| Al-7Si-Mg合金凝固过程形核模型建立及枝晶生长过程数值模拟* |
陈瑞1,许庆彦1( ),吴勤芳2,郭会廷2,柳百成1 |
1 清华大学材料学院先进成形制造教育部重点实验室, 北京 100084
2 明志科技有限公司, 苏州 215006 |
|
| NUCLEATION MODEL AND DENDRITE GROWTH SIMULATION IN SOLIDIFICATON PROCESS OF Al-7Si-Mg ALLOY |
Rui CHEN1,Qingyan XU1( ),Qinfang WU2,Huiting GUO2,Baicheng LIU1 |
1 Key Laboratory for Advanced Materials Processing Technology, Ministry of Education, School of Materials Science and Engineering, Tsinghua University, Beijing 100084
2 Mingzhi Technology Co. Limited, Suzhou 215006 |
引用本文:
陈瑞, 许庆彦, 吴勤芳, 郭会廷, 柳百成. Al-7Si-Mg合金凝固过程形核模型建立及枝晶生长过程数值模拟*[J]. 金属学报, 2015, 51(6): 733-744.
Rui CHEN,
Qingyan XU,
Qinfang WU,
Huiting GUO,
Baicheng LIU.
NUCLEATION MODEL AND DENDRITE GROWTH SIMULATION IN SOLIDIFICATON PROCESS OF Al-7Si-Mg ALLOY[J]. Acta Metall Sin, 2015, 51(6): 733-744.
| [1] | Shi Y F. PhD Dissertation, Tsinghua University, Beijing, 2013 (石玉峰. 清华大学博士学位论文, 北京, 2013) | | [2] | Y?ld?r?m M, ?zyürek D. Mater Des, 2013; 51: 767 | | [3] | Chen R, Shi Y F, Xu Q Y, Liu B C. Trans Nonferrous Met Soc China, 2014; 24: 1645 | | [4] | Zhu M, Jian Z Y, Yang G C, Zhou Y H. Mater Des, 2012; 36: 243 | | [5] | Birol Y. Mater Sci Eng, 2013; A559: 394 | | [6] | Wang Q G, Davidson C J. J Mater Sci, 2001; 36: 739 | | [7] | Ceschini L, Morri A, Morri A, Pivetti G. Mater Des, 2011; 32: 1367 | | [8] | Samuel A M, Samuel F H. Metall Mater Trans, 1995; 367A: 111 | | [9] | Wang Q G. Metall Mater Trans, 2003; 34A: 2887 | | [10] | Zhang L Y, Jiang Y H, Ma Z, Shan S F, Jia Y Z, Fan C Z, Wang W K. J Mater Process Technol, 2008; 207: 107 | | [11] | Li B, Xu Q Y, Pan D, Liu B C, Xiong Y C, Zhou Y J, Hong R Z. Acta Metall Sin, 2008; 44: 243 (李 斌, 许庆彦, 潘 冬, 柳百成, 熊艳才, 周永江, 洪润洲. 金属学报, 2008; 44: 243) | | [12] | Huo L, Han Z Q, Liu B C. Acta Metall Sin, 2009; 45: 1414 (霍 亮, 韩志强, 柳百成. 金属学报, 2009; 45: 1414) | | [13] | Wu M W, Xiong S M. Acta Metall Sin, 2010; 46: 1534 (吴孟武, 熊守美. 金属学报, 2010; 46: 1534) | | [14] | Shi Y F, Xu Q Y, Gong M, Liu B C. Acta Metall Sin, 2011; 47: 620 (石玉峰, 许庆彦, 龚 铭, 柳百成. 金属学报, 2011; 47: 620) | | [15] | Zhu M F, Cao W, Chen S L, Hong C P, Chang Y A. J Phase Equilib Diffus, 2007; 28: 130 | | [16] | Zhang X F, Zhao J Z, Jiang H X, Zhu M F. Acta Mater, 2012; 60: 2249 | | [17] | Shi Y F, Zhang Y, Xu Q Y, Liu B C. IOP Conf Ser: Mater Sci Eng, 2012; 33: 012112 | | [18] | Michelic S C, Thuswaldner J M, Bernhard C. Acta Mater, 2010; 58: 2738 | | [19] | Zhao J Z, Li L, Zhang X F. Acta Metall Sin, 2014; 50: 641 (赵九洲, 李 璐, 张显飞. 金属学报, 2014; 50: 641) | | [20] | Thévoz P H, Desbiolles J L, Rappaz M. Metall Mater Trans, 1989; 20A: 311 | | [21] | Oldfield W. Trans ASM, 1966; 59: 945 | | [22] | Stefanescu D M, Upadhya G, Bandyopadhyay D. Metall Mater Trans, 1990; 21A: 997 | | [23] | Guzowski M M, Sigworth G K, Sentner D A. Metall Mater Trans, 1987; 18A: 603 | | [24] | Johnsson M, B?ckerud L, Sigworth G K. Metall Mater Trans, 1993; 24A: 481 | | [25] | Greer A L, Bunn A M, Tronche A, Evans P V, Bristow D J. Acta Mater, 2000; 48: 2823 | | [26] | Quested T E, Greer A L. Acta Mater, 2005; 53: 2683 | | [27] | Chen R, Xu Q Y, Liu B C. J Mater Sci Technol, 2014; 30: 1311 | | [28] | Jiang H X, Zhao J Z. Acta Metall Sin, 2011; 47: 1099 (江鸿翔, 赵九洲. 金属学报, 2011; 47: 1099) | | [29] | Ohser J, Lorz U. Quantitative Gefuege Analyse. DVG, Leipzig-Stuttgart, 1994 | | [30] | Wang Q G, Cáceres C H. Mater Sci Forum, 1996; 24: 2159 | | [31] | Wang M Y, Xu Y J, Zheng Q W, Wu S J, Jing T, Chawal N. Metall Maters Trans, 2014; 45A: 1 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|