Please wait a minute...
金属学报  2012, Vol. 48 Issue (9): 1067-1073    DOI: 10.3724/SP.J.1037.2012.00094
  论文 本期目录 | 过刊浏览 |
VC沉淀粒子对TWIP钢加工硬化行为的影响
张志波, 刘振宇, 张维娜
东北大学轧制技术及连轧自动化国家重点实验室, 沈阳 110819
EFFECT OF VC PARTICLES ON THE STRAIN HARDENING BEHAVIOR OF TWIP STEEL
ZHANG Zhibo, LIU Zhenyu, ZHANG Weina
State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819
引用本文:

张志波 刘振宇 张维娜. VC沉淀粒子对TWIP钢加工硬化行为的影响[J]. 金属学报, 2012, 48(9): 1067-1073.
, , . EFFECT OF VC PARTICLES ON THE STRAIN HARDENING BEHAVIOR OF TWIP STEEL[J]. Acta Metall Sin, 2012, 48(9): 1067-1073.

全文: PDF(3174 KB)  
摘要: 对Fe-Mn-C系2种TWIP钢Fe22Mn0.6C和Fe22Mn0.6C0.19V的显微组织、力学性能及加工硬化行为进行了研究. 结果表明, 经900℃固溶处理后的Fe22Mn0.6C0.19V钢和经800℃固溶处理的Fe22Mn0.6C钢具有晶粒尺寸相近的奥氏体组织; Fe22Mn0.6C0.19V钢在真应变ε>0.14后进入加工硬化速率平台区, 而Fe22Mn0.6C钢则在ε>0.12后即进入加工硬化速率平台区;  Fe22Mn0.6C0.19V钢在ε>0.21以后结束了加工硬化速率平台区, 其平台区明显较Fe22Mn0.6C钢短;  Fe22Mn0.6C0.19V钢加工硬化速率平台在ε>0.21以后结束是由VC沉淀粒子与TWIP钢形变孪晶相互作用引起的, VC沉淀粒子对于TWIP钢形变孪晶的产生及增殖都有明显的抑制作用.
关键词 : TWIP钢,  加工硬化速率,  VC沉淀粒子,  形变孪晶    
Abstract:The twinning induced plasticity (TWIP) steel has received more and more attention for its outstanding combination of good strength and high ductile. It has been proposed that deformation twinning plays an important role in controlling the deformation behavior. The formation of deformation twins is influenced by deformation temperature, strain rate, pre-deformation, grain size and precipitates. The generation of deformation twins in austenitic steel is closely related to precipitates. However, the relationship between strain hardening rate and precipitates in TWIP steels has not been clarified. In this work, the effect of vanadium carbides on the microstructure, strain hardening behavior and mechanical properties of Fe-Mn-C TWIP steel was investigated. The specimens of Fe22Mn0.6C and Fe22Mn0.6C0.19V TWIP steels with similar grain sizes were fabricated through solution treatments at different temperatures. Mechanical properties were measured by tensile tests, and microstructure evolution was observed by EBSD and TEM. The strain hardening rate (dσ/dε)-true strain (ε) curves of two steels were drawn. The results show that for the Fe22Mn0.6C0.19V steel, the strain hardening rate platform appear when true strain ε>0.14, while the strain hardening rate platform appear when the ε>0.12 for the Fe22Mn0.6C steel. The platform of Fe22Mn0.6C steel is significantly longer than that of Fe22Mn0.6C0.19V steel, The platform of Fe22Mn0.6C0.19V steel disappear quickly as true strain ε>0.21. Tensile specimens of Fe22Mn0.6C and Fe22Mn0.6C0.19V steels were observed by TEM, the results show that both the generation and propagation of deformation twins are inhibited significantly by vanadium carbides.
Key words: TWIP steel    strain hardening rate    vanadium carbides    deformation twins
收稿日期: 2012-02-24     
ZTFLH: 

TG115.213

 
基金资助:

国家自然科学基金项目50874131和中央高校基本科研业务费专项资金项目N100507002资助

作者简介: 张志波, 男, 1983年生, 博士生
[1] Frommeyer G, Br¨ux U, Neumann P. ISIJ Int, 2003; 43: 438

[2] Gr¨assel O, Kr¨uger L, Frommeyer G, Meyer L W. Int J Plast, 2000; 16: 1391

[3] Wang S H, Liu Z Y, Wang G D, Liu J L, Liang G F , Li Q L. J Iron Steel Res, 2010; 17: 70

[4] Vercammen S, Blanpai B, Cooman B C D, Wollants P. Acta Mater, 2004; 52: 2005

[5] Christian J W, Mahajan S. Prog Mater Sci, 1995; 39: 1

[6] Allain S, Chateau J P, Bouaziz O, Migot S, Guelton N. Mater Sci Eng, 2004; A387–389: 158

[7] Hokka M, Kuokkala V T, Curtze S, Vuoristo T, Apostol M. J Phys IV France, 2006; 134: 1301

[8] Xiong R G, Fu R Y , Su Y, Li Q , Wei X C, Li L. J Iron Steel Res, 2009; 16: 81

[9] Li N, Wang Y D, Peng R L, Sun X, Liaw P K, Wu G L, Wang L, Cai H N. Acta Mater, 2011; 59: 6369

