					引用本文:
						|  |  
    					|  |  
    					| 金属材料疲劳性能预测统一模型探索 |  
						| 张哲峰(  ), 刘睿, 张振军, 田艳中, 张鹏 |  
					| 中国科学院金属研究所 沈阳 110016 |  
						|  |  
    					| Exploration on the Unified Model for Fatigue Properties Prediction of Metallic Materials |  
						| Zhefeng ZHANG(  ), Rui LIU, Zhenjun ZHANG, Yanzhong TIAN, Peng ZHANG |  
						| Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |  
								张哲峰, 刘睿, 张振军, 田艳中, 张鹏. 金属材料疲劳性能预测统一模型探索[J]. 金属学报, 2018, 54(11): 1693-1704.	
																												Zhefeng ZHANG,
																								Rui LIU,
																								Zhenjun ZHANG,
																								Yanzhong TIAN,
																												Peng ZHANG. 
				Exploration on the Unified Model for Fatigue Properties Prediction of Metallic Materials[J]. Acta Metall Sin, 2018, 54(11): 1693-1704.
 
					
						| 
								
									|  
          
          
            
             
			              
            
									            
									                
																														  
																| | [1] | Ashby M F.Materials Selection in Mechanical Design[M]. 4th Ed., Burlington: Butterworth-Heinemann, 2010: 1 |  | [2] | Meyers M A, Chawla K K.Mechanical Behavior of Materials [M]. 2nd Ed., New York: Cambridge University Press, 2005: 1 |  | [3] | Suresh S.Fatigue of Materials [M]. 2nd Ed., Cambridge: Cambridge University Press, 1998: 1 |  | [4] | Forrest P G.Fatigue of Metals [M]. Oxford: Pergamon Press, 1962: 1 |  | [5] | Zhao S B, Manual of Anti-Fatigue Design [M]. 2nd Ed., Beijing: China Machine Press, 2015: 1(赵少汴. 抗疲劳设计手册 [M]. 第2版. 北京: 机械工业出版社, 2015: 1) |  | [6] | Basquin O H.The exponential law of endurance tests[J]. Am. Soc. Test. Mater., 1910, 10: 625 |  | [7] | Coffin L F Jr. A study of the effects of cyclic thermal stresses on a ductile metal[J]. Trans. ASTM, 1954, 76: 931 |  | [8] | Manson S S.Behavior of materials under conditions of thermal stress [R]. USA: National Advisory Committee for Aeronautics, 1953 |  | [9] | Callister W D Jr, Rethwisch D G. Materials Science and Engineering: An Introduction[M]. 8th Ed., John Wiley and Sons, Inc, 2010: 1 |  | [10] | Shao C W, Zhang P, Liu R, et al.Low-cycle and extremely-low-cycle fatigue behaviors of high-Mn austenitic TRIP/TWIP alloys: Property evaluation, damage mechanisms and life prediction[J]. Acta Mater., 2016, 103: 781 |  | [11] | Kim Y W, Kim G, Hong S G, et al.Energy-based approach to predict the fatigue life behavior of pre-strained Fe-18Mn TWIP steel[J]. Mater. Sci. Eng., 2011, A528: 4696 |  | [12] | Liu R.Investigations on Tensile and Fatigue Properties of Cu-Al alloys [D]. Beijing: University of Chinese Academy of Sciences, 2018(刘睿. 铜铝合金拉伸与疲劳性能研究 [D]. 北京: 中国科学院大学, 2018) |  | [13] | Liu R, Zhang Z J, Zhang P, et al.Extremely-low-cycle fatigue behaviors of Cu and Cu-Al alloys: Damage mechanisms and life prediction[J]. Acta Mater., 2015, 83: 341 |  | [14] | Shimada K, Komotori J, Shimizu M.The applicability of the Manson-Coffin law and Miner's law to extremely low cycle fatigue[J]. Trans. Jpn. Soc. Mech. Eng., 1987, 53A: 1178 |  | [15] | Shao C W, Zhang P, Liu R, et al.A remarkable improvement of low-cycle fatigue resistance of high-Mn austenitic TWIP