| 长期热循环条件下全片层高Nb-TiAl合金显微组织稳定性 |
| 方璐1),丁贤飞2),张来启1),郝国建1),林均品1) |
| 1) 北京科技大学新金属材料国家重点实验室, 北京100083
2) 北京科技大学国家材料服役安全科学中心, 北京100083 |
|
| MICROSTRUCTURE STABILITY IN A FULLY LAMELLAR HIGH Nb-TiAl ALLOY AFTER LONG-TERM THERMAL CYCLING |
| FANG Lu 1), DING Xianfei2), ZHANG Laiqi1), HAO Guojian1), LIN Junpin1) |
| 1) State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing,Beijing 100083
2) National Center for Materials Service Safety, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
方璐,丁贤飞,张来启,郝国建,林均品. 长期热循环条件下全片层高Nb-TiAl合金显微组织稳定性[J]. 金属学报, 2013, 49(11): 1416-1422.
FANG Lu,
DING Xianfei,
ZHANG Laiqi,
HAO Guojian,
LIN Junpin.
MICROSTRUCTURE STABILITY IN A FULLY LAMELLAR HIGH Nb-TiAl ALLOY AFTER LONG-TERM THERMAL CYCLING[J]. Acta Metall Sin, 2013, 49(11): 1416-1422.
| [1] Kim Y W. JOM, 1995; 47: 39
[2] Wu X. Intermetallics, 2006; 14: 1114
[3] Lin J P, Xu X J, Wang Y L, He S F, Zhang Y, Song X P, Chen G L.Intermetallics, 2007; 15: 668
[4] Appel F, Brossmann U, Christoph U, Eggert S, Janschek P, Lorenz U,Mulauer J, Oehring M, Paul J D H. Adv Eng Mater, 2000; 2: 699
[5] Zhao W Y, Pei Y L, Zhang D H, Ma Y, Gong S K, Xu H B. Intermetallics, 2011; 19: 429
[6] Kim Y W. J Mater Sci Technol, 1994; 10: 79
[7] Es-Souni M, Bartels A, Wagner R. Mater Sci Eng, 1995; A192-193: 698
[8] Morris M A, Leboeuf M. Mater Sci Eng, 1997: A239-240: 429
[9] Hu D, Godfrey A B, Loretto M H. Intermetallics, 1998; 6: 413
[10] Ramanujan R V, Maziasz P J, Liu C T. Acta Mater, 1996; 44: 2611
[11] Huang Z W, Voice W, Bowen P. Intermetallics, 2000; 8: 417
[12] Cheng T T. Intermetallics, 1999; 7: 995
[13] Huang Z W, Cong T. Intermetallics, 2010; 18: 161
[14] Beschliesser M, Chatterjee A, Lorich A, Knabl W, Kestler H, Dehm G,Clemens H. Mater Sci Eng, 2002; A329-331: 124
[15] Geng H B, He S Y, Lei T Q. Acta Metall Sin, 1996; 32: 51
(耿洪滨, 何世禹, 雷廷权. 金属学报, 1996; 32: 51)
[16] Manna I, Pabi S K, Gust W. Int Mater Rev, 2001; 46: 53
[17] Qin G, Wang J, Hao S. Intermetallics, 1999; 7: 1
[18] Wang X P, Zheng Y R. J Mater Eng, 2000; (7): 20
(汪小平, 郑运荣. 材料工程, 2000; (7): 20)
[19] Tang J C, Huang B Y, He Y H, Xie K. Trans Nonferrous Met Soc China, 2000; 10: 10 |
|