| 核用新型耐高温、抗辐照、耐液态金属腐蚀结构材料——SIMP钢的研究进展* |
杨柯1( ),严伟1,王志光2,单以银1,石全强1,史显波1,王威1 |
1 中国科学院金属研究所, 沈阳 110016
2 中国科学院近代物理研究所, 兰州 730000 |
|
| DEVELOPMENT OF A NOVEL STRUCTURAL MATERIAL (SIMP STEEL) FOR NUCLEAR EQUIPMENT WITH BALANCED RESIS-TANCES TO HIGH TEMPERATURE, RADIATION AND LIQUID METAL CORROSION |
Ke YANG1( ),Wei YAN1,Zhiguang WANG2,Yiyin SHAN1,Quanqiang SHI1,Xianbo SHI1,Wei WANG1 |
1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
2 Institute of Modern Physics, Chinese Academy of Sciences, Lanzhou 730000, China |
引用本文:
杨柯, 严伟, 王志光, 单以银, 石全强, 史显波, 王威. 核用新型耐高温、抗辐照、耐液态金属腐蚀结构材料——SIMP钢的研究进展*[J]. 金属学报, 2016, 52(10): 1207-1221.
Ke YANG,
Wei YAN,
Zhiguang WANG,
Yiyin SHAN,
Quanqiang SHI,
Xianbo SHI,
Wei WANG.
DEVELOPMENT OF A NOVEL STRUCTURAL MATERIAL (SIMP STEEL) FOR NUCLEAR EQUIPMENT WITH BALANCED RESIS-TANCES TO HIGH TEMPERATURE, RADIATION AND LIQUID METAL CORROSION[J]. Acta Metall Sin, 2016, 52(10): 1207-1221.
| [1] | Team of Strategic Priority Program on ADS Transmutation System of Advanced Fission Energy.Bull Chin Acad Sci, 2015; (4): 527 | | [1] | (中国科学院"未来先进核裂变能—ADS嬗变系统"战略性先导科技专项研究团队. 中国科学院院刊, 2015; (4): 527) | | [2] | Yeliseyeva O, Tsisar V, Benamati G.Corros Sci, 2008; 50: 1672 | | [3] | Martinelli L, Balbaud-Célérier F, Terlain A, Delpech S, Santarini G, Favergeon J, Moulin G, Tabarant M, Picard G.Corros Sci, 2008; 50: 2523 | | [4] | Martinelli L, Balbaud-Célérier F, Terlain A, Bosonnet S, Picard G, Santarini G.Corros Sci, 2008; 50: 2537 | | [5] | Martinelli L, Balbaud-Célérier F.Mater Corros, 2011; 62: 531 | | [6] | Schroer C, Konys J.J Eng Gas Turbines Power, 2010; 132: 082 | | [7] | Klueh R L, Harries D R.High-Chromium Ferritic and Martensitic Steels for Nuclear Applications. ASTM West Conshohocken, PA: American Society for Testing and Materials, 2001: 1 | | [8] | Klueh R, Nelson A.J Nucl Mater, 2007; 371: 37 | | [9] | Chen Y X, Yan W, Hu P, Shan Y Y, Yang K.Acta Metall Sin, 2011; 11: 1372 | | [9] | (陈云翔, 严伟, 胡平, 单以银, 杨柯. 金属学报, 2011; 11: 1372) | | [10] | Hu P, Yan W, Sha W, Wang W, Shan Y Y, Yang K.J Mater Sci Technol, 2011; 27: 344 | | [11] | Chen X Z, Shen Z, Chen X, Lei Y C, Huang Q Y.Fusion Eng Des, 2011; 86: 2943 | | [12] | Huang Q Y, Li C J, Wu Q S, Liu S J, Gao S, Guo Z H, Yan Z L, Huang B, Yong S, Zhu Z Q, Chen Y P, Ling X X, Wu Y C.J Nucl Mater, 2011; 417: 85 | | [13] | Peng L, Huang Q Y, Li C J, Liu S J. J Nucl Mater, 2009; 386-388: 312 | | [14] | Huang Q, Li J G, Chen Y X. J Nucl Mater, 2004; 329-333: 268 | | [15] | Huang L X, Hu X, Yang C G, Yan W, Xiao F R, Shan Y Y, Yang K.J Nucl Mater, 2013; 443: 479 | | [16] | Hu X, Huang L X, Yan W, Wang W, Sha W, Shan Y Y, Yang K.Mater Sci Eng, 2014; A613: 404 | | [17] | Hu X, Huang L