| 回火温度对26CrMo钻杆钢显微组织和力学性能的影响 |
舒志强1( ),袁鹏斌2,欧阳志英1,龚丹梅1,白雪明1 |
1 上海海隆石油管材研究所 上海 200949 2 海隆石油工业集团有限公司 上海 200949 |
|
| Effects of Tempering Temperature on Microstructure and Mechanical Properties of Drill Pipe Steel 26CrMo |
Zhiqiang SHU1( ),Pengbin YUAN2,Zhiying OUYANG1,Danmei GONG1,Xueming BAI1 |
1 Shanghai Hailong Oil Tubular Goods Research Institute, Shanghai 200949, China 2 Hilong Group of Companies Ltd., Shanghai 200949, China |
引用本文:
舒志强,袁鹏斌,欧阳志英,龚丹梅,白雪明. 回火温度对26CrMo钻杆钢显微组织和力学性能的影响[J]. 金属学报, 2017, 53(6): 669-676.
Zhiqiang SHU,
Pengbin YUAN,
Zhiying OUYANG,
Danmei GONG,
Xueming BAI.
Effects of Tempering Temperature on Microstructure and Mechanical Properties of Drill Pipe Steel 26CrMo[J]. Acta Metall Sin, 2017, 53(6): 669-676.
| [1] | Liu X S.Drilling Technology Principle [M]. Beijing: Petroleum Industry Press, 1988: 95 | | [1] | (刘希圣. 钻井工艺原理 [M]. 北京: 石油工业出版社, 1988: 95) | | [2] | Long Z H, Zhang J H.Drilling Engineering [M]. Beijing: China Petrochemical Press, 2010: 64 | | [2] | (龙芝辉, 张锦宏. 钻井工程[M]. 北京: 中国石化出版社, 2010: 64) | | [3] | Gao L X, Zhang Y.String Design and Oil Tubular Goods Selection [M]. Beijing: Petroleum Industry Press, 2013: 97 | | [3] | (高连新, 张毅. 管柱设计与油井管选材 [M]. 北京: 石油工业出版社, 2013: 97) | | [4] | Zhang Y, Zhao R C, Zhang R X.Comment on technical quality of high-strength drill pipes made at home and abroad[J]. Steel Pipe, 2000, 29(5): 1 | | [4] | (张毅, 赵仁存, 张汝忻. 国内外高强度钻杆的技术质量评述 [J]. 钢管, 2000, 29(5): 1) | | [5] | Li J Q, Yu L S, Niu C J, et al.The production status and development trend of drill pipe[J]. Welded Pipe Tube, 2011, 34(11): 35 | | [5] | (李建强, 于丽松, 牛成杰等. 石油钻杆的生产现状与发展趋势[J]. 焊管, 2011, 34(11): 35) | | [6] | Wang X H, Zhang G J, Li F P, et al.Chemical composition, heat treatment and mechanical properties of drill pipe steel[J]. Petrol. Tub. Goods Instrum., 2015, 1(2): 33 | | [6] | (王新虎, 张冠军, 李方坡等. 钻杆钢的成分、热处理工艺及其力学性能[J]. 石油管材与仪器, 2015, 1(2): 33) | | [7] | Qian Q, Cao G Z, Liu C, et al.Influence by tempering temperature on performance of 26CrMo4s/2 drill pipe blank[J]. Steel Pipe, 2012, 41(5): 36 | | [7] | (钱强, 曹贵贞, 刘聪等. 回火温度对26CrMo4s/2钢钻杆用管性能的影响[J]. 钢管, 2012, 41(5): 36) | | [8] | Cao J J, Chen M A.Research on heat treatment technology of 26CrMoNbTiB (S135) drill pipe[J]. Met. Mater. Metall. Eng., 2007, 35(2): 28 | | [8] | (曹建军, 陈明安. 26CrMoNbTiB (S135)钻杆管热处理工艺的研究[J]. 金属材料与冶金工程, 2007, 35(2): 28) | | [9] | Zhang Z P, Zhang J S, Ning B Q.Effects of tempering temperature on microstructure and mechanical properties of 28CrMo47V steel[J]. Hot Work. Technol., 2012, 41(18): 184 | | [9] | (张哲平, 张佳森, 宁保群. 回火温度对28CrMo47V钢组织和性能的影响[J]. 热加工工艺, 2012, 41(18): 184) | | [10] | He S L, Cai H P, Han L H.Study on heat treatment process improving strength and toughness of S135 drill pipe[J]. Steel Pipe, 2011, 40(suppl.): 7 | | [10] | (何石磊, 蔡和平, 韩礼红. 提高S135钻杆强韧性的热处理工艺研究[J]. 钢管, 2011, 40(增刊): 7) | | [11] | Shaeri M H, Saghafian H, Shabestari S G.Effects of austempering and martempering processes on amount of retained austenite in Cr-Mo steels (FMU-226) used in mill liner[J]. J. Iron Steel Res. Int., 2010, 17: 53 | | [12] | Huang B S, Jiang Z Y, Pan H H, et al.Influence of different heat treatment on corrosion resistance of G105 pipe[J]. J. Chin. Soc. Corros. Protect., 2012, 32: 67 | | [12] | (黄本生, 江仲英, 潘欢欢等. 热处理工艺对G105钻杆材料抗腐蚀性能的影响[J]. 中国腐蚀与防护学报, 2012, 32: 67) | | [13] | Ouyang Z Y, Shu Z Q, Yuan P B.Effect of yield ratio on the performance of high strength and high ductility drill pipe[J]. Phys. Test. Chem. Anal.