5456铝合金PLC效应的两种临界机制研究 |
符师桦,程腾,张青川,曹鹏涛,胡琦 |
中国科学技术大学中国科学院材料力学行为和设计重点实验室, 合肥 230027 |
|
STUDY ON TWO CRITICAL MECHANISMS OF PLC EFFECT OF 5456 Al–BASED ALLOY |
FU Shihua, CHENG Teng, ZHANG Qingchuan, CAO Pengtao, HU Qi |
CAS Key Laboratory of Mechanical Behavior and Design of Materials, University of Science and Technology of China, Hefei 230027 |
引用本文:
符师桦 程腾 张青川 曹鹏涛 胡琦. 5456铝合金PLC效应的两种临界机制研究[J]. 金属学报, 2012, 48(12): 1453-1458.
FU Shihua CHENG Teng ZHANG Qingchuan CAO Pengtao HU Qi.
STUDY ON TWO CRITICAL MECHANISMS OF PLC EFFECT OF 5456 Al–BASED ALLOY[J]. Acta Metall Sin, 2012, 48(12): 1453-1458.
[1] Cottrell A H. Philos Mag, 1953; 44: 829
[2] Cieslar M, Fressengeas C, Karimi A, Martin J L. Scr Mater, 2003; 48: 1105
[3] Nagarjuna S, Anozie F N, Evans J T. Mater Sci Technol, 2003; 19: 1661
[4] Lu J Y, Jiang Z Y, Zhang Q C. Acta Metall Sin, 2006; 42:139
(卢俊勇, 蒋震宇, 张青川. 金属学报, 2006; 42: 139)
[5] Liu H W, Zhang Q C, Lu J Y, Xiang G F, Wu X P. Acta Metall Sin, 2006; 42: 925
(刘颢文, 张青川, 卢俊勇, 项国富, 伍小平. 金属学报, 2006; 42: 925)
[6] Sleeswyk A W. Acta Metall, 1958; 6: 598
[7] Mulford R A, Kocks U F. Acta Metall, 1979; 27: 1125
[8] McCormick P G. Acta Metall, 1988; 36: 3061
[9] Springer F, Nortmann A, Schwink C. Phys Status Solidi, 1998; 170A: 63
[10] Klose F B, Ziegenbein A, Weidenm¨uller J, Neuh¨auser H, Hahner P. Comput Mater Sci, 2003; 26: 80
[11] Balik J, Lukac P, Kubin L P. Scr Mater, 2000; 42: 465
[12] Chihab K, Fressengeas C. Mater Sci Eng, 2003; A356: 102
[13] Peng K P, Chen W Z, Qian K W. Mater Sci Eng, 2006;A419: 53
[14] Cui C Y, Gu Y F, Yuan Y, Harada H. Scr Mater, 2011;64: 502
[15] Kubin L P, Estrin Y. Acta Metall Mater, 1990; 38: 697
[16] McCormick P G. Acta Metall, 1972; 20: 351
[17] Brechet Y, Estrin Y. Acta Metall Mater, 1995; 43: 955
[18] Cai M C, Niu L S, Yu T, Shi H J, Ma X F. Mater Sci Eng,2010; A527: 5175
[19] Rodriguez P, Venkadesan S. Solid State Phenom, 1995;42–43: 257
[20] Soare M A, Curtin W A. Acta Mater, 2008; 56: 4091
[21] Flor H, Neuh¨auser H. Acta Metall, 1980; 28: 939
[22] Rizzi E, H¨ahner P. Int J Plasticity, 2004; 20: 121
[23] Hu Q, Zhang Q C, Cao P T, Fu S H. Acta Mater, 2012; 60: 1647 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|