| 2024铝合金薄板激光冲击波加载的实验研究 |
| 冯爱新1,2,聂贵锋1, 薛伟2,曹宇鹏1,3, 徐晓翔1, 李彬1, 施芬1 |
1. 江苏大学机械工程学院, 镇江 212013
2. 温州大学机械工程学院, 温州 325035
3. 南通大学机械工程学院, 南通 226019 |
|
| EXPERIMENTAL RESEARCH ON LASER SHOCK WAVE LOADING MECHANISM OF 2024 ALUMINUM ALLOY SHEET |
| FENG Aixin 1,2, NIE Guifeng 1, XUE Wei 2, CAO Yupeng 1,3, XU Xiaoxiang 1, LI Bin 1, SHI Fen 1 |
1. School of Mechanical Engineering, Jiangsu University, Zhenjiang 212013
2. School of Mechanical Engineering, Wenzhou University, Wenzhou 325035
3. School of Mechanical Engineering, Nantong University, Nantong 226019 |
引用本文:
冯爱新 聂贵锋 薛伟 曹宇鹏 徐晓翔 李彬 施芬. 2024铝合金薄板激光冲击波加载的实验研究[J]. 金属学报, 2012, 48(2): 205-210.
,
,
,
,
,
.
EXPERIMENTAL RESEARCH ON LASER SHOCK WAVE LOADING MECHANISM OF 2024 ALUMINUM ALLOY SHEET[J]. Acta Metall Sin, 2012, 48(2): 205-210.
| [1] Zhang Y K, Hu C L, Cai L, Yang J C, Zhang X R. Appl Phys, 2001; 72A: 113[2] Zhang Y K, Lu J Z, Ren X D, Yao H B, Yao H X. Mater Des, 2009; 30: 1697[3] Zhang Y K, You J, Lu J Z, Cui C Y, Jiang Y F, Ren X D. Surf Coat Technol, 2010; 204: 3947[4] Lu J Z, Luo K Y, Feng A X, Zhong J W, Sun G F, Zhang L, Qian Xi M. Chin J Lasers, 2010; 37: 2664(鲁金忠, 罗开玉, 冯爱新, 钟俊伟, 孙桂芳, 张 磊, 钱晓明. 中国激光, 2010; 37: 2664)[5] Yang X, Zou H C, Dai S J. Appl Laser, 1998; 18(4): 179(杨 晓, 邹鸿承, 戴蜀娟. 应用激光, 1998; 18(4): 179)[6] Huang S, Zhou J Z, Jiang S Q, Zhu Y B, Hu L L. Chin J Lasers, 2010; 37: 256(黄舒, 周建忠, 蒋素琴, 朱银波, 胡玲玲. 中国激光, 2010; 37: 256)[7] Gu Y Y, Zhang L F, Lu J Z, Zhang Y K. Chin J Lasers, 2009; 36: 3318(顾永玉, 张凌峰, 鲁金忠, 张永康. 中国激光, 2009; 36: 3318)[8] Montross C S, Ye L. Int Fatigue, 2002; 24: 1021[9] Li Z Y, Zhu W H, Cheng J Y, Guo D H, Wu H X. Chin J Lasers, 1997; 24: 259.(李志勇, 朱文辉, 程经毅, 郭大浩, 吴鸿兴. 中国激光, 1997; 24: 259)[10] Liu L, Wang S B, Wu H X, Guo D H, Liao P Y. Laser Technol, 2007; 31: 134(刘丽, 王声波, 吴鸿兴, 郭大浩, 廖培育. 激光技术, 2007; 31: 134)[11] Tang T M, Zhang Y K. Nantong Inst Technol, 1999; 15(1): 26(唐通鸣, 张永康. 南通工学院学报, 1999; 15(1): 26)[12] Yu S S, Xiao H B, Wang F, Yuan B, Zhang Y K. Chin J Lasers, 2010; 37: 1386(于水生, 姚红兵, 王飞, 袁 蓓, 张永康. 中国激光, 2010; 37: 1386)[13] Liao P Y, Wang S B, Sheng J J, Liu L, Xia X P. Appl Laser, 2007; 27(2): 110(廖培育, 王声波, 盛晶晶, 刘 丽, 夏小平. 应用激光, 2007; 27(2): 110)[14] Tang Y X, Zhang Y K, Zhang H, Yu C Y. Trans Met Heat Treat, 1997; 18(4): 22(唐亚新, 张永康, 张宏, 余承业. 金属热处理学报, 1997; 18(4): 22)[15] Zhang L F, Zhang Y K, Ren X D, Feng A X. Trans Chin Soc Agric Machine, 2007; 38(1): 127(张凌峰, 张永康, 任旭东, 冯爱新. 农业机械学报, 2007; 38(1): 127)[16] Zhang Y K, Chen J F, Xu R J. Chin J Lasers, 2008; 35: 1067(张永康, 陈菊芳, 许仁军. 中国激光, 2008; 35: 1067)[17] Liu H W. Mechanics of Materials. Beijing: Higher Education Press, 2004: 216(刘鸿文. 材料力学. 北京: 高等教育出版社, 2004: 216)[18] Luo X M, Ma H, Zhang J W, Zhang Y K. Mater Rev, 2010; 24(3): 11(罗新民, 马 辉, 张静文, 张永康. 材料导报, 2010; 24(3): 11)[19] Yang X M. Numerical Simulation for Explosion and Phenomena. Hefei: University of Science and Technology of China Press, 2010: 31(杨秀敏. 爆炸冲击现象数值模拟. 合肥: 中国科学技术大学出版社, 2010: 31)[20] Hu Y X. PhD Thesis, Shanghai Jiao Tong University, 2008(胡永祥. 上海交通大学博士学位论文, 2008)[21] Gu Y Y, Zhang Y K, Zhang X Q, Shi J G. Acta Phys Sin, 2006; 55: 5885(顾永玉, 张永康, 张兴权, 史建国. 物理学报, 2006; 55: 5885)[22] Ma X Q. Impact Dynamics. Beijing: Beijing Institue of Technology Press, 1992: 1(马晓青. 冲击动力学. 北京:北京理工大学出版社, 1992: 1) |
|