| 前躯体组织对C—Mn—Si钢组织特征及力学行为的影响 |
| 任勇强,谢振家,张宏伟,袁胜福,宋婷婷,尚成嘉 |
| 北京科技大学材料科学与工程学院, 北京 100083 |
|
| EFFECT OF PRECURSOR MICROSTRUCTURE ON MORPHOLOGY FEATURE AND MECHANICAL PROPERTY OF C—Mn—Si STEEL |
| REN Yongqiang, XIE Zhenjia, ZHANG Hongwei, YUAN Shengfu, SONG Tingting, SHANG Chengjia |
| School of Materials Science and Engineering, University of Science and Technology Beijing,Beijing 100083 |
引用本文:
任勇强,谢振家,张宏伟,袁胜福,宋婷婷,尚成嘉. 前躯体组织对C—Mn—Si钢组织特征及力学行为的影响[J]. 金属学报, 2013, 49(12): 1558-1566.
REN Yongqiang,
XIE Zhenjia,
ZHANG Hongwei,
YUAN Shengfu,
SONG Tingting,
SHANG Chengjia.
EFFECT OF PRECURSOR MICROSTRUCTURE ON MORPHOLOGY FEATURE AND MECHANICAL PROPERTY OF C—Mn—Si STEEL[J]. Acta Metall Sin, 2013, 49(12): 1558-1566.
| [1] Speich G R, Demarest V A, Miller R L. Metall Trans, 1981; 12A: 1419
[2] Takashi F, Hirofumi M, Michio E, Hiroshi T, Kazuo K, Osamu A, Teruaki Y.Trans ISIJ, 1981; 21: 812
[3] Matsumura O, SakumaY, Takechi H. Scr Metall, 1987; 21: 1301
[4] Matsumura O, SakumaY, Takechi H. ISIJ Int, 1992; 32: 1014
[5] Sugimoto K, Misu M, Kobayashi M, Shirasawa H. ISIJ Int, 1993; 33: 775
[6] Speer J G, Matlock D K, De Cooman B C, Schroth J G. Acta Mater, 2003; 51: 2611
[7] Speer J G, Edmonds D V, Rizzo F C, Matlock D K. Curr Opin Solid State Mater Sci, 2004; 8: 219
[8] Edmonds D V, He K, Rizzo F C, De Cooman B C, Matlock D K, Speer J G.Mater Sci Eng, 2006; A438—440: 25
[9] De Moor E, Lacroix S, Clarke A J, Penning J, Speer J G. Metall Mater Trans, 2008; 39A: 2586
[10] Liu H P, Lu X W, Jin X J, Dong H, Shi J. Scr Mater, 2011; 64: 749
[11] Paravicini B E, Santofimia M J, Zhao L, Sietsma J, Anelli E. Mater Sci Eng, 2013; A559: 486
[12] Santofimia M J, Nguyen—Minh T, Zhao L, Petrov R, Sabirov I, Sietsma J.Mater Sci Eng, 2010; A527: 6429
[13] Maruyama H. J Jpn Soc Heat Treat, 1977; 17: 198
[14] Nishiyama Z. Martensitic Transformations. New York: Academic Press, 1978: 60
[15] Sugimoto K, Usui N, Kobayashi M, Hashimoto S. ISIJ Int, 1992; 32: 1311
[16] Chiang J, Lawrence B, Boyd J D, Pilkey A K. Mater Sci Eng, 2011; A528: 4516
[17] Santofimia M J, Zhao L, Sietsma J. Metall Mater Trans, 2009; 40A: 46
[18] Sakuma Y, Matlock D K, Krauss G. Metall Trans, 1992; 23A: 1221
[19] Kim S J, Lee C G, Choi I, Lee S. Metall Mater Trans, 2001; 32A: 505
[20] Ren Y Q, Xie Z J, Shang C J. Acta Metall Sin, 2012; 48: 1074
(任勇强, 谢振家, 尚成嘉.金属学报, 2012; 48: 1074)
[21] Dieter G E. Mechanical Metallurgy. 2nd Ed., New York: McGraw—Hill Book Company, 1988: 87
[22] Jacques P, Cornet X, Harlet P, Ladri$\grave{\rm e$re J, Delannay F. Metall Mater Trans, 1998; 29A: 2383
[23] Yakubovsky O, Fonstein N, Bhattacharya D. In: De Cooman B C ed.,Proceedings Conference Trip—Aided High Strength Ferrous Alloys,Aachen: Wissenschaftsverlag Mainz Gmbh, 2002: 263
[24] Mahieu J, Maki J, De Cooman B C, Claessens S. Metall Mater Trans, 2002; 33A: 2573
[25] Bai D Q, Chiro A D, Yue S. Mater Sci Forum, 1998; 284—286: 253
[26] Wang J, Van Der Zwaag S. Metall Mater Trans, 2001; 32A: 1527
[27] Pereloma E V, Timokhina I B, Hodgson P D. Mater Sci Eng, 1999; 273—275: 448
[28] Baik S C, Park S H, Kwon O, Kim D I, Oh K H. ISIJ Int, 2006; 46: 599
[29] Thierry I, Jos$\acute{\rm e$e D, Audrey C, Christopher O. Steel Res, 2002; 6—7: 218
[30] Kwon E P, Fujieda S, Shinoda K, Suzuki S. Mater Sci Eng, 2011; A528: 5007
[31] Ryde L. Mater Sci Technol, 2006; 22: 1297
[32] Xiong X C, Chen B, Huang M X, Wang J F, Wang L. Scr Mater, 2013; 68: 321
[33] Tsukatani I, Hashimoto S I, Inoue T. ISIJ Int, 1991; 31: 992
[34] Sugimoto K I, Misu M, Kobayashi M, Shirasawa H. ISIJ Int, 1993; 33: 775 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|