| 自由落体条件下Ti-6Al-4V合金微液滴的快速凝固研究 |
翟斌, 周凯, 吕鹏, 王海鹏( ) |
| 西北工业大学应用物理系 西安 710072 |
|
| Rapid Solidification of Ti-6Al-4V Alloy Micro-Droplets Under Free Fall Condition |
Bin ZHAI, Kai ZHOU, Peng Lü, Haipeng WANG( ) |
| Department of Applied Physics, Northwestern Polytechnical University, Xi'an 710072, China |
引用本文:
翟斌, 周凯, 吕鹏, 王海鹏. 自由落体条件下Ti-6Al-4V合金微液滴的快速凝固研究[J]. 金属学报, 2018, 54(5): 824-830.
Bin ZHAI,
Kai ZHOU,
Peng Lü,
Haipeng WANG.
Rapid Solidification of Ti-6Al-4V Alloy Micro-Droplets Under Free Fall Condition[J]. Acta Metall Sin, 2018, 54(5): 824-830.
| [1] | Devaraj A, Joshi V V, Srivastava A, et al.A low-cost hierarchical nanostructured beta-titanium alloy with high strength[J]. Nat. Commun., 2016, 7: 11176 | | [2] | Zou P F, Wang H P, Yang S J, et al.Anomalous temperature dependence of liquid state density for Ni50Ti50 alloy investigated under electrostatic levitation state[J]. Chem. Phys. Lett., 2017, 681: 101 | | [3] | Zhang S Z, Li C, Hou W T, et al.Longitudinal compression behavior of functionally graded Ti-6Al-4V meshes[J]. J. Mater. Sci. Technol., 2016, 32: 1098 | | [4] | Zhao Z, Chen J, Guo S, et al.Influence of α/β interface phase on the tensile properties of laser cladding deposited Ti-6Al-4V titanium alloy[J]. J. Mater. Sci. Technol., 2017, 33: 675 | | [5] | Liu H H, Niinomi M, Nakai M, et al.β-type titanium alloys for spinal fixation surgery with high Young's modulus variability and good mechanical properties[J]. Acta Biomater., 2015, 24: 361 | | [6] | Kobryn P A, Moore E H, Semiatin S L.The effect of laser power and traverse speed on microstructure, porosity, and build height in laser-deposited Ti-6Al-4V[J]. Scr. Mater., 2000, 43: 299 | | [7] | Thijs L, Verhaeghe F, Craeghs T, et al.A study of the microstructural evolution during selective laser melting of Ti-6Al-4V[J]. Acta Mater., 2010, 58: 3303 | | [8] | Vrancken B, Thijs L, Kruth J P, et al.Heat treatment of Ti6Al4V produced by Selective Laser Melting: Microstructure and mechanical properties[J]. J. Alloys Compd., 2012, 541: 177 | | [9] | He T, Hu R, Zhang T B, et al.Effect of Nb content on solidification characteristics and microsegregation in cast Ti-48Al-xNb alloys[J]. Acta Metall. Sin.(Engl. Lett.), 2016, 29: 714 | | [10] | Liu Y, Hu R, Zhang T B, et al.Dendritic growth and microstructure evolution with different cooling rates in Ti-48Al-2Cr-2Nb alloy[J]. J. Mater. Eng. Perform., 2016, 25: 38 | | [11] | Zhou K, Wei B.Determination of the thermophysical properties of liquid and solid Ti-6Al-4V alloy[J]. Appl. Phys., 2016, 122A: 248 | | [12] | Wang H Y, Liu R P, Zhan Z J, et al.Dynamic and thermal computation of Fe-66.7%Si droplets free falling in a drop tube[J]. Acta Metall. Sin., 2005, 41: 940(王海燕, 刘日平, 战再吉等. Fe-66.7%Si合金液滴落管实验的动力学和传热学计算[J]. 金属学报, 2005, 41: 940) | | [13] | Oloyede O, Bigg T D, Cochrane R F, et al.Microstructure evolution and mechanical properties of drop-tube processed, rapidly solidified grey cast iron[J]. Mater. Sci. Eng., 2016, A654: 143 | | [14] | Luo S B, Wang W L, Xia Z C, et al.Theoretical prediction and experimental observation for microstructural evolution of undercooled nickel-titanium eutectic type alloys[J]. J. Alloys Compd., 2017, 692: 265 | | [15] | Wang G Q, Zhao Z B, Yu B B, et al.Effect of base material on microstructure and texture evolution of a Ti-6Al-4V electron-beam welded joint[J]. Acta Metall. Sin.(Engl. Lett.), 2017, 30: 499 | | [16] | Broderick T F, Jackson A G, Jones H, et al.The effect of cooling conditions on the microstructure of rapidly solidified Ti-6Al-4V[J]. Metall. Mater. Trans., 1985, 16: 1951 | | [17] | Ding R, Guo Z X, Wilson A.Microstructural evolution of a Ti-6Al-4V alloy during thermomechanical processing[J]. Mater. Sci. Eng., 2002, A327: 233 | | [18] | Grant P S, Cantor B, Katgerman L.Modelling of droplet dynamic and thermal histories during spray forming—I. Individual droplet behavior[J]. Acta Metall. Mater., 1993, 41: 3097 | | [19] | Lee E S, Ahn S.Solidification progress and heat transfer analysis of gas-atomized alloy droplets during spray forming[J]. Acta Metall. Mater., 1994, 42: 3231 | | [20] | Xu Z Y.Martensitic Transformation and Martensite [M]. Beijing: Science Press, 1980: 29(徐祖耀. 马氏体相变与马氏体 [M]. 北京: 科学出版社, 1980: 29) | | [21] | Ramirez-Ledesma A L, Lopez-Molina E, Lopez H F, et al. Athermal ε-martensite transformation in a Co-20Cr alloy: Effect of rapid solidification on plate nucleation[J]. Acta Mater., 2016, 111: 138 | | [22] | Ahmed T, Rack H J.Phase transformations during cooling in α+β titanium alloys[J]. Mater. Sci. Eng., 1998, A243: 206 | | [23] | Peng X N, Guo H Z, Wang T, et al.Effects of β treatments on microstructures and mechanical properties of TC4-DT titanium alloy[J]. Mater. Sci. Eng., 2012, A533: 55 | | [24] | Hrabe N, Quinn T.Effects of processing on microstructure and mechanical properties of a titanium alloy (Ti-6Al-4V) fabricated using electron beam melting (EBM), Part 2: Energy input, orientation, and location[J]. Mater. Sci. Eng., 2013, A573: 271 | | [25] | Wu S Q, Lu Y J, Gan Y L, et al.Microstructural evolution and microhardness of a selective-laser-melted Ti-6Al-4V alloy after post heat treatments[J]. J. Alloys Compd., 2016, 672: 643 | | [26] | Wang L, Su Y Q, Wang S J, et al.Effect of melt hydrogenation on structure and hardness of TC21 alloy[J]. Rare Met. Mater. Eng., 2011, 40: 321(王亮, 苏彦庆, 王书杰等. 液态置氢对TC21合金组织及硬度的影响[J]. 稀有金属材料与工程, 2011, 40: 321) |
|
|