| 介质阻挡放电等离子体辅助球磨及其在材料制备中的应用* |
朱敏1,2( ),鲁忠臣2,3,胡仁宗1,2,欧阳柳章1,2 |
1 华南理工大学材料科学与工程学院, 广州 510640
2 华南理工大学广东省先进储能材料重点实验室, 广州 510640
3 华南理工大学机械与汽车工程学院, 广州 510640 |
|
| DIELECTRIC BARRIER DISCHARGE PLASMA ASSISTED BALL MILLING TECHNOLOGY AND ITS APPLICATIONS IN MATERIALS FABRICATION |
Min ZHU1,2( ),Zhongchen LU2,3,Renzong HU1,2,Liuzhang OUYANG1,2 |
1 School of Materials Science and Engineering, South China University of Technology, Guangzhou 510640, China
2 Key Laboratory of Advanced Energy Storage Materials of Guangdong Province, South China University of Technology, Guangzhou 510640, China
3 School of Mechanical and Automotive Engineering, South China University of Technology, Guangzhou 510640, China |
引用本文:
朱敏, 鲁忠臣, 胡仁宗, 欧阳柳章. 介质阻挡放电等离子体辅助球磨及其在材料制备中的应用*[J]. 金属学报, 2016, 52(10): 1239-1248.
Min ZHU,
Zhongchen LU,
Renzong HU,
Liuzhang OUYANG.
DIELECTRIC BARRIER DISCHARGE PLASMA ASSISTED BALL MILLING TECHNOLOGY AND ITS APPLICATIONS IN MATERIALS FABRICATION[J]. Acta Metall Sin, 2016, 52(10): 1239-1248.
| [1] | Benjamin J S.Metall Trans, 1970; 1: 2943 | | [2] | Koch C C.Nanostruct Mater, 1993; 2: 109 | | [3] | Dai L Y, Chen Q L, Lin S F, Ouyang L Z.Mater Rev, 2009; 23(2): 59 | | [3] | (戴乐阳, 陈清林, 林少芬, 欧阳柳章. 材料导报, 2009; 23(2): 59) | | [4] | Dai L Y, Zeng M Q, Tong Y Q, Ouyang L Z, Zhu M, Li Y Y.J Funct Mater, 2005; 36: 1158 | | [4] | (戴乐阳, 曾美琴, 童燕青, 欧阳柳章, 朱敏, 李元元. 功能材料, 2005; 36: 1158) | | [5] | Mordyuk B N, Prokopenko G I.Ultrasonics, 2004; 42: 43 | | [6] | Calka A, Radlinski A P.Mater Sci Eng, 1991; A134: 1350 | | [7] | Wang D P, Li X D, Chang Y, Qi M.J Rare Earth (Engl Lett), 2013; 31: 366 | | [8] | Chelvane J A, Palit M, Basumatary H, Pandian S.J Magn Magn Mater, 2013; 343: 144 | | [9] | Luton M J, Jayanth C S, Disko M M, Matrasa1 S, Vallon J. In: Kear B H, McCandlish L E, Polk D E, Siegel R W eds., MRS Proceedings, Cambridge University Press, 1988; 132: 79 | | [10] | Chung K H, He J H, Shin D H.Mater Sci Eng, 2003; A356: 23 | | [11] | Calka A, Wexler D.Nature, 2002; 419: 147 | | [12] | Calka A, Wexler D.J Metastable Nanocryst Mater, 2004; 20: 111 | | [13] | Mosbah A, Calka A, Wexler D.J Alloys Compd, 2006; 424: 279 | | [14] | Varin R A, Chiu C, Li S, Calka A, Wexler D.J Alloys Compd, 2004; 370: 230 | | [15] | Calka A, Mosbah A, Stanford N, Balaz P.J Alloys Compd, 2008; 455: 285 | | [16] | Needham S A, Calka A, Wang G X, Mosbah A, Liu H K.Electochem Commun, 2006; 8: 434 | | [17] | Yuan Q, Zheng Y, Yu H.Int J Refract Met Hard Mater, 2009; 27: 121 | | [18] | Quan Y, Zheng Y, Yu H Z.Trans Nonferrous Met Soc China, 2011; 21: 1545 | | [19] | Zhu M, Dai L Y, Cao B, Zeng M Q, Ouyang L Z, Tong Y Q, Li B.China Patent, ZL200510036231, 2007) | | [19] | (朱敏, 戴乐阳, 曹彪, 曾美琴, 欧阳柳章, 童燕青, 李北. 中国专利, ZL200510036231, 2007) | | [20] | Wang X X.High Volt Eng, 2009; 35(1): 1 | | [20] | (王新新. 高电压技术, 2009; 35(1): 1) | | [21] | Yang X P, Dai L Y, Zeng M Q, Ouyang L Z.Mater Rev, 2010; 24: 320 | | [21] | (杨小平, 戴乐阳, 曾美琴, 欧阳柳章. 材料导报, 2010; 24: 320) | | [22] | Sun Q D.Master Thesis, Tianjin University, 2013 | | [22] | (孙启迪. 