| 第二相对镁基材料微弧氧化过程的影响机制* |
王艳秋1( ),吴昆2,王福会1,3 |
1 哈尔滨工程大学超轻材料与表面技术教育部重点实验室, 哈尔滨 150001 2 哈尔滨工业大学材料科学与工程学院, 哈尔滨 150001 3 中国科学院金属研究所, 沈阳 110016 |
|
| EFFECTS OF SECOND PHASES ON MICROARC OXIDATION PROCESS OF MAGNESIUM BASE MATERIALS |
Yanqiu WANG1( ),Kun WU2,Fuhui WANG1,3 |
1) Education Ministry Key Laboratory of Superlight Materials and Surface Technology, Harbin Engineering University, Harbin 150001, China 2) School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China 3) Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
引用本文:
王艳秋,吴昆,王福会. 第二相对镁基材料微弧氧化过程的影响机制*[J]. 金属学报, 2016, 52(6): 689-697.
Yanqiu WANG,
Kun WU,
Fuhui WANG.
EFFECTS OF SECOND PHASES ON MICROARC OXIDATION PROCESS OF MAGNESIUM BASE MATERIALS[J]. Acta Metall Sin, 2016, 52(6): 689-697.
| [1] | Van T B, Brown S D, Wirtz G P.Ceram Bull, 1977; 56: 563 | | [2] | Ikonopisov S.Electrochim Acta, 1977; 22: 1077 | | [3] | Srinivasan P B, Liang J, Blawert C, Stormer M, Dietzel W.Appl Surf Sci, 2009; 255: 4212 | | [4] | Li X J, Cheng G A, Xue W B, Zheng R T, Cheng Y J.Mater Chem Phys, 2008; 107: 148 | | [5] | Wang Y M, Lei T Q, Jiang B L, Guo L X.Appl Surf Sci, 2004; 233: 258 | | [6] | Verdier S, Boinet M, Maximovitch S, Dalard F.Corros Sci, 2005; 47: 1429 | | [7] | Krishtal M M.Met Sci Heat Treat, 2004; 46: 378 | | [8] | Khaselev O, Weiss D, Yahalom J.Corros Sci, 2001; 43: 1295 | | [9] | Khaselev O, Yahalom J.Corros Sci, 1998; 40: 1149 | | [10] | Hsiao H Y, Tsai W T.J Mater Res, 2005; 20: 2763 | | [11] | Zhu Q Z, Xue W B, Lu L, Du J C, Liu G J, Li W F.Acta Metall Sin, 2011; 47: 74 | | [11] | (朱庆振, 薛文斌, 鲁亮, 杜建成, 刘贯军, 李文芳. 金属学报, 2011; 47: 74) | | [12] | Xue W B.Appl Surf Sci, 2006; 252: 6195 | | [13] | Xue W B, Wu X L, Li X J, Tian H.J Alloys Compd, 2006; 425: 302 | | [14] | Xue W B, Jin Q, Zhu Q Z, Hua M, Ma Y Y. J Alloys Compd, 2009; 482: 208 | | [15] | Arrabal R, Matykina E, Skeldon P, Thompson G E.Appl Surf Sci, 2009; 255: 5071 | | [16] | Arrabal R, Pardo A, Merino M C, Mohedano M, Casajús P, Matykina E, Skeldon P, Thompson G E. Corros Sci, 2010; 52: 3738 | | [17] | Hihara L H, Latanision R M.Int Mater Rev, 1994; 39: 245 | | [18] | Trzaskoma P P, McCafferty E, Crowe C R.J Electrochem Soc, 1983; 130: 1804 | | [19] | Pohlman S L.Corrosion, 1978; 34: 156 | | [20] | Turhan M C, Li Q Q, Jha H, Singer R F, Virtanen S.Electrochim Acta, 2011; 56: 7141 | | [21] | Xue W B.Acta Metall Sin, 2006; 42: 350 | | [21] | (薛文斌. 金属学报, 2006; 42: 350) | | [22] | Wang Y Q, Wang X J, Zhang T, Wu K, Wang F H.J Mater Sci Technol, 2013; 29: 1129 | | [23] | Wang Y Q, Wang X J, Wu K, Wang F H.J Mater Sci Technol, 2013; 29: 267 | | [24] | Wang Y Q, Wang X J, Gong W X, Wu K, Wang F H.Appl Surf Sci, 2013; 283: 906 | | [25] | Liu R, Weng N, Xue W B, Hua M, Liu G J, Li W F. Surf Coat Technol, 2015; 269: 212 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|