| NiTi合金中马氏体相变失稳与局部化的原位多场研究 |
| 杜泓飞1,曾攀1, 2,赵加清3,雷丽萍1, 2,方刚1, 2,瞿体明1, 2 |
| 1.清华大学机械工程系, 北京 100084
2.清华大学先进成形制造教育部重点实验室, 北京 100084
3.清华大学核能与新能源技术研究院, 北京 100084 |
|
| IN SITU MULTI-FIELDS INVESTIGATION ON INSTABILITY AND TRANSFORMATION LOCALIZATION OF MARTENSITIC PHASE TRANSFORMATION IN NiTi ALLOYS |
| DU Hongfei 1, ZENG Pan1, 2, ZHAO Jiaqing3,LEI Liping1, 2, FANG Gang1, 2, QU Timing1, 2 |
| 1. Department of Mechanical Engineering, Tsinghua University, Beijing 100084
2. Key Laboratory for Advanced Material Processing Technology, Ministry of Education, Tsinghua University, Beijing,100084
3. Institute of Nuclear and New Energy Technology, Tsinghua University, Beijing 100084 |
引用本文:
杜泓飞,曾攀1,赵加清,雷丽萍,方刚,瞿体明. NiTi合金中马氏体相变失稳与局部化的原位多场研究[J]. 金属学报, 2013, 49(1): 17-25.
DU Hongfei,
ZENG Pan,
ZHAO Jiaqing,
LEI Liping,
FANG Gang,
QU Timing.
IN SITU MULTI-FIELDS INVESTIGATION ON INSTABILITY AND TRANSFORMATION LOCALIZATION OF MARTENSITIC PHASE TRANSFORMATION IN NiTi ALLOYS[J]. Acta Metall Sin, 2013, 49(1): 17-25.
| [1] Zhao L C, Cai W, Zheng Y F. Shape Memory Effect and Superelasticity in Alloys. Beijing: National Defense Industry Press, 2002: 5 (赵连城, 蔡伟, 郑玉峰. 合金的形状记忆效应与超弹性. 北京: 国防工业出版社, 2002: 5) [2] Otsuka K, Wayman C M, translated by Zhang C C, Su J C. Shape Memory Materials. Shanghai: Second Military Medical University Press, 2003: 30 (Otsuka K, Wayman C M著, 张春才, 苏佳灿译. 形状记忆材料. 上海: 第二军医大学出版社, 2003: 30) [3] Otsuka K, Wayman C M. Shape Memory Materials. Cambridge: Cambridge University Press, 1998: 20 [4] Shaw J A, Kyriakides S. Acta Mater, 1997; 45: 683 [5] Li Z Q, Sun Q P. Int J Plast, 2002; 18: 1481 [6] Sittner P, Liu Y, Novak V. J Mech Phys Solids, 2005; 53: 1719 [7] Brinson L C, Schmidt I, Lammering R. J Mech Phys Solids, 2004; 52: 1549 [8] Daly S, Ravichandran G, Bhattacharya K. Acta Mater, 2007; 55: 3593 [9] Daly S, Miller A, Ravichandran G, Bhattacharya K. Acta Mater, 2007; 55: 6322 [10] Favier D, Louche H, Schlosser P, Orgeas L, Vacher P, Debove L. Acta Mater, 2007; 55: 5310 [11] Zhang X H, Feng P, He Y J, Yu T X, Sun Q P. Int J Mech Sci, 2010; 52: 1660 [12] Kim K, Daly S. Exp Mech, 2011; 51: 641 [13] Sutton M A, Orteu J J, Schreier H W. Image Correlation For Shape Motion And Deformation Measurements.New York: Springer, 2009: 36 [14] Zhao J Q, Zeng P, Lei L P, Ma Y. Opt Laser Eng, 2012; 50: 473 [15] Zhao J Q, Zeng P, Lei L P, Du H F, He W B, Liu Y, Xu Y J. Opt Laser Eng, 2012; 50: 1662 [16] Zhao J Q. PhD Thesis, Tsinghua University, 2012 (赵加清. 清华大学博士论文, 北京, 2012) [17] Reedlunn B, Daly S, Hector L, Zavattieri P, Shaw J. Exp Tech, 2011; 35: 1 [18] Chu T C, Ranson W F, Sutton M A. Exp Mech, 1985; 25: 232 [19] Sutton M A, McNeill S R, Helm J D. Photo-Mechanics, 2000; 77: 323 [20] Churchill C B, Shaw J A, Iadicola M A. Exp Tech, 2010; 34: 63 [21] Shaw J A, Kyriakides S. Int J Plast, 1998; 13: 837 [22] Churchill C B, Shaw J A, Iadicola M A. Exp Tech, 2009; 33: 51 [23] Feng P, Sun Q P. J Mech Phys Solids, 2006; 54: 1568 [24] Feng P, Sun Q P. Smart Mater Struct, 2007; 16: S179 [25] Zhang Y T, Qi D X. The Theory on Strain Localization and its Applications. Tianjin: Tianjin University Press, 2010: 43 (张义同, 齐德. 应变局部化理论及应用. 天津: 天津大学出版社, 2010: 43) |
|