奥氏体化与冷却速率对过共析钢组织的影响 |
李俊杰,Godfrey Andrew,刘伟 |
清华大学材料科学与工程系, 北京 100084 |
|
EFFECTS OF AUSTENITIZATION AND COOLING RATES ON THE MICROSTRUCTURE IN A HYPEREUTECTOID STEEL |
LI Junjie, Godfrey Andrew, LIU Wei |
Department of Materials Science and Engineering, Tsinghua University, Beijing 100084 |
引用本文:
李俊杰,Godfrey Andrew,刘伟. 奥氏体化与冷却速率对过共析钢组织的影响[J]. 金属学报, 2013, 49(5): 583-592.
LI Junjie,
Godfrey Andrew,
LIU Wei.
EFFECTS OF AUSTENITIZATION AND COOLING RATES ON THE MICROSTRUCTURE IN A HYPEREUTECTOID STEEL[J]. Acta Metall Sin, 2013, 49(5): 583-592.
[1] Li Y J, Choi P, Goto S, Borchers C, Raabe D, Kirchheim R. Acta Mater, 2012; 60: 4005
[2] Tashiro H. Nipp Steel Tec Rep, 1999; 80: 6
[3] Choi H C, Park K T. Scr Mater, 1996; 34: 857
[4] Taleff E M, Sridhar G B, Pourladian B. Wire J Int, 2003; 36: 73
[5] Bae C M, Nam W J, Lee C S. Metall Mater Trans, 2000; 31A: 2665
[6] Jang Y S, Phaniraj M P, Kim D I, Shim J H, Huh M Y. Metall Mater Trans, 2010; 41A: 2078
[7] Kanetsuki Y, Ibaraki N, Ashida S. ISIJ Int, 1991; 31: 304
[8] Taleff E M, Syn C K, Lesuer D R, Sherby D. Metall Mater Trans, 1996; 27A: 111
[9] Peng H F, Song X Y, Gao A G, Ma X L. Mater Lett, 2005; 59: 3330
[10] Zhang Y D, Esling C, Gong M L, Vincent G, Zhao X, Zuo L. Scr Mater, 2006; 54: 1897
[11] San Martin D, Rivera-Diaz-del-Castillo P E J, Garcia-de-Andres C. Scr Mater, 2008; 58: 926
[12] Elwazri A M, Wanjara P, Yue S. Metall Mater Trans, 2005; 36A: 2297
[13] Li Y, Yang Z M. Acta Metall Sin, 2010; 46: 1501
(李翼, 杨忠民. 金属学报, 2010; 46: 1501)
[14] Han K, Mottishaw T D, Smith G, Edmonds D V, Stacey A G. Mater Sci Eng, 1995; A190: 207
[15] Liu Z C. Heat Treat Met, 2007; 33: 1
(刘宗昌. 金属热处理, 2007; 33: 1)
[16] Roberts G A, Mehl R F. Trans AIME, 1943; 154: 318
[17] Porter D A, Easterling K E, Sherif M Y, translated by Chen L, Yu Y N. Phase Transformation in Metals and
Alloys. Beijing: Higher Education Press, 2011: 63
(Porter D A, Easterling K E, Sherif M Y 著, 陈冷, 余永宁 译. 金属和合金中的相变. 北京: 高等教育出版社, 2011: 63)
[18] Borchardt F S. Master Thesis, University of Pittsburgh, 2004
[19] Scheil E. Arch Eisenhuttenw, 1935; 8: 565
[20] Brandt W H. Trans AIME, 1946; 167: 550
[21] Hull F C, Colton R A, Mehl R F. Trans AIME, 1942; 50: 185
[22] Guo N. PhD Dissertation, Chongqing University, 2012
(郭宁. 重庆大学博士学位论文, 2012)
[23] Howell P R. Mater Charact, 1998; 40: 227
[24] Elwazri A M, Wanjara P, Yue S. Mater Sci Eng, 2005; A404: 91
[25] Han K, Smith G, Edmonds D V. Metall Mater Trans, 1995; 26A: 1617
[26] Han K, Edmonds D V, Smith G. Metall Mater Trans, 2001; 32A: 1313
[27] Nesterov D, Levchenko N, Sapozhkov V, Shevchenko A. Steel Trans, 1992; 22: 191
[28] Hung C Y, Spanos G, Rosenberg R O, Kral M V. Acta Mater, 2002; 50: 3781
[29] Kral M V, Spanos G. Acta Mater, 1999; 47: 711
[30] Kral M V, Spanos G. Acta Mater, 2003; 51: 301
[31] Spanos G, Kral M V. Int Mater Rev, 2009; 54: 19
[32] Kral M V, Spanos G. Scr Mater, 1997; 36: 875
[33] Kral M V, Mangan M A, Spanos G, Rosenberg R O. Mater Charact, 2000; 45: 17 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|