al dissimilar alloys [J]. Rare Met. Mater. Eng., 2013, 42: 478 | | [33] | 吕世雄, 杨 涛, 黄永宪等. Ti/Al TIG微熔钎焊界面行为及接头断裂行为 [J]. 稀有金属材料与工程, 2013, 42: 478 | | [34] | WeiS Z, LiY J. Welding defects and improving technologies during fusion welding of Ti/Al dissimilar lightweight alloys [J]. Weld. Technol., 2014, 43(4): 59 | | [34] | 魏守征, 李亚江. 钛/铝异种轻金属熔焊缺陷及解决工艺 [J]. 焊接技术, 2014, 43(4): 59 | | [35] | SomashekaraM A, NaveenkumarM, KumarA, et al. Investigations into effect of weld-deposition pattern on residual stress evolution for metallic additive manufacturing [J]. Int. J. Adv. Manuf. Technol., 2017, 90: 2009 | | [36] | WeiS Z, LiY J, WangJ, et al. Effect of pulsed current on interfacial microstructure during welding-brazing of Ti/Al dissimilar alloys [J]. Trans. China Weld. Inst., 2015, 36(10): 49 | | [36] | 魏守征, 李亚江, 王 娟等. 脉冲电流对钛/铝异种金属熔钎焊界面特征的影响 [J]. 焊接学报, 2015, 36(10): 49 | | [37] | MaZ P, YuX L, MengQ W. Microstructure and fracture behavior of arc welding-brazing joints between titanium and aluminum dissimilar alloys [J]. Chin. J. Nonferrous Met., 2015, 25: 3067 | | [37] | 马志鹏, 于心泷, 孟庆武. 钛/铝异种合金电弧熔钎焊接接头的组织与断裂行为 [J]. 中国有色金属学报, 2015, 25: 3067 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|