X, Yan W, Wang W, Sha W, Shan Y Y, Yang K.Mater Sci Eng, 2013; A586: 253 | | [18] | Hu X, Huang L X, Wang W G, Yang Z G, Sha W, Wang W, Yan W, Shan Y Y.Fusion Eng Des, 2013; 88: 3050 | | [19] | Lindau R, M?slang A, Rieth M, Klimiankou M, Materna-Morris E, Alamo A, Tavassoli A A F, Cayron C, Lancha A M, Fernandez P, Baluc N, Sch?ublin R, Diegele E, Filacchioni G, Rensman J W, van der Schaaf B, Lucon E, Dietz W. Fusion Eng Des, 2005; 75-79: 989 | | [20] | Lindau R, M?slang A, Schirra M. Fusion Eng Des, 2002; 61-62: 659 | | [21] | Lucon E, Decréton M, van Walle E.Fusion Eng Des, 2003; 69: 373 | | [22] | Lucon E, Vandermeulen W. J Nucl Mater, 2009; 386-388: 254 | | [23] | Marmy P, Kruml T.J Nucl Mater, 2008; 377: 52 | | [24] | Tong Z, Dai Y.J Nucl Mater, 2010; 398: 43 | | [25] | Wang J, Lu S P, Dong W C, Li D Z, Rong L J.Mater Des, 2014; 64: 550 | | [26] | Stubbins J F, Gelles D S. J Nucl Mater, 1996; 233-237: 331 | | [27] | Lapena J, Garcia-Mazario M, Fernandez P, Lancha A M. J Nucl Mater, 2000; 283-287: 662 | | [28] | Nishimura A, Nagasaka T, Inoue N, Muroga T, Namba C. J Nucl Mater, 2000; 283-287: 677 | | [29] | Li H L, Nishimura A, Li Z X, Nagasaka T, Muroga T.Fusion Eng Des, 2006; 81: 241 | | [30] | Li Y F, Nagasaka T, Muroga T, Huang Q Y, Wu Y C. J Nucl Mater, 2009; 386-388: 495 | | [31] | Eliseeva O, Tsisar V, Fedirko V, Matychak Y S.Mater Sci, 2004; 40: 260 | | [32] | Eliseeva O I, Tsisar V P.Mater Sci, 2007; 43: 230 | | [33] | Huntz A M, Bague V, Beauple G, Haut C, Severac C, Lecour P, Longaygue X, Ropital F.Appl Surf Sci, 2003; 207: 255 | | [34] | Panait C G, Bendick W, Fuchsmann A, Gourgues-Lorenzon A F, Besson J.Int J Pressure Vessels Piping, 2010; 87: 326 | | [35] | Aghajani A, Somsen C, Eggeler G.Acta Mater, 2009; 57: 5093 | | [36] | Abd El-Azim M E, Ibrahim O H, El-Desoky O E.Mater Sci Eng, 2013; A560: 678 | | [37] | Taneike M, Fujitsuna N, Abe F.Mater Sci Technol, 2004; 20: 1455 | | [38] | Cerjak H, Hofer P, Schaffernak B.ISIJ Int, 1999; 39: 874 | | [39] | Yong Q L.Secondary Phases in Steels. Beijing: Metallurgical Industry Press, 2006: 433 | | [39] | (雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 433) | | [40] | Shi Q Q, Liu J, Wang W, Yan W, Shan Y Y, Yang K.Oxid Met, 2015; 83: 521 | | [41] | Niu Y, Wang S, Gao F, Zhang Z G, Gesmundo F.Corros Sci, 2008; 50: 345 | | [42] | Asteman H, Spiegel M.Corros Sci, 2008; 50: 1734 | | [43] | Stott F H, Wei F I.Oxid Met, 1989; 31: 369 | | [44] | Babu N, Balasubramaniam R, Ghosh A.Corros Sci, 2001; 43: 2239 | | [45] | Abderrazik G B, Moulin G, Huntz A, Young E.Solid State Ionics, 1987; 22: 285 | | [46] | Nychka J, Clarke D.Oxid Met, 2005; 63: 325 | | [47] | Mougin J, Dupeux M, Antoni L, Galerie A.Mater Sci Eng, 2003; A359: 44 | | [48] | Li M S.High Temperature Corrosion of Metal. Beijing: Metallurgical Industry Press, 2001: 1 | | [48] | (李美栓. 