| 高氮钢焊缝的组织和冲击性能研究 |
| 李冬杰,陆善平,李殿中,李依依 |
| 中国科学院金属研究所 沈阳材料科学国家(联合)实验室, 沈阳 110016 |
|
| INVESTIGATION OF THE MICROSTRUCTURE AND IMPACT PROPERTIES OF THE HIGH NITROGEN STAINLESS STEEL WELD |
| LI Dongjie, LU Shanping, LI Dianzhong, LI Yiyi |
| Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
李冬杰, 陆善平, 李殿中, 李依依. 高氮钢焊缝的组织和冲击性能研究[J]. 金属学报, 2013, 49(2): 129-136.
LI Dongjie,
LU Shanping,
LI Dianzhong,
LI Yiyi.
INVESTIGATION OF THE MICROSTRUCTURE AND IMPACT PROPERTIES OF THE HIGH NITROGEN STAINLESS STEEL WELD[J]. Acta Metall Sin, 2013, 49(2): 129-136.
| [1] Berns H. ISIJ Int, 1996; 36: 909 [2] Ikegami Y, Nemoto R. ISIJ Int, 1996; 36: 855 [3] Rawers I C, White H, Doan R. ISIJ Int, 1996; 36: 746 [4] Gavriljuk V G. ISIJ Int, 1996; 36: 738 [5] Liu W, Zheng Y G, Liu C S, Yao Z M, Ke W. Acta Metall Sin, 2003; 39:85 (柳伟, 郑玉贵, 刘常升, 姚治铭, 柯伟. 金属学报, 2003; 39: 85) [6] Bi H Y, Jiang X X, Li S Z, Yang J X. Acta Metall Sin, 1997; 33: 1069 (毕红运, 姜晓霞, 李诗卓, 杨景祥. 金属学报, 1997; 33: 1069) [7] Lu S P, Li D J, Li D Z, Li Y Y. Trans Chin Weld Inst, 2010; 31(2):21 (陆善平, 李冬杰, 李殿中, 李依依. 焊接学报, 2010; 31(2): 21) [8] Tanaka M, Terasaki H, Ushio M, Lowke J J. Plasma Chem Plasma Process,2003; 23: 585 [9] Tanaka M, Tashiro S, Ushio M, Mita T, Murphy A B, Lowke J J. Vacuum,2006; 80: 1195 [10] Burgardt P, Heiple C R. Weld J, 1986; 65(6): 150 [11] Sahoo P, DebRoy T, McNallan M J. Metall Trans, 1988; 19B: 483 [12] Katayama S, Fujimoto T, Matsunawa A. Trans JWRI, 1985; 14(1): 123 [13] Arata Y, Matsuda F, Katayama S. Trans JWRI, 1976; 5(2): 135 [14] Brooks J A, Thompson A W, Williams J C. Weld J, 1984; 63(3): 71s [15] Fredriksson H. Metall Trans, 1972; 3: 2989 [16] Leone G L, Kerr H W. Weld J, 1982; 61(1): 13s [17] Lippold J C, Savage W F. Weld J, 1980; 59(2): 48s [18] Lu S P, Fujii H, Nogi K. Scr Mater, 2004; 51: 271 [19] Lu S P, Fujii H, Nogi K. Sci Technol Weld Join, 2007; 12: 689 [20] Howse D S, Lucas W. Sci Technol Weld Join, 2000; 15(5): 189 [21] Liu L M, Zhang Z D, Song G, Wang L. Metall Mater Trans, 2007; 38A:649 [22] Huang H Y. Metall Mater Trans, 2010; 41A: 2829 [23] Anderko K, Schafer L, Materna-Morris E. J Nucl Mater, 1991; 179-181:492 [24] Schafer L. J Nuclear Mater, 1998; 258-263: 1336 [25] Wang P, Lu S P, Xiao N M, Li D Z, Li Y Y. Mater Sci Eng, 2010; A527: 3210 |
|