| 金属强度的尺寸效应* |
黄晓旭( ) |
| (Danish-Chinese Center for Nanometals, Department of Wind Energy, Technical University of Denmark, DK-4000 Roskilde, Denmark) |
|
| SIZE EFFECTS ON THE STRENGTH OF METALS |
HUANG Xiaoxu( ) |
| Danish-Chinese Center for Nanometals, Department of Wind Energy, Technical University of Denmark, DK-4000 Roskilde, Denmark |
引用本文:
黄晓旭. 金属强度的尺寸效应*[J]. 金属学报, 2014, 50(2): 137-140.
Xiaoxu HUANG.
SIZE EFFECTS ON THE STRENGTH OF METALS[J]. Acta Metall Sin, 2014, 50(2): 137-140.
| [1] |
Hall E O. Proc Phys Soc, 1951; 64B: 747
|
| [2] |
Petch N J. J Iron Steel Inst, 1953; 174: 25
|
| [3] |
Armstrong R W, Codd I, Douthwaite R M, Petch N J. Philos Mag, 1962; 7: 45
|
| [4] |
Takaki S. Mater Sci Forum, 2010; 654-656: 11
|
| [5] |
Eshelby J D, Frank F C, Nabarro F R N. Philos Mag, 1951; 42: 351
|
| [6] |
Li J C M. Trans TMS-AIME, 1963; 227: 239
|
| [7] |
Conrad H, Jung K. Mater Sci Eng, 2005; A391: 272
|
| [8] |
Dunstan D J, Bushby A J. Inter J Plast, 2014; 53: 56
|
| [9] |
Schiøtz J, Jacobsen K W. Science, 2003; 301: 1357
|
| [10] |
Kamikawa N, Huang X, Tsuji N, Hansen N. Acta Mater, 2009; 57: 4198
|
| [11] |
Hansen N. Acta Metall, 1977; 25: 863
|
| [12] |
Brenner S S. J Appl Phys, 1956; 27: 1484
|
| [13] |
Brenner S S. J Appl Phys, 1957; 28: 1023
|
| [14] |
Uchic M D, Shade P A, Dimiduk D M. Annu Rev Mater Res, 2009; 39: 361
|
| [15] |
Sudharshan Phani P, Johanns K E, George E P, Pharr G M. Acta Mater, 2013; 61: 2489
|
| [16] |
Johanns K E, Sedlmayr A, Sudharshan Phani P, Mönig R, Kraft O, George E P, Pharr G M. J Mater Res, 2012; 27: 508
|
| [17] |
Dehm G. Prog Mater Sci, 2009; 54: 664
|
| [18] |
Shan Z W, Mishra R K, Asif S A S, Warren O L, Minor A M. Nat Mater, 2008; 7: 115
|
| [19] |
Sudharshan Phani P, Johanns K E, Duscher G, Gali A, George E P, Pharr G M. Acta Mater, 2011; 59: 2172
|
| [20] |
Dunstan D J, Bushby A J. Int J Plast, 2013; 40: 152
|
| [21] |
Huang X, Tsuji N, Hansn N. Science, 2006; 312: 249
|
| [22] |
Huang X, Kamikawa N, Hansen N. Mater Sci Eng, 2008; A483-484 : 102
|
| [23] |
Huang X, Kamikawa N, Hansen N. J Mater Sci, 2008; 43: 7397
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|