Cu熔体中原子团簇在凝固过程中的演变规律分子动力学模拟 |
坚增运1,李娜1,常芳娥1,方雯1,赵志伟1,董广志1,介万奇2
|
1. 西安工业大学材料科学与化工学院, 西安710032
2. 西北工业大学凝固技术国家重点实验室, 西安 710072 |
|
MOLECULAR DYNAMICS SIMULATION OF THE ATOM CLUSTER EVOLUTION IN COPPER MELT DURING SOLIDIFICATION PROCESS |
JIAN Zengyun1, LI Na1, CHANG Fang'e1, FANG Wen1, ZHAO Zhiwei1, DONG Guangzhi1,JIE Wanqi2 |
1. School of Materials Science and Chemical Engineering, Xi'an Technological University, Xi'an 710032
2. State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072 |
引用本文:
坚增运,李娜,常芳娥,方雯,赵志伟,董广志,介万奇. Cu熔体中原子团簇在凝固过程中的演变规律分子动力学模拟[J]. 金属学报, 2012, 48(6): 703-708.
,
,
,
,
,
,
.
MOLECULAR DYNAMICS SIMULATION OF THE ATOM CLUSTER EVOLUTION IN COPPER MELT DURING SOLIDIFICATION PROCESS[J]. Acta Metall Sin, 2012, 48(6): 703-708.
[1] Gibson J M. Science, 2009; 326: 942
[2] Bernal J. Nature, 1959; 183: 141
[3] Qi D W, Wang S. Phys Rev, 1991; 44B: 884
[4] Liu R S, Dong K J, Tian Z A, Liu H R, Peng P, Yu A B. J Phys: Comdens Matter, 2008; 19: 196103
[5] Wang R S, Hou H Y, Chen G L. Acta Metall Sin, 2009; 45: 692
(王荣山, 候怀宇, 陈国良. 金属学报, 2009; 45: 692)
[6] Mondal K, Murty B S. J Non--Crystalline Solids,2006; 352: 5257
[7] Li Y D, Hao Q H, Cao Q L, Liu C S. Phy Rev, 2008; 78B: 174202
[8] Cheng Z N, Luo X C, Ma J P, Shao J, Chen N Y. Sci China, 1991; 4A: 440
(程兆年, 罗学才, 马剑鹏, 邵俊, 陈念贻.中国科学, 1991; 4A: 440)
[9] Hui X D, Liu X J, Gao R, Hou H Y, Fang H Z, Liu X K, Chen G L. Sci China, 2008; 38G: 406
(惠希东, 刘雄军, 高蕊, 侯怀宇, 方华志, 刘梓葵, 陈国良.中国科学, 2008; 38G: 406)
[10] Liu H R, Liu R S, Zhang A L, Hou Z Y, Wang X, Tian Z A. Chin Phys, 2007; 16, 3747
[11] Li J Y, Liu R S, Zhou Z, Xie Q, Peng P. J Mater Sci Technol, 1998; 14: 461
[12] Ten Wolde P R, Ruiz-Montero M J, Frenkel D. J Chem Phys, 1996; 104: 9932
[13] Malley B O, Snook I. Phys Rev Lett, 2003; 90: 085702
[14] Jian Z Y, Chen J, Chang F E, Zeng Z, He T, Jie W Q. Sci China, 2010; 53E: 3203
[15] Liu C S, Xia J C, Zhu Z G, Sun D Y. J Chem Phys,2001; 114: 7506
[16] Mishin Y, Mehl M J, Papaconstantopoulos D A, Voter A F, Kress J D. Phys Rev, 2001; 63B: 224106
[17] Morris J R, Wang C Z, Ho K M, Chan C T. Phys Rev,1994; 49B: 3109
[18] Honeycutt J D, Andersen H C. J Phys Chem, 1987; 91: 4950
[19] Zhao Y, Hu Z Q, Zhao J Z. Acta Metall Sin,2008; 44: 1157
(赵毅, 胡壮麒, 赵九洲. 金属学报, 2008; 44: 1157)
[20] Turkdogen E T. Physical of High Temperature Techonlogy.New York: Academic Press, 1980: 1
[21] Jian Z Y, Li N, Zhu M, Chen J, Chang F E, Jie W Q. Acta Mater, 2012; 60: 3590
[22] David R. CRC Handbook of Chemistry and Physics.Tokyo: CRC Press, 1989: 1
[23] Jian Z Y, Chang F E, Ma W H, Yan W. Sci China, 2000; 30E: 10
[24] Brandes E A, Brook G B. Smithells Metals Refrence Book.7th ed., Oxford: Butterworth, 1992: 1
[25] Guthrie R I L, Iida T. Mater Sci Eng, 1994; A178: 35
[26] Barin I, Knacke O. Thermochemical Properties of Inorganic Substances. Berlin: Springer-Verlag, 1973: 1 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|