天津大学硕士学位论文, 2013) | | [23] | Dai L Y, Lin S F, Chen Q L, Yang X P.Mod Manuf Eng, 2010; 5(5): 48 | | [23] | (戴乐阳, 林少芬, 陈清林, 杨小平. 现代制造工程, 2010; 5(5): 48) | | [24] | Dai L Y.PhD Dissertation, South China University of Technology, Guangzhou, 2006 | | [24] | (戴乐阳, 华南理工大学博士学位论文, 广州, 2006) | | [25] | Zhu M, Dai L Y, Gu N S, Cao B, Ouyang L Z.J Alloys Compd, 2009; 478: 624 | | [26] | Dai L Y.Acta Metall Sin (Engl Lett), 2013; 26: 63 | | [27] | Dai L Y, Cao B, Zhu M.Acta Metall Sin (Engl Lett), 2006; 19: 411 | | [28] | Conrad H, Yang D.Acta Mater, 2002; 50: 2851 | | [29] | Chen Z H.Master Thesis, South China University of Technology, Guangzhou, 2015 | | [29] | (陈志鸿. 华南理工大学硕士学位论文, 广州, 2015) | | [30] | Jia C X, Chen P, Wang Q, Wang J, Ren R.Chin J Mater Res, 2015; 29: 10 | | [30] | (贾彩霞, 陈平, 王乾, 王静, 任荣. 材料研究学报, 2015; 29: 10) | | [31] | Meng R G.Master Thesis, Jimei University, Xiamen, 2013 | | [31] | (孟荣刚. 集美大学硕士学位论文, 厦门, 2013) | | [32] | Yang X P.Master Thesis, South China University of Technology, Guangzhou, 2010 | | [32] | (杨小平. 华南理工大学硕士学位论文, 广州, 2010) | | [33] | Dai L Y, Lin S F, Chen J F, Zeng M Q, Zhu M.Int J Refract Met Hard Mater, 2012; 30: 48 | | [34] | Zhu M, Bao X Y, Yang X P, Gu N S, Wang H, Zeng M Q, Dai L Y.Metall Mater Trans, 2011; 42: 2930 | | [35] | Wang W, Lu Z C, Chen Z H, Zeng M Q, Wang H, Zhu M.J Rare Earth (Engl Lett), DOI: 10.1007/S12598-016-0769-5 | | [36] | Hu R Z, Yang L C, Zhu M.Chin Sci Bull (Chin Ver), 2013; 58: 3140 | | [36] | (胡仁宗, 杨黎春, 朱敏. 科学通报(中文版), 2013; 58: 3140) | | [37] | Hu R Z.PhD Dissertation, South China University of Technology, Guangzhou, 2011 | | [37] | (胡仁宗. 华南理工大学博士学位论文, 广州, 2011) | | [38] | Liu H, Hu R, Zeng M, Liu J W, Zhu M.J Mater Chem, 2012; 22A: 8022 | | [39] | Hui L, Hu R Z, Sun W, Zeng M Q, Yang L C, Liu J W, Zhu M,J Power Sources, 2013; 242: 114 | | [40] | Zhang H Y, Hu R Z, Liu H, Sun W, Lu Z C, Liu J W, Yang L C, Zhang Y, Zhu M.J Mater Chem, 2016; 4A: 10321 | | [41] | W. Sun, R.Z.Hu, H. Liu, M. Q. Zeng, M. Zhu.J Power Sources, 2014; 268:610 | | [42] | Ouyang L Z, Guo L N, Cai W H, Ye J S, Hu R Z, Liu J W, Yang LC, Zhu M.J Mater Chem A, 2014; 2A: 11280 | | [43] | Wang Y K, Yang L C, Hu R Z, Sun W, Liu J W, Ouyang L Z, Yuan B, Wang H, Zhu M.J Power Sources, 2015; 288: 314 | | [44] | Zaluska A, Zaluski L, Str?m-Olsen J O.J Alloys Compd, 1999; 288: 217 | | [45] | Huot J, Tremblay M L, Schulz R.J Alloys Compd, 2003; 356: 603 | | [46] | Lu Y S, Zhu M, Wang H, Li Z M, Ouyang L Z, Liu J W.Int J Hydrogen Energy, 2014; 39: 14033 | | [47] | Ouyang L Z, Cao Z J, Wang H, Liu J W, Sun D L, Zhang Q A, Zhu M.J Alloys Compd, 2014; 586: 113 | | [48] | Cao Z J, Ouyang L Z, Wu Y, Wang H, Liu J W, Fang F, Sun D L, Zhang Q A, Zhu M.Dual-tuning effects of In, Al, and Ti on the thermodynamics and kinetics of Mg85In5Al5Ti5 alloy synthesized by plasma milling.J Alloys Compd, 2015; 623: 354 | | [49] | Ouyang L Z, Cao Z J, Li L L, Wang H, Liu J W, Min D, Chen Y W, Xiao F M, Tang R H, Zhu M.Int J Hydrogen Energy, 2014; 39: 12765 | | [50] | Dai L Y, Zhang B J, Lin S F, Liu Z J, Wang W C.Chin J Nonferrous Met, 2015; 1: 171 | | [50] | (戴乐阳, 张宝剑, 林少芬, 刘志杰, 王文春. 中国有色金属学报, 2015; 1: 171) |
|
|