| 累积叠轧Mg/Al多层复合板材的织构演变及力学性能* |
李眉娟1,刘晓龙1,刘蕴韬1,郑明毅2,王琛2,陈东风1( ) |
1 中国原子能科学研究院核物理研究所, 北京 102413 2 哈尔滨工业大学材料科学与工程学院, 哈尔滨 150001 |
|
| TEXTURE EVOLUTION AND MECHANICAL PROPER-TIES OF Mg/Al MULTILAYERED COMPOSITE SHEETSPROCESSED BY ACCUMULATIVE ROLL BONDING |
Meijuan LI1,Xiaolong LIU1,Yuntao LIU1,Mingyi ZHENG2,Chen WANG2,Dongfeng CHEN1( ) |
1 Department of Nuclear Physics, China Institute of Atomic Energy, Beijing 102413, China 2 School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China |
引用本文:
李眉娟,刘晓龙,刘蕴韬,郑明毅,王琛,陈东风. 累积叠轧Mg/Al多层复合板材的织构演变及力学性能*[J]. 金属学报, 2016, 52(4): 463-472.
Meijuan LI,
Xiaolong LIU,
Yuntao LIU,
Mingyi ZHENG,
Chen WANG,
Dongfeng CHEN.
TEXTURE EVOLUTION AND MECHANICAL PROPER-TIES OF Mg/Al MULTILAYERED COMPOSITE SHEETSPROCESSED BY ACCUMULATIVE ROLL BONDING[J]. Acta Metall Sin, 2016, 52(4): 463-472.
| [1] | Yang Z, Li J P, Zhang J X, Lonmer G W, Robson J.Acta Metall, 2008; 21: 313 | | [2] | Saito Y, Utsunomiya H, Tsuji N, Sakai T.Acta Mater, 1999; 47: 579 | | [3] | Koizumi Y, Ueyama M, Tsuji N, Minamino Y, Ota K.J Alloys Compd, 2003; 355: 47 | | [4] | Wang Y Q, Hou H L, Li Z Q.J Plast Eng, 2006; 5(13): 45 | | [4] | (王耀奇, 侯红亮, 李志强. 塑性工程学报, 2006; 5(13): 45) | | [5] | Xu R C, Tang D, Ren X P, Wang X H, Wen Y H.Rare Met, 2007; 26: 230 | | [6] | Yang D, Cizek P, Hodgson P, Wen C.Scr Mater, 2010; 62: 321 | | [7] | Chang H, Zheng M Y, Gan W M, Xu C, Brokmeier H G.Rare Met Mater Eng, 2013; 42: 0441 | | [8] | Chino Y, Mabuchi M.Scr Mater, 2009; 60: 447 | | [9] | Tsuji N, Saito Y, Lee S H, Minamino Y.Adv Eng Mater, 2005; 5: 338 | | [10] | Huang X, Tsuji N, Hansen N, Minamino Y.Mater Sci Eng, 2003; A340: 265 | | [11] | Li B L, Tsuji N, Kamikawa N.Mater Sci Eng, 2006; A423: 331 | | [12] | Kamikawa N, Sakai T, Tsuji N.Acta Mater, 2007; 55: 5873 | | [13] | Sakai T, Hamada S, Saito Y.Scr Mater, 2001; 44: 2569 | | [14] | Pérez-Prado M T, Del Valle J A, Ruano O A.Scr Mater, 2004; 51: 1093 | | [15] | Zhan M Y, Li Y Y, Chen W P, Chen W D.J Mater Sci, 2007; 42: 9256 | | [16] | Jiang L, Pérez-Prado M T, Gruber P A, Arzt E, Ruano O A, Kassner M E.Acta Mater, 2008; 56: 1228 | | [17] | Terada D, Inoue S, Tsuji N.J Mater Sci, 2007; 42: 1673 | | [18] | Del Valle J A, Pérez-Prado M T, Ruano O A. Mater Sci Eng, 2005; A410-411: 353 | | [19] | Pérez-Prado M T, Del Valle J A, Ruano O A.Scr Mater, 2004; 50: 667 | | [20] | Chang H, Zheng M Y, Wu K, Gan W M, Tong L B, Brokmeier H G.Mater Sci Eng, 2010; A527: 7176 | | [21] | Ion S E, Humpreys F J, White S H.Acta Mater, 1982; 30: 1909 | | [22] | Del Valle J A, Pérez-Prado M T, Ruano O A.Mater Sci Eng, 2003; A355: 68 | | [23] | Barnett M R, Nave M D, Bettles C J.Mater Sci Eng, 2004; A386: 205 | | [24] | Huang X S, Suzuki K, Watazu A, Shigematsu I, Satio N.J Alloys Compd, 2008; 457: 408 | | [25] | Kamikawa N, Tsuji N, Minamino Y.Sci Technol Adv Mater, 2004; 5: 163 | | [26] | Li S, Sun F, Li H.Acta Mater, 2010; 58: 1317 | | [27] | Skrotzki W, Hunsche I, Huttenrauch J, Oertel C G, Brokmeier H G, Hoppel H W, Topic I.Textures and Microstructures, 2008; 8: 1 | | [28] | Raei M, Toroghinejad M R, Jamaati R, Szpunar J A.Mater Sci Eng, 2010; A527: 7068 | | [29] | Chang H.PhD Dissertation, Harbin Institute of Technology, 2011 | | [29] | (常海. 哈尔滨工业大学博士学位论文, 2011) | | [30] | Humphreys F J, Hatherly M.Recrystallization and Related Annealing Phenomena. 2nd Ed., Oxford: Elsevier Science Ltd, 2004: 1 | | [31] | Chang H, Zheng M Y, Xu C, Fan G D, Brokmeier H G, Wu K.Mater Sci Eng, 2012; A543: 249 | | [32] | Gatti J R, Bhattacharjee P P.J Mater Eng Perform, 2014; 23: 4453 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|