(Phys. Test.), 2013, 49A: 17 | | [13] | (欧阳志英, 舒志强, 袁鹏斌. 屈强比对高强度高塑性钻杆性能的影响[J]. 理化检验-物理分册, 2013, 49A: 17) | | [14] | Li Y H, Xin X X, Fan Y G.Discussion on the yield-tensile ratio parameters of high-strength pipe line steel[J]. China Petrol. Mach., 2006, 34(9): 105 | | [14] | (李晓红, 辛希贤, 樊玉光. 高强度管线钢屈强比参数的一些探讨[J]. 石油机械, 2006, 34(9): 105) | | [15] | Gao H L.Analysis and commentary on yield ratio of pipeline steel[J]. Welded Pipe Tube, 2010, 33(6): 10 | | [15] | (高惠临. 管线钢屈强比分析与评述[J]. 焊管, 2010, 33(6): 10) | | [16] | Tang Z T.Relationship between fracture and force-displacement curve of impact specimen[J]. Phys. Exam. Test., 2004, (4): 1 | | [16] | (唐振廷. 冲击试样断口与力-位移曲线之间的关系[J]. 物理测试, 2004, (4): 1) | | [17] | Wang H, Han L H, Hu F, et al.Effect of tempering temperature on precipitate and mechanical properties of an anti-sulfur, drill pipe steel in H2S containing environments[J]. Trans. Mater. Heat Treat., 2012, 33(3): 88 | | [17] | (王航, 韩礼红, 胡锋等. 回火温度对抗硫钻杆钢析出相形貌及力学性能的影响[J]. 材料热处理学报, 2012, 33(3): 88) | | [18] | Wu X L, Niu J, Dong J M.Effect of tempering temperature on microstructure and properties of 25Cr2Ni4MoV steel[J]. Hot Work. Technol., 2008, 37(20): 76 | | [18] | (吴新丽, 牛靖, 董俊明. 回火温度对25Cr2Ni4MoV钢组织和性能的影响[J]. 热加工工艺, 2008, 37(20): 76) | | [19] | Hui W J, Dong H, Weng Y Q, et al.Effect of heat treatment para-meters on mechanical properties of high strength Cr-Mo-V steel[J]. Acta Metall. Sin., 2002, 38: 1009 | | [19] | (惠卫军, 董瀚, 翁宇庆等. 回火温度对Cr-Mo-V系高强度钢力学性能的影响[J]. 金属学报, 2002, 38: 1009) | | [20] | Qin B, Wang Z Y, Sun Q S.Effect of tempering temperature on properties of 00Cr16Ni5Mo stainless steel[J]. Mater. Charact., 2008, 59: 1096 | | [21] | Wen T, Hu X F, Song Y Y, et al.Effect of tempering temperature on carbide and mechanical properties in a Fe-Cr-Ni-Mo high-strength steel[J]. Acta Metall. Sin., 2014, 50: 447 | | [21] | (温涛, 胡小锋, 宋元元等. 回火温度对一种Fe-Cr-Ni-Mo高强钢碳化物及其力学性能的影响[J]. 金属学报, 2014, 50: 447) | | [22] | Cui Z Q, Qin Y C.Metallographic and Heat Treatment [M]. 2nd Ed., Beijing: China Machine Press, 2007: 196 | | [22] | (崔忠圻, 覃耀春. 金属学与热处理 [M]. 第2版. 北京: 机械工业出版社, 2007: 196) | | [23] | Cui Y X, Wang C L.Metal Fracture Analysis [M]. Harbin: Harbin Industrial University Press, 1998: 73 | | [23] | (崔约贤, 王长利. 金属断口分析 [M]. 哈尔滨: 哈尔滨工业大学出版社, 1998: 73) | | [24] | Chen J D, Mo W L, Wang P, et al.Effects of tempering temperature on the impact toughness of steel 42CrMo[J]. Acta Metall. Sin., 2012, 48: 1186 | | [24] | (陈俊丹, 莫文林, 王培等. 回火温度对42CrMo钢冲击韧性的影响[J]. 金属学报, 2012, 48: 1186) | | [25] | Yuan S P, Liu G, Wang R H, et al.Coupling effect of multiple precipitates on the ductile fracture of aged Al-Mg-Si alloys[J]. Scr. Mater., 2007, 57: 865 | | [26] | Zhou H J, Tu M J, Deng Z J, et al.On the development of strength potentialities of metallic materials, the second part——Rational balance between strength and ductility or toughness[J]. J. Xi′an Jiaotong Univ., 1980, 14(1): 25 | | [26] | (周惠久, 涂铭旌, 邓增杰等. 再论发挥金属材料强度潜力问题——强度、塑性、韧度的合理配合[J]. 西安交通大学学报, 1980, 14(1): 25) | | [27] | Shu D L.Mechanical Properties of Materials [M]. 2nd Ed., Beijing: China Machine Press, 2007: 15 | | [27] | (束德林. 工程材料力学性能 [M]. 第2版. 北京: 机械工业出版社, 2007: 15) | | [28] | Zhou H J, Huang M Z.The Strength Theory of Metal Materials [M]. Beijing: Science Press, 1989: 215 | | [28] | (周惠久, 黄明志. 金属材料强度学 [M]. 北京: 科学出版社, 1989: 215) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|