| 不同浓度富Fe相粒子对Al-Mg-Si-Cu系合金弯边性能的影响* |
邢辉,郭明星( ),汪小锋,张艳,张济山,庄林忠 |
| 北京科技大学新金属材料国家重点实验室, 北京 100083 |
|
| EFFECT OF Fe-RICH PHASE PARTICLES WITH DIFFER-ENT CONCENTRATIONS ON THE BENDABILITYOF Al-Mg-Si-Cu SERIES ALLOYS |
Hui XING,Mingxing GUO( ),Xiaofeng WANG,Yan ZHANG,Jishan ZHANG,Linzhong ZHUANG |
| State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
邢辉, 郭明星, 汪小锋, 张艳, 张济山, 庄林忠. 不同浓度富Fe相粒子对Al-Mg-Si-Cu系合金弯边性能的影响*[J]. 金属学报, 2016, 52(3): 271-280.
Hui XING,
Mingxing GUO,
Xiaofeng WANG,
Yan ZHANG,
Jishan ZHANG,
Linzhong ZHUANG.
EFFECT OF Fe-RICH PHASE PARTICLES WITH DIFFER-ENT CONCENTRATIONS ON THE BENDABILITYOF Al-Mg-Si-Cu SERIES ALLOYS[J]. Acta Metall Sin, 2016, 52(3): 271-280.
| [1] | Miller W S, Zhuang L, Bottema J, Wittebrood A J, De Smet P, Haszler A, Vieregge A.Mater Sci Eng, 2000; A280: 37 | | [2] | Wang D.Shanghai Nonferrous Met, 2013; 34(3): 130 | | [2] | (王丹. 上海有色金属, 2013; 34(3): 130) | | [3] | Wang M J, Huang D Y, Jiang H T.Heat Treatment Met, 2006; (09): 34 | | [3] | (王孟君, 黄电源, 姜海涛. 金属热处理, 2006; (09): 34) | | [4] | Sun J.Tech Educ, 2010; (02): 26 | | [4] | (孙静. 技术与教育, 2010; (02): 26) | | [5] | Liu Y W, Wang S W.Auto Engineer, 2011; (02): 50 | | [5] | (刘伟燕, 王书伟. 汽车工程师, 2011; (02): 50) | | [6] | Zhang Q X, Guo M X, Hu X Q, Cao L Y, Zhuang L Z, Zhang J S.Acta Metall Sin, 2013; 49: 1604 | | [6] | (张巧霞, 郭明星, 胡晓倩, 曹零勇, 庄林忠, 张济山. 金属学报, 2013; 49: 1604) | | [7] | Cui L, Guo M X, Peng X Y, Zhang Y, Zhang J S, Zhuang L Z.Acta Metall Sin, 2015; 51: 289 | | [7] | (崔莉, 郭明星, 彭祥阳, 张艳, 张济山, 庄林忠. 金属学报, 2015; 51: 289) | | [8] | Wang A D. Master Thesis, Dalian University of Technology, 2011 | | [8] | (王安东. 大连理工大学硕士学位论文, 2011) | | [9] | Wang X F, Guo M X, Cao L Y, Luo J R, Zhang J S, Zhuang L Z.Mater Sci Eng, 2015; A621: 8 | | [10] | Sarkar J, Kutty T R G, Wilkinson D S, Embury J D, Lloyd D J.Mater Sci Eng, 2004; A369: 258 | | [11] | Itoh G, Suzuki T, Horikawa K. Mater Sci Forum, 2002; 396-402: 1193 | | [12] | Hirth S M, Marshall G J, Court S A, Lloyd D J. Mater Sci Eng, 2001; A319-321: 452 | | [13] | Datsko J, Yang C T.J Eng Ind, 1960; 82: 309 | | [14] | Davidkov A, Petrov R H, Smet P D, Schepers B, Kestens L A I.Mater Sci Eng, 2011; A528: 7068 | | [15] | Castany P, Diologent F, Rossoll A, Despois J F, Bezen?on C, Mortensen A.Mater Sci Eng, 2013; A559: 558 | | [16] | Mulazimoglu M, Zaluska A, Gruzleski J, Paray F.Metall Mater Trans, 1996; 27A: 929 | | [17] | Allen C M, O'Reilly K A Q, Cantor B, Evans P V.Prog Mater Sci, 1998; 43: 89 | | [18] | Tanihata H, Sugawara T, Matsuda K, Ikeno S.J Mater Sci, 1999; 34: 1205 | | [19] | Couper M J, Rinderer B, Yao J Y. Mater Sci Forum, 2006; 519-521: 303 | | [20] | Peng X Y, Guo M X, Wang X F, Cui L, Zhang J S, Zhuang L Z.Acta Metall Sin, 2015; 51: 169 | | [20] | (彭祥阳, 郭明星, 汪小锋, 崔莉, 张济山, 庄林忠. 金属学报, 2015; 51: 169) | | [21] | Wang X F, Guo M X, Chapuis A, Luo J R, Zhang J S, Zhuang L Z.Mater Sci Eng, 2015; A644: 137 | | [22] | Lievers W B, Pilkey A K, Worswick M J.Mech Mater, 2003; 35: 661 | | [23] | Lloyd D J, Weatherly G C, Perovic D D.In: Subodh K Das ed., Proceedings of Symposium: Automotive Alloys 1999, San Diego: TMS, 2000: 211 | | [24] | Lv D. Master Thesis, Lanzhou University of Technology, 2009 | | [24] | (吕丹. 兰州理工大学硕士学位论文, 2009) | | [25] | Fan X G.PhD Dissertation, Harbin Institute of Technology, 2007 | | [25] | (樊喜刚. 哈尔滨工业大学博士学位论文, 2007) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|