| Ni-Fe-Cr合金固溶处理后的组织变化及其对性能的影响 |
陈胜虎( ), 戎利建 |
| 中国科学院金属研究所中国科学院核用材料与安全评价重点实验室 沈阳 110016 |
|
| Microstructure Evolution During Solution Treatment and Its Effects on the Properties of Ni-Fe-Cr Alloy |
Shenghu CHEN( ), Lijian RONG |
| Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
引用本文:
陈胜虎, 戎利建. Ni-Fe-Cr合金固溶处理后的组织变化及其对性能的影响[J]. 金属学报, 2018, 54(3): 385-392.
Shenghu CHEN,
Lijian RONG.
Microstructure Evolution During Solution Treatment and Its Effects on the Properties of Ni-Fe-Cr Alloy[J]. Acta Metall Sin, 2018, 54(3): 385-392.
| [1] | Pan Y M, Dunn D S, Cragnolino G A, et al.Grain-boundary chemistry and intergranular corrosion in alloy 825[J]. Metall. Mater. Trans., 2000, 31A: 1163 | | [2] | Persaud S Y, Smith J, Korinek A, et al.High resolution analysis of oxidation in Ni-Fe-Cr alloys after exposure to 315 ℃ deaerated water with added hydrogen[J]. Corros. Sci., 2016, 106: 236 | | [3] | Zhang L N, Szpunar J A, Basu R, et al.Influence of cold deformation on the corrosion behavior of Ni-Fe-Cr alloy 028[J]. J. Alloys Compd, 2014, 616: 235 | | [4] | Zhao Q, Xia S, Zhou B X, et al.Effect of thermal-mechanical processing on the grain boundary character distribution of alloy 825 tubes[J]. Acta Metall. Sin., 2015, 51: 1465(赵清, 夏爽, 周邦新等. 形变及热处理对825合金管材晶界特征分布的影响 [J]. 金属学报, 2015, 51: 1465) | | [5] | Feng Y, He D L, Gong D S, et al.Corrosion resistance properties of domestic 825 alloy[J]. J. Chin. Soc. Corros. Prot., 2013, 33: 164(冯勇, 何德良, 龚德胜等. 国产825合金的耐腐蚀性能研究 [J]. 中国腐蚀与防护学报, 2013, 33: 164) | | [6] | Ganesan P, Clatworthy E F, Harris J A.Development of a time-temperature transformation diagram for alloy 925[J]. Corrosion, 1988, 44: 827 | | [7] | Zhao Z, Li J Y, Dong J X, et al.Oxidation behavior during high temperature homo-genization treatment of cast Ni-Fe based corrosion resistant 925 alloy[J]. J. Chin. Soc. Corros. Prot., 2017, 37: 1(赵展, 李景阳, 董建新等. 925镍铁基耐蚀合金均匀化及高温氧化行为 [J]. 中国腐蚀与防护学报, 2017, 37: 1) | | [8] | Aytekin H, Ak?in Y.Characterization of borided incoloy 825 alloy[J]. Mater. Des., 2013, 50: 515 | | [9] | Rosenberg S J, Irish C R.Solubility of carbon in 18-percent-chromium-10-percent-nickel austenite[J]. J. Res. Natl. Bur. Stand., 1952, 48: 40 | | [10] | Pardo A, Merino M C, Coy A E, et al.Influence of Ti, C and N concentration on the intergranular corrosion behavior of AISI 316Ti and 321 stainless steels[J]. Acta Mater. 2007, 55: 2239 | | [11] | Gustafson A.Coarsening of TiC in austenitic stainless steel-experiments and simulations in comparison[J]. Mater. Sci. Eng., 2000, A287: 52 | | [12] | Cui Z Q, Qin Y C.Metallography and Heat Treatment [M]. 2nd Ed., Beijing: China Machine Press, 2007: 226(崔忠圻. 覃耀春. 金属学与热处理 [M]. 第2版. 北京: 机械工业出版社, 2007: 226) | | [13] | NSF825. NAS high corrosion resistant nickel alloy [EB/OL]. Nippon Yakin Kogyo Co., Ltd, 2011, | | [14] | Song X Y, Gu N J, Liu G Q, et al.Computer simulation of the influence of second-phase particle quantity on matrix grain growth[J]. Acta Metall. Sin., 2000, 36: 592(宋晓艳, 谷南驹, 刘国权等. 第二相粒子含量对基体晶粒长大影响的计算机仿真研究 [J]. 金属学报, 2000, 36: 592) | | [15] | Chen S H, Zhao M J, Rong L J.Effect of grain size on the hydrogen embrittlement sensitivity of a precipitation strengthened Fe-Ni based alloy[J]. Mater. Sci. Eng., 2014, A594: 98 | | [16] | Fu L M, Shan A D, Wang W.Effect of Nb solute drag and NbC precipitate pinning on the recrystallization grain growth in low carbon Nb-microacloyed steel[J]. Acta Metall. Sin., 2010, 46: 832(付立铭, 单爱党, 王巍. 低碳Nb微合金钢中Nb溶质拖曳和析出相NbC钉扎对再结晶晶粒长大的影响 [J]. 金属学报, 2010, 46: 832) | | [17] | Han L Z, Chen R K, Gu J F, et al.Behavior of austenite grain growth in X12CrMoWVNbN10-1-1 ferrite heat-resistant steel[J]. Acta Metall. Sin., 2009, 45: 1446(韩利战, 陈睿恺, 顾剑锋等. X12CrMoWVNbN10-1-1铁素体耐热钢奥氏体晶粒长大行为的研究 [J]. 金属学报, 2009, 45: 1446) | | [18] | Hua P T, Shen H S, Tai C T, et al.On the intergranular corrosion of 18-8stainless steel at different potentials[J]. Acta Metall. Sin., 1965, 8: 103(华保定, 沈行素, 戴钟道等. 18铬-8镍型不锈钢的晶间腐蚀与电位的关系 [J]. 金属学报, 1965, 8: 103) | | [19] | Crum J R, Tassen C S, Nagashima T.Precipitation reactions and corrosion resistance of thermally aged and welded alloy 825 [A]. Corrosion 97[C]. New Orleans, Louisiana: NACE International, 1997: 520 | | [20] | Kokawa H, Shimada M, Sato Y S.Grain-boundary structure and precipitation in sensitized austenitic stainless steel[J]. JOM, 2007, 52(7): 34 | | [21] | Tachibana S, Kuronuma, Yokota T, et al.Effect of hot rolling and cooling conditions on intergranular corrosion behavior in alloy 625 clad steel[J]. Corros. Sci., 2015, 99: 125 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|