金属的高温腐蚀. 北京: 冶金工业出版社, 2001: 1) | | [49] | Kaur I, Gust W.Fundamentals of Grain and Interphase Boundary Diffusion. Stuttgart: Ziegler Press, 1988: 1 | | [50] | Tortorici P C, Dayananda M.Mater Sci Eng, 1998; A244: 207 | | [51] | Pint B A, Wright I G. Mater Sci Forum, 2004; 461-464: 799 | | [52] | Deacon R M, DuPont J, Kiely C, Marder A, Tortorelli P.Oxid Met, 2009; 72: 87 | | [53] | Airiskallio E, Nurmi E, Heinonen M H, Vayrynen I J, Kokko K, Ropo M, Punkkinen M P J, Pitkanen H, Alatalo M, Kollar J, Johansson B, Vitos L.Corros Sci, 2010; 52: 3394 | | [54] | Stott F H, Wei F I.Oxid Met, 1989; 31: 369 | | [55] | Mikkelsen L, Linderoth S, Bilde-S?rensen J. Mater Sci Forum, 2004; 461-464: 117 | | [56] | Pettersson R, Liu L, Sund J.Corros Eng Sci Technol, 2005; 40: 211 | | [57] | Bamba G, Wouters Y, Galerie A, Charlot F, Dellali A.Acta Mater, 2006; 54: 3917 | | [58] | Truman J E, Pirt K R.Corros Sci, 1976; 16: 103 | | [59] | Ishitsuka T, Inoue Y, Ogawa H.Oxid Met, 2004; 61: 125 | | [60] | Robertson J, Manning M I.Mater Sci Technol, 1989; 5: 741 | | [61] | Wang S, Wu Y, Ni C S, Niu Y.Corros Sci, 2009; 51: 511 | | [62] | Horita T, Kishimoto H, Yamaji K, Sakai N, Xiong Y, Brito M E, Yokokawa H.J Power Sources, 2006; 157: 681 | | [63] | Horita T, Yamaji K, Yokokawa H, Toji A, Uehara T, Ogasawara K, Kameda H, Matsuzaki Y, Yamashita S.Int J Hydrogen Energy, 2008; 33: 6308 | | [64] | Liu S, Tang D, Wu H B, Wang L D.J Mater Process Technol, 2013; 213: 1068 | | [65] | Paúl A, Elmrabet S, Alves L C, da Silva M F, Soares J C, Odriozola J A.Nucl Instrum Methods Phys Res, 2001; 181B: 394 | | [66] | Riffard F, Buscail H, Caudron E, Cueff R, Issartel C, Perrier S.Mater Charact, 2002; 49: 55 | | [67] | Li B, Gleeson B.Oxid Met, 2006; 65: 101 | | [68] | Trindade V B, Krupp U, Hanjari B Z, Yang S, Christ H J.Mater Res, 2005; 8: 371 | | [69] | Steiner H.J Nucl Mater, 2009; 383: 267 | | [70] | Eriko Y, Kevin G, Laure M.Corros Sci, 2011; 53: 3075 | | [71] | Schroer C, Skrypnik A, Wedemeyer O, Konys J.Corros Sci, 2012; 61: 63 | | [72] | Schroer C, Wedemeyer O, Novotny J, Skrypnik A, Konys J.Corros Sci, 2014; 84: 113 | | [73] | Cathcart J V, Manly W D.Corrosion, 1956; 12: 43 | | [74] | Malkow T, Steiner H, Muscher H, Konys J.J Nucl Mater, 2004; 335: 199 | | [75] | Marino A, Lim J, Keijers S, Van den Bosch J, Deconinck J.Nucl Eng Des, 2013; 265: 576 | | [76] | Blacha L, Mizera J, Folega P.Metalurgija, 2014; 53: 51 | | [77] | Koury D, Johnson A L, Welch J, Farley J W.J Nucl Mater, 2012; 429: 210 | | [78] | Shankar Rao V, Lim