| 脉冲磁场处理Fe52Co34Hf7B6Cu1非晶的低温真空退火效应 |
| 晁月盛,王莉,张艳辉,朱涵娴,罗丽平 |
| 东北大学理学院, 沈阳 110819 |
|
| EFFECT OF LOW-TEMPERATURE VACUUM ANNEALING ON THE MAGNETIC PULSED AMORPHOUS Fe52Co34Hf7B6Cu1 ALLOY |
| CHAO Yuesheng, WANG Li, ZHANG Yanhui, ZHU Hanxian, LUO Liping |
| College of Sciences, Northeastern University, Shenyang 110819 |
引用本文:
晁月盛,王莉,张艳辉,朱涵娴,罗丽平. 脉冲磁场处理Fe52Co34Hf7B6Cu1非晶的低温真空退火效应[J]. 金属学报, 2012, 48(6): 749-752.
,
,
.
EFFECT OF LOW-TEMPERATURE VACUUM ANNEALING ON THE MAGNETIC PULSED AMORPHOUS Fe52Co34Hf7B6Cu1 ALLOY[J]. Acta Metall Sin, 2012, 48(6): 749-752.
| [1] Kowalczyk M, Ferenc J, Liang X B, Kulik T. J Magn Magn Mater,2006; 04: e651[2] Liang X B, Ferenc J, Kulik T, Xu B S. Mater Sci Eng,2006; A426: 169[3] Liang X B, Kulik T, Ferenc J, Kowalczyk M, Vlasak G, Sun W S,Xu B S. Physica, 2005; 370B: 151[4] Kulik T, Liang X B, Ferenc J, Xu B S. Surf Eng China, 2004; 68: 1 (Kulik T, 梁秀兵, Ferenc J, 徐滨士. 中国表面工程, 2004; 68: 1)[5] Blazquez J S, Franco V, Conde C F, Conde A, Ferenc J, Kulik T. J Non--Cryst Solids, 2007; 353: 872[6] Xiao S H, Chao Y S, Zhou B L. Acta Phys Sin, 2000; 49: 288 (肖素红, 晁月盛, 周本濂, 物理学报, 2000; 49: 288)[7] Chao Y S, Li M Y, Geng Y, Liu J G. Acta Phys Sin, 2004; 53: 3453 (晁月盛, 李明扬, 耿岩, 刘吉刚. 物理学报2004; 53: 3453)[8] Chao Y S, Zhang Y H, Guo H, Zhang L, Wang X G. Acta Metall Sin,2007; 43: 231 (晁月盛, 张艳辉, 郭红, 张莉, 王兴刚. 金属学报, 2007; 43: 231)[9] Chao Y S, Zhu H X, Li Z M. J Phys, 2009; 188: 012038[10] Kopcewicz M, Gonser U, Wagner H G. Appl Phys, 1980; 23: 1[11] Kopcewicz M, Wagner H G, Gonser U. J Magn Magn Mater,1983; 40: 139[12] Majumdar B, Bysak S, Akhtar D. J Magn Magn Mater, 2007; 309: 300[13] Chao Y S, Guo H, Gao X Y, Luo L P, Zhu H X. Acta Phys Sin,2011; 60: 017504 (晁月盛, 郭红, 高翔宇, 罗丽平, 朱涵娴. 物理学报, 2011; 60: 017504)[14] Sato K, Murakami H, Kobayashi Y, Sprengel W, Schaefer H E. J Non-Cryst Solids, 2007; 353: 1882[15] Tian S. Physical Properties of Materials. Beijing: Aviation and Aerospace University Press, 2000: 265 (田莳. 材料物理性能. 北京: 北京航空航天大学出社, 2000: 265) |
|