| Al-6.3Zn-2.8Mg-1.8Cu铸造铝合金的组织和室温力学性能 |
| 杨光昱,孟宏帅,齐元昊,刘少军,介万奇 |
| 西北工业大学凝固技术国家重点实验室, 西安 710072 |
|
| MICROSTRUCTURES AND ROOM TEMPERATURE MECHANICAL PROPERTIES OF Al–6.3Zn–2.8Mg–1.8Cu CASTING ALUMINUM ALLOY |
| YANG Guangyu, MENG Hongshuai, LIU Shaojun, QI Yuanhao, JIE Wanqi |
| State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi’an 710072 |
引用本文:
杨光昱 孟宏帅 齐元昊 刘少军 介万奇. Al-6.3Zn-2.8Mg-1.8Cu铸造铝合金的组织和室温力学性能[J]. 金属学报, 2012, 48(2): 211-219.
,
,
,
,
.
MICROSTRUCTURES AND ROOM TEMPERATURE MECHANICAL PROPERTIES OF Al–6.3Zn–2.8Mg–1.8Cu CASTING ALUMINUM ALLOY[J]. Acta Metall Sin, 2012, 48(2): 211-219.
| [1] Heinz A, Haszler A, Keidel C, Moldenhauer S. Mater Sci Eng, 2000; A280: 102[2] Srivatsan T S. J Mater Sci, 1992; 27: 4772[3] Zakharov V V, Rostova T D. Met Sci Heat Treat, 1995; 37(5–6): 203[4] Mukhopadhyay A K, Reddy G M, Prasad K S, Varma V K, Mondac C. In: Nie J F, Morton A J, Muddle B C, eds., Proc 9th Int Conf on Aluminium Alloys, Australia: Instituteof Materials Engineering Australia Ltd, 2004: 883[5] Wang H B, Huang J F, Yang B, Zhang J S, Zhang Y A, Xiong B Q. Mater Rev, 2003; 17(9): 1(王洪斌, 黄进峰, 杨滨, 张济山, 张永安, 熊柏青. 材料导报, 2003; 17(9): 1)[6] Chen C Q. Chin J Nonferrour Met, 2002; 12(3): 22(陈昌麒. 中国有色金属学报, 2002; 12(3): 22)[7] Chen K H, Liu H W, Zhang Z, Li S, Todd R I. J Mater Process Technol, 2003; 142: 190[8] Mondal C, Mukhopadhyay A K. Mater Sci Eng, 2005; A391: 367[9] Xie F Y, Yan X Y, Ding L, Zhang F, Chen S L, Chu M G, Chang Y A. Mater Sci Eng, 2003; A355: 144[10] Manish D D. PhD Thesis, Georgia Institute of Technology, 2000[11] Fan X G. PhD Thesis, Harbin Institute of Technology, 2007(樊喜刚. 哈尔滨工业大学博士学位论文, 2007)[12] Fan X G, Jiang D M, Meng Q C, Zhong L. Mater Lett, 2006; 60: 1475[13] Starink M J, Wang S C. Acta Mater, 2003; 51: 5131[14] Poole W J, Sæter J A, Skjervold S, Watercoo G. Metall Mater Trans, 2000; 31A: 2327[15] Starink M J, Li X M. Metall Mater Trans, 2003; 34A: 899[16] You W, Lin S Y. Alum Fabr, 1999; 22(1): 4(游文, 林顺岩. 铝加工, 1999; 22(1): 4)[17] Si N C, Fu M X. Nonferrous Metal Material and Preparation. Beijing: Chemical Industry Press, 2006: 36(司乃潮, 傅明喜. 有色金属材料及制备. 北京: 化学工业出版社, 2006: 36)[18] Li Y Y, Guo GW, Luo Z Q, Long Y. Spec Cast Nonferrous Alloys, 2000; 6: 45(李元元, 郭国文, 罗宗强, 龙雁. 特种铸造及有色合金, 2000; 6: 45)[19] Li N K, Cui J Z. Light Alloy Fabr Technol, 2008; 36(1): 5(李念奎, 崔建忠. 轻合金加工技术, 2008; 36(1): 5)[20] Zhang B C. Nonferrous Metal and Heat–treatment. Xi’an: NWPU Industry Press, 1993: 62(张宝昌. 有色金属及其热处理. 西安: 西北工业大学出版社, 1993: 62)[21] Sheppard T. Extrusion of Aluminium Alloy. London: Kluwer Academic Publisher, 1999: 23[22] Alekseev A A, Fridlyander I N, Berg L B. Mater Sci Forum, 2002; 396–342: 821[23] Rokhlin L L, Dobatkina T V, Bochvar N R, Lysova E V. J Alloys Compd, 2004; 367: 10[24] Metallographic Atlas Compilation Group. Wrought Aluminum Alloy Metallographic Atlas. Beijing: Metallurgical Industry Press, 1975: 157(金相图谱编写组. 变形铝合金金相图谱. 北京: 冶金工业出版, 1975: 157)[25] Ding H L, Xin Z H. Practical Aluminum, Copper and Its Alloys Heat Treatment and Metallurgical Failure Analysis. Beijing: Machinery Industry Press, 2008: 102(丁惠麟, 辛智华. 实用铝、铜及其合金金相热处理和失效分析. 北京: 机械工业出版社, 2008: 102)[26] Lu S S, Gu K D, Zheng L S. Nonferrous Casting Alloys and Melting. Beijing: National Defense Industry Press, 1983: 52(陆树荪, 顾开道, 郑来苏. 有色铸造合金及熔炼. 北京: 国防工业出版社, 1983: 52) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|