Man YAO1( ),Wei CUI1,Xudong WANG1,Haixuan XU2,S R PHILLPOT3 |
1 School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024
2 Department of Materials Science and Engineering, University of Tennessee, Knoxiville, TN37996, USA
3 Department of Materials Science and Engineering, University of Florida, Gainesville, FL 32611, USA |
引用本文:
姚曼, 崔薇, 王旭东, 徐海譞, PHILLPOT S R. W辐照损伤初期的分子动力学研究*[J]. 金属学报, 2015, 51(6): 724-732.
Man YAO,
Wei CUI,
Xudong WANG,
Haixuan XU,
S R PHILLPOT.
MOLECULAR DYNAMICS SIMULATION OF INITIAL RADIATION DAMAGE IN TUNGSTEN[J]. Acta Metall Sin, 2015, 51(6): 724-732.
| [1] | Bolt H, Barabash V, Federici G, Linke J, Loarte A, Roth J, Sato K. J Nucl Mater, 2002; 307: 43 | | [2] | Borovikov V, Tang X Z, Perez D, Bai X M, Uberuaga B P, Voter A F. J Phys—Condens Matter, 2013; 25: 035402 | | [3] | Troev T, Nankov N, Yoshiie T. Nucl Instr Meth, 2011; 269B: 566 | | [4] | Rieth M, Dudarev S L, Gonzalez de Vicente S M, Aktaa J, Ahlgren T, Antusch S, Palacios T. J Nucl Mater, 2013; 432: 482 | | [5] | He X F, Yang W, Fan S. Acta Phys Sin, 2009; 58: 8657 (贺新福, 杨 文, 樊 胜. 物理学报, 2009; 58: 8657) | | [6] | Guinan M W, Kinney J H. J Nucl Mater, 1981; 103-104: 1319 | | [7] | Xu Q, Yoshiie T, Huang H C. Nucl Instr Meth, 2003; 206B: 123 | | [8] | Li M, Cui J C, Wang J, Hou Q. J Nucl Mater, 2013; 433: 17 | | [9] | Caturla M J, Diaz de la Rubia T, Victoria M, Corzine R K, James M R, Greene G A. J Nucl Mater, 2001; 296: 90 | | [10] | Troev T, Popov E, Staikov P, Nankov N, Yoshiie T. Nucl Instr Meth, 2009; 267B: 535 | | [11] | Park N Y, Kim Y C, Seok H K, Han S H, Cho S, Cha P R. Nucl Instr Meth, 2007; 265B: 47 | | [12] | Fu B Q, Xu B, Lai W S, Yuan Y, Xu H Y, Li C, Jia Y Z, Liu W. J Nucl Mater, 2013; 441: 24 | | [13] | Biersack J P, Ziegler J F. Nucl Instrum Methods Phys Res, 1982; 194: 93 | | [14] | Lee B J, Baskes M I, Kim H, Yang K C. Phys Rev, 2001; 64B: 184102 | | [15] | Yao M, Gao X, Zeng W P, Wang X D, Xu H X, Phillpot S R. Acta Metall Sin, 2013; 49: 530 (姚 曼, 高 晓, 曾维鹏, 王旭东, 徐海譞, Phillpot S R. 金属学报, 2013; 49: 530) | | [16] | Xu H X. From Electronic Structure of Point Defects to Physical Properties of Complex Materials Using Atomic-level Simulations. Gainesville: University of Florida, 2010: 148 | | [17] | Bacon D J, Calder A F, Gao F, Kapinos V G, Wooding S J. Nucl Instr Meth, 1995; 102B: 37 | | [18] | Norgett M J, Robinson M T, Torrens I M. Nucl Eng Des, 1975; 33: 50 | | [19] | Bj?rkas C, Nordlund K, Dudarev S. Nucl Instr Meth, 2009; 267B: 3204 | | [20] | Bacon D J, Gao F, Osetsky Y N. J Nucl Mater, 2000; 276: 1 | | [21] | Wooding S J, Bacon D J, Phythian W J. Philos Mag, 1995; 72A: 1261 | | [22] | Fikar J, Schaeublin R. Nucl Instr Meth, 2007; 255B: 27 | | [23] | Gao F, Bacon D J, Flewitt P E J, Lewis T A. J Nucl Mater, 1997; 249: 77 | | [24] | Derlet P M, Nguyen-Manh D, Dudarev S L. Phys Rev, 2007; 76B: 054107 | | [25] | Fikar J, Schaeublin R. J Nucl Mater, 2009; 386-388: 97 | | [26] | Nguyen-Manh D, Horsfield A P, Dudarev S L. Phys Rev, 2006; 73B: 020101 | | [27] | Bai X M, Voter A F, Hoagland R G, Nastasi M, Uberuaga B P. Science, 2010; 327: 1631 | | [28] | Vajda P, Biget M, Lucasson A, Lucasson P. J Phys, 1977; 7F: L123 | | [29] | Maury F, Biget M, Vajda P, Lucasson A, Lucasson P. Radiat Eff Defects Solids, 1978; 38: 53 | | [30] | Sigle W, Seeger A. Phys Status Solidi, 1994; 146A: 57 | | [31] | Zepeda-Ruiz L A, Han S, Srolovitz D J, Car R, Wirth B D. Phys Rev, 2003; 67B: 134114 | | [32] | King W E, Benedek R. Phys Rev, 1981; 23B: 6335 |
|
|