[10] Bouaziz O, Allain S, Estrin Y. Scr Mater, 2010; 62: 713

[11] Bouaziz O, Allain S, Scott C. Scr Mater, 2008; 58: 484

[12] Gutierrez–Urrutia I, Zaefferer S, Raabe D. Mater Sci Eng, 2010; A527: 3552

[13] Wang S H, Liu Z Y, Wang G D. Acta Metall Sin, 2009; 45: 1083

(王书涵, 刘振宇, 王国栋. 金属学报, 2009; 45: 1083)

[14] Bracke L, Verbeken K, KestensL, PenningJ. Acta Mater, 2009; 57: 1512

[15] Jiang L. PhD Thesis, Montreal: Mcgill University, 2004

[16] Dumay A. PhD Thesis, Nancy: Institut National Polytechnique de Lorraine, 2008

[17] Chateau J P, Dumay A, Allain S, Jacques A. J Phys: Conf Ser, 2010; 240: 012023

[18] Scott C, Remy B, Collet J L, Cael A, Bao C, Danoix F, Malard B, Curfs C. Int J Mater Res, 2011; 102: 538

[19] Wilkens M. Phys Statd Solid, 1970; 2A: 359

[20] Furuhara T, Shinyoshi T, Miyamoto G, Yamaguchi J, Sugita N, Kimura N, Takemura N, Maki T. ISIJ Int, 2003; 43: 2028

[21] Renard K, Ryelandt S, Jacques P J. Mater Sci Eng, 2010; A527: 2969

[22] Bouaziz O, Allain S, Scott C P, Cugy P, Barbier D. Curr Opin Solid State Mater Sci, 2011; 15: 141

[23] Bouaziz O, Guelton N. Mater Sci Eng, 2001; A319–321: 246

[24] Sevillano J G. Scr Mater, 2008; 59: 135

[25] Allain S, Chateau J P, Dahmoun D, Bouaziz O. Mater Sci Eng, 2004; A387–389: 272

[26] Danaf E E, Kalidindi S R, Doherty R D. Metall Mater Trans, 1999; 30A: 1223

[27] M¨ullner P, Solcnthalcr C. Mater Sci Eng, 1997; A230: 107
[1] 司永礼, 薛金涛, 王幸福, 梁驹华, 史子木, 韩福生. Cr添加对孪生诱发塑性钢腐蚀行为的影响[J]. 金属学报, 2023, 59(7): 905-914.
[2] 彭俊, 金鑫焱, 钟勇, 王利. 基板表层组织对Fe-16Mn-0.7C-1.5Al TWIP钢可镀性的影响[J]. 金属学报, 2022, 58(12): 1600-1610.
[3] 胡晨, 潘帅, 黄明欣. 高强高韧异质结构温轧TWIP钢[J]. 金属学报, 2022, 58(11): 1519-1526.
[4] 余晨帆, 赵聪聪, 张哲峰, 刘伟. 选区激光熔化316L不锈钢的拉伸性能[J]. 金属学报, 2020, 56(5): 683-692.
[5] 李根, 兰鹏, 张家泉. 基于Ce变质处理的TWIP钢凝固组织细化[J]. 金属学报, 2020, 56(5): 704-714.
[6] 李亦庄,黄明欣. 基于中子衍射和同步辐射X射线衍射的TWIP钢位错密度计算方法[J]. 金属学报, 2020, 56(4): 487-493.
[7] 李金许,王伟,周耀,刘神光,付豪,王正,阚博. 汽车用先进高强钢的氢脆研究进展[J]. 金属学报, 2020, 56(4): 444-458.
[8] 董福涛,薛飞,田亚强,陈连生,杜林秀,刘相华. 退火温度对TWIP钢组织性能和氢致脆性的影响[J]. 金属学报, 2019, 55(6): 792-800.
[9] 高钰璧, 丁雨田, 陈建军, 许佳玉, 马元俊, 张东. 挤压态GH3625合金冷变形过程中的组织和织构演变[J]. 金属学报, 2019, 55(4): 547-554.
[10] 周博, 隋曼龄. AZ31镁合金拉伸扭折带结构的产生及交互作用机制[J]. 金属学报, 2019, 55(12): 1512-1518.
[11] 李冬冬, 钱立和, 刘帅, 孟江英, 张福成. Mn含量对Fe-Mn-C孪生诱发塑性钢拉伸变形行为的影响[J]. 金属学报, 2018, 54(12): 1777-1784.
[12] 单智伟, 刘博宇. Mg的{101̅2}形变孪晶机制*[J]. 金属学报, 2016, 52(10): 1267-1278.
[13] 袁晓云, 陈礼清. 一种高锰奥氏体TWIP钢的高温热变形与再结晶行为*[J]. 金属学报, 2015, 51(6): 651-658.
[14] 孙朝阳, 郭祥如, 黄杰, 郭宁, 王善伟, 杨竞. 耦合孪生的TWIP钢单晶体塑性变形行为模拟研究[J]. 金属学报, 2015, 51(3): 357-363.
[15] 孙朝阳,郭祥如,郭宁,杨竞,黄杰. 耦合孪生的TWIP钢多晶体塑性变形行为研究*[J]. 金属学报, 2015, 51(12): 1507-1515.