J, Hwang I S, Singhal L K.Corros Sci, 2012; 63: 113 | | [79] | Susmikanti M, Andiwijayakusuma D, Ghofir, Maulana A.In: Su'ud Z, Waris A eds., The 3rd Int Conf on Advances in Nuclear Science and Engineering, Melville: Amer Inst Physic, 2012: 185 | | [80] | Hosemann P, Dickerson R, Dickerson P, Li N, Maloy S A.Corros Sci, 2013; 66: 196 | | [81] | Lambrinou K, Koch V, Coen G, Van den Bosch J, Schroer C.J Nucl Mater, 2014; 450: 244 | | [82] | Kondo M, Takahashi M, Miura K, Onizawa T.J Nucl Mater, 2006; 357: 97 | | [83] | Brissonneau L, Beauchamp F, Morier O, Schroer C, Konys J, Kobzova A, Di Gabriele F, Courouau J L.J Nucl Mater, 2011; 415: 348 | | [84] | Ganesan R, Gnanasekaran T, Srinivasa R S.J Nucl Mater, 2006; 349: 133 | | [85] | Lim J, Manfredi G, Gavrilov S, Rosseel K, Aerts A, Van den Bosch J.Sens Actuators, 2014; 204B: 388 | | [86] | Li N.J Nucl Mater, 2002; 300: 73 | | [87] | Ilincev G, Karnik D, Paulovic M, Doubkova A.Nucl Eng Des, 2006; 236: 1909 | | [88] | Viswanathan R, Sarver J, Tanzosh J M.J Mater Eng Perform, 2006; 15: 255 | | [89] | Fry A, Osgerby S, Wright M.Comp Methods Appl Mech Eng, 2002; 85: 374 | | [90] | Ren X, Sridharan K, Allen T R.Mater Corros, 2010; 61: 748 | | [91] | Bischoff J, Motta A T, Comstock R J.J Nucl Mater, 2009; 392: 272 | | [92] | Shi Q Q, Liu J, Luan H, Yang Z G, Wang W, Yan W, Shan Y Y, Yang K.J Nucl Mater, 2015; 457: 135 | | [93] | Birks N, Meier G H, Pettit F S.Introduction to the High Temperature Oxidation of Metals. New York: Cambridge University Press: 2006: 1 | | [94] | Martinelli L, Balbaud-Celerier F, Terlain A, Bosonnet S, Picard G, Santarini G.Corros Sci, 2008; 50: 2537 | | [95] | Bischoff J, Motta A T.J Nucl Mater, 2012; 424: 261 | | [96] | Liu J, Shi Q Q, Luan H, Yan W, Sha W, Wang W, Shan Y Y, Yang K.Mater Sci Eng, 2016; A670: 97 | | [97] | Wang J, Gao X, Wang Z G, Wei K F, Yao C F, Cui M H, Sun J R, Li B S, Pang L L, Zhu Y B, Luo P, Chang H L, Zhang H P, Zhu H P, Wang D, Du Y Y, Xie E Q.Chin Phys Lett, 2015; 32(7): 076101 | | [98] | Wang J, Gao X, Gao N, Wang Z G, Cui M H, Wei K F, Yao C F, Sun J R, Li B S, Zhu Y B, Pang L L, Li Y F, Wang D, Xie E Q.J Nucl Mater, 2015; 457: 182 | | [99] | Zhu H P, Wang Z G, Gao X, Cui M H, Li B S, Sun J R, Yao C F, Wei K F, Shen T L, Pang L L.Nucl Instrum Meth, 2015; 344B: 5 | | [100] | Zhu H P, Wang Z G, Cui M H, Li B S, Gao X, Sun J R, Yao C F, Wei K F, Shen T L, Pang L L, Zhu Y B, Li Y F, Wang J, Xie E Q.Appl Surf Sci, 2015; 326: 1 | | [101] | Li Y F, Shen T L, Gao Xing, Yao C F, Wei K F, Sun J R, Li B S, Zhu Y B, Pang L L, Cui M H, Chang H L, Wang J, Zhu H P, Hu B T, Wang Z G.Chin Phys Lett, 2013; 30: 126101 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|