alloys with similar tensile properties: Importance of slip mode[J]. Acta Mater., 2016, 118: 196 |  | [16] | An X H, Wu S D, Wang Z G, et al.Enhanced cyclic deformation responses of ultrafine-grained Cu and nanocrystalline Cu-Al alloys[J]. Acta Mater., 2014, 74: 200 |  | [17] | An X H, Lin Q Y, Wu S D, et al.Improved fatigue strengths of nanocrystalline Cu and Cu-Al alloys[J]. Mater. Res. Lett., 2015, 3: 135 |  | [18] | Xue P, Huang Z Y, Wang B B, et al.Intrinsic high cycle fatigue behavior of ultrafine grained pure Cu with stable structure[J]. Sci. China Mater., 2016, 59: 531 |  | [19] | Liu R, Tian Y Z, Zhang Z J, et al.Exploring the fatigue strength improvement of Cu-Al alloys[J]. Acta Mater., 2018, 144: 613 |  | [20] | Liu R, Tian Y Z, Zhang Z J, et al.Fatigue strength plateau induced by microstructure inhomogeneity[J]. Mater. Sci. Eng., 2017, A702: 259 |  | [21] | Liu R, Zhang Z J, Zhang Z F.The criteria for microstructure evolution of Cu and Cu-Al alloys induced by cyclic loading[J]. Mater. Sci. Eng., 2016, A666: 123 |  | [22] | Valiev R Z, Islamgaliev R K, Alexandrov I V.Bulk nanostructured materials from severe plastic deformation[J]. Prog. Mater. Sci., 2000, 45: 103 |  | [23] | Valiev R.Nanostructuring of metals by severe plastic deformation for advanced properties[J]. Nat. Mater., 2004, 3: 511 |  | [24] | H?ppel H W, Zhou Z M, Mughrabi H, et al.Microstructural study of the parameters governing coarsening and cyclic softening in fatigued ultrafine-grained copper[J]. Philos. Mag., 2002, 82A: 1781 |  | [25] | Argon A S.Strengthening Mechanisms in Crystal Plasticity [M]. New York: Oxford University Press, 2008: 1 |  | [26] | Agnew S R, Vinogradov A Y, Hashimoto S, et al.Overview of fatigue performance of Cu processed by severe plastic deformation[J]. J. Electron. Mater., 1999, 28: 1038 |  | [27] | Kocks U F, Mecking H.Physics and phenomenology of strain hardening: The FCC case[J]. Prog. Mater. Sci., 2003, 48: 171 |  | [28] | Qu S, An X H, Yang H J, et al.Microstructural evolution and mechanical properties of Cu-Al alloys subjected to equal channel angular pressing[J]. Acta Mater., 2009, 57: 1586 |  | [29] | Liu R, Zhang Z J, Li L L, et al.Microscopic mechanisms contributing to the synchronous improvement of strength and plasticity (SISP) for TWIP copper alloys[J]. Sci. Rep., 2015, 5: 9550 |  | [30] | Li X Y, Lu K.Playing with defects in metals[J]. Nat. Mater., 2017, 16: 700 |  | [31] | Murr L E.Interfacial Phenomena in Metals and Alloys[M]. London: Addison-Wesley Educational Publishers Inc., 1975: 1 |  | [32] | An X H, Lin Q Y, Wu S D, et al.Significance of stacking fault energy on microstructural evolution in Cu and Cu-Al alloys processed by high-pressure torsion[J]. Philos. Mag., 2011, 91: 3307 | 
 |  
             
												
											    	
											        	|  | Viewed |  
											        	|  |  |  
												        |  | Full text 
 | 
 
 |  
												        |  |  |  
												        |  | Abstract 
 | 
 |  
												        |  |  |  
												        |  | Cited |  |  
												        |  |  |  |  
													    |  | Shared |  |  
													    |  |  |  |  
													    |  | Discussed |  |  |  |  |