| 低碳钢中残余奥氏体的调控及对力学性能的影响 |
| 任勇强, 谢振家, 尚成嘉 |
| 北京科技大学材料科学与工程学院, 北京 100083 |
|
| REGULATION OF RETAINED AUSTENITE AND ITS EFFECT ON THE MECHANICAL PROPERTIES OF LOW CARBON STEEL |
| REN Yongqiang, XIE Zhenjia, SHANG Chengjia |
| School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
任勇强 谢振家 尚成嘉. 低碳钢中残余奥氏体的调控及对力学性能的影响[J]. 金属学报, 2012, 48(9): 1074-1080.
,
,
.
REGULATION OF RETAINED AUSTENITE AND ITS EFFECT ON THE MECHANICAL PROPERTIES OF LOW CARBON STEEL[J]. Acta Metall Sin, 2012, 48(9): 1074-1080.
| [1] McFarlan W H. US Pat, 3378360, 1968[2] Hayami S, Furukawa T. Microalloying 75. New York: Union Carbide Corp, 1977: 311[3] Matsumura O, Sakuma Y, Takechi H. Scr Metall, 1987; 21: 1301[4] Matsumura O, Sakuma Y, Takechi H. ISIJ Int, 1987; 27: 570[5] Matsumura O, Sakuma Y, Takechi H. ISIJ Int, 1992; 32: 1014[6] Sugimoto K, Misu M, Kobayashi M, Shirasawa H. ISIJ Int, 1993; 33: 775[7] Gr¨assel O, Frommeyer G. Mater Sci Technol, 1998; 14: 1213[8] Bouaziz O, Guelton N. Mater Sci Eng, 2001; A319–321: 246[9] Barnett M R. Mater Sci Eng, 2007; A464: 1[10] Speer J G, Matlock D K, De Cooman B C, Schroth J G. Acta Mater, 2003; 51: 2611[11] Matlock D K, Brautigam V E, Speer J G. Mater Sci Forum, 2003; 426–432: 1089[12] Sakuma Y, Matsumura O, Takechi H. Metall Mater Trans, 1991; A22: 489[13] Herrera C, Ponge D, Raabe D. Acta Mater, 2011; 59: 4653[14] Girault E, Jacques P, Harlet Ph, Mols K, Van Humbeeck J, Aernoudt E, Delannay F. Mater Charact, 1998; 40: 111[15] Ray A, Dhua S K. Mater Charact, 1996; 37: 1[16] Speer J G, Streicher A M, Matlock D K, Rizzo F C, Krauss G. In: Damm E B, Merwin M eds., Austenite Formation and Decomposition, Warrendale: TMS, 2003: 505[17] Edmonds DV, He K, Rizzo F C, De CoomanB C,Matlock D K, Speer J G. Mater Sci Eng, 2006; A438–440: 25[18] De Cooman B C, Speer J G. In: Lee H C ed., The 3rd Int Conf on Advanced Structural Steels. Gyeongju: The Korean Institute of Metals and Materials, 2006: 798[19] Streicher A M, Speer J G, Matlock D K, De Cooman B C. In: Speer J G ed., Proc Int Conf on Advanced High Strength Sheet Steels for Automotive Applications. Warrendale: AIST, 2004: 51[20] Speer J G, Edmonds D V, Rizzo F C, Matlock D K. Opin Curr Solid State Mater Sci, 2004; 8: 219[21] Sugimoto K, Tsunezawa M, Hojo T, Ikeda S. ISIJ Int, 2004; 44: 1608[22] Raabe D, Ponge D, Dmitrieva O, Sander B. Scr Mater, 2009; 60: 1141[23] Shi J, Sun X J, Wang M Q, Hui W J, Dong H, Cao W Q. Scr Mater, 2010; 63: 815[24] Wang C Y, Shi J, CaoWQ, Dong H. Mater Sci Eng, 2010; A527: 3442[25] Li H Y, Lu X W, Wu X C, Min Y A, Jin X J. Mater Sci Eng, 2010; A527: 6255[26] Santofimia M J, Zhao L, Sietsma J. Metall Mater Trans, 2009; A40: 46[27] Mukherjee M, Mohanty O N, Hashimoto S, Hojo T, Sugimoto K. ISIJ Int, 2006; 46: 316[28] Fan X. Metallic X–ray Physics. Beijing: Mechanical Industry Press, 1989: 159(范雄. 金属X射线学. 北京: 机械工业出版社, 1989: 159)[29] Sugimoto K, Usui N, Kobayashi M, Hashimoto S. ISIJ Int, 1992; 32: 1311[30] Cullity B D. Elements of X–ray Diffraction. Massachusetts: Addison–Wesley, 1978: 359[31] Santofimia M J, Nguyen–Minh T, Zhao L, Petrov R, Sabirov I, Sietsma J. Mater Sci Eng, 2010; A527: 6429[32] Thomas G A, Speer J G, Matlock D K. Metall Mater Trans, 2011; 42A: 3652[33] Zhang K, Xu W Z, Guo Z H, Rong Y H, Wang M Q, Dong H. Acta Metall Sin, 2011; 47: 489(张 柯, 许为宗, 郭正洪, 戎咏华, 王毛球, 董 瀚. 金属学报, 2011; 47: 489)[34] Santofimia M J, Zhao L, Petrov R, Kwakernaak C, Sloof W G, Sietsma J. Acta Mater, 2011; 59: 6059[35] Nouri A, Saghafian H, Kheirandish Sh. J Iron Steel Res Int, 2010; 17(5): 44[36] Speich G R, Demarest V A, Miller R L. Metall Mater Trans, 1981; 12A: 1419[37] Santofimia M J, Zhao L, Sietsma J. Metall Mater Trans, 2011; 42A: 3620 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|