| 机械振动辅助激光熔覆NiCrBSi-TiC复合涂层中颗粒相行为特征 |
| 王传琦, 刘洪喜, 周荣, 蒋业华, 张晓伟 |
| 昆明理工大学材料科学与工程学院, 昆明 650093 |
|
| CHARACTERISTIC BEHAVIORS OF PARTICLE PHASES IN NiCrBSi-TiC COMPOSITE COATING BY LASER CLADDING ASSISTED BY MECHANICAL VIBRATION |
| WANG Chuanqi, LIU Hongxi, ZHOU Rong, JIANG Yehua, ZHANG Xiaowei |
| Faculty of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093 |
引用本文:
王传琦, 刘洪喜, 周荣, 蒋业华, 张晓伟. 机械振动辅助激光熔覆NiCrBSi-TiC复合涂层中颗粒相行为特征[J]. 金属学报, 2013, 49(2): 221-228.
WANG Chuanqi,
LIU Hongxi,
ZHOU Rong,
JIANG Yehua,
ZHANG Xiaowei.
CHARACTERISTIC BEHAVIORS OF PARTICLE PHASES IN NiCrBSi-TiC COMPOSITE COATING BY LASER CLADDING ASSISTED BY MECHANICAL VIBRATION[J]. Acta Metall Sin, 2013, 49(2): 221-228.
| [1] Sun R L, Mao J F, Yang D Z. Surf Coat Technol, 2002; 155: 203 [2] Lei Y W, Sun R L, Tang Y, Niu W. Opt Laser Technol, 2012; 44: 1141 [3] Fernandez E, Cadenas M, Gonzalez R, Navas C, Fernandez R,Damborenea J D. Wear, 2005; 259: 870 [4] Ma H B, Zhang W P. Rare Met Mater Eng, 2010; 39: 2189 (马海波, 张维平. 稀有金属材料与工程, 2010; 39: 2189) [5] Wu C F, Ma M X, Wu A P, Liu W J, Zhong M L, Zhang W M, Zhang H J. Acta Metall Sin, 2009; 45: 1091 (吴朝锋, 马明星, 吴爱平, 刘文今, 钟敏霖, 张伟明, 张红军. 金属学报, 2009; 45: 1091) [6] Lu X W, Lin X, Cao Y Q, Hu J, Gao B, Huang W D. Rare Met Mater Eng, 2011; 40: 714 (吕晓卫, 林鑫, 曹永青, 胡江, 高勃, 黄卫东. 稀有金属材料与工程, 2011; 40: 714) [7] Yang S, Zhong M L, Liu W J. J Aero Mater, 2002; 22(1): 26 (杨森, 钟敏霖, 刘文今. 航空材料学报, 2002; 22(1): 26) [8] Yang S, Liu W J, Zhong M L, Wang Z J. Mater Lett, 2004; 58: 2958 [9] Wang X H, Zhang M, Zou Z D, Qu S Y. Chin J Mech Eng, 2003; 39: 37 (王新洪, 张敏, 邹增大, 曲仕尧. 机械工程学报, 2003; 39: 37) [10] Cui C Y, Guo Z X, Wang H Y, Hu J D. J Mater Process Technol, 2007; 183: 380 [11] Sun R L, Guo L X, Dong S L, Yang D Z. Chin J Lasers, 2001; 28: 275 (孙荣禄, 郭立新, 董尚利, 杨德庄. 中国激光, 2001; 28: 275) [12] Sun R L, Yang D Z, Guo L X, Dong S L. Surf Coat Technol, 2001; 135: 307 [13] Wang C Q, Liu H X, Zhou R, Zhang X W, Zeng W H, Jiang Y H. Trans Mater Heat Treat, 2011; 32(7): 145 (王传琦, 刘洪喜, 周荣, 张晓伟, 曾维华, 蒋业华. 材料热处理学报, 2011; 32(7): 145) [14] Zhang H, Shi Y, Kutsuna M, Xu G J. Nucl Eng Des, 2010; 240: 2691 [15] Guo C, Zhou J S, Chen J M, Zhao J R, Yu Y J, Zhou H D. Wear, 2011; 270: 492 [16] Wu X L, Chen G N. Acta Metall Sin, 1998; 34: 1284 (武晓雷, 陈光南. 金属学报, 1998; 34: 1284) [17] Wang Z K, Zheng Q G, Tao Z Y, Ye H Q, Chen Q M. Acta Metall Sin, 1999; 35: 1027 (王忠柯, 郑启光, 陶曾毅, 叶和清, 陈清明. 金属学报, 1999; 35: 1027) [18] Hu C, Barnard L, Mridha S, Baker T N. J Mater Process Technol, 1996; 58: 87 [19] Sun R L, Lu W X, Yang X J. J Chin Ceram Soc, 2005; 33: 1448 (孙荣禄, 吕伟鑫, 杨贤金. 硅酸盐学报, 2005; 33: 1448) [20] Pei Y T. Acta Metall Sin, 1998; 34: 987 (裴宇韬. 金属学报, 1998; 34: 987) [21] Kurz W, Fisher D J, translated by Li J G, Hu Q D. Fundamentals of Solidification. Beijing: Higher Education Press, 2010: 28 (Kurz W, Fisher D J 著, 李建国, 胡侨丹译. 凝固原理. 北京: 高等教育出版社, 2010: 28) [22] Wang H M, Zhang J H, Tang Y J, Hu Z Q, Yukawa N, Morinaga M, Murata Y. Mater Sci Eng, 1992; A156: 109 [23] Chen Y, Wang H M. Rare Met Mater Eng, 2003; 32: 569 (陈瑶, 王华明. 稀有金属材料与工程, 2003; 32: 569) [24] Fernandez R, Lecomte J C, Kattamis T Z. Metall Mater Trans, 1978; 9A: 1381 [25] Jackson K A. Mater Sci Eng, 1984; 65: 7 [26] Zhang S, Zhang C H, Kang Y P, Wu W T, Wang M C, Wen X Z. Chin J Nonferrous Met, 2001; 11: 1026 (张松, 张春华, 康煜平, 吴维?, 王茂才,文効忠. 中国有色金属学报, 2001; 11: 1026) [27] Li Y X, Bai P K, Wang Y M, Hu J D, Guo Z X. Mater Des, 2009; 30: 140 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|