| 不锈钢薄板高速激光焊驼峰焊道形成倾向及其影响因素 |
| 裴莹蕾1,单际国1,2,任家烈1 |
1. 清华大学机械工程系, 北京 100084\par
2. 清华大学 先进成形制造教育部重点实验室, 北京 100084 |
|
| STUDY OF HUMPING TENDENCY AND AFFECTING FACTORS IN HIGH SPEED LASER WELDING OF STAINLESS STEEL SHEET |
| PEI Yinglei 1, SHAN Jiguo 1,2, REN Jialie 1 |
1. Department of Mechanical Engineering, Tsinghua University, Beijing 100084
2. Key Laboratory for Advanced Materials Processing Technology, Ministry of Education, Tsinghua University, Beijing 100084 |
引用本文:
裴莹蕾 单际国 任家烈. 不锈钢薄板高速激光焊驼峰焊道形成倾向及其影响因素[J]. 金属学报, 2012, 48(12): 1431-1436.
PEI Yinglei SHAN Jiguo REN Jialie.
STUDY OF HUMPING TENDENCY AND AFFECTING FACTORS IN HIGH SPEED LASER WELDING OF STAINLESS STEEL SHEET[J]. Acta Metall Sin, 2012, 48(12): 1431-1436.
| [1] Albright C E, Chiang S. In: Santa C ed., ICALEO’88 proceedings, Berlin/IFS: Springer, 1988: 207[2] Nguyen T C, Weckman D C, Johnson D A, Kerr H W. Sci Technol Weld Join, 2006; 11: 618[3] Wei P S. J Heat Transfer, 2011; 133: 031005–1[4] Nguyen T C, Weckman D C. Sci Technol Weld Join, 2005; 10: 447[5] Nguyen T C, Weckman D C. Johmson D A. Weld J, 2007; 86: 360[6] Hu Z K, Wu C S. Acta Metall Sin, 2008; 44: 1445(胡志坤, 武传松. 金属学报, 2008; 44: 1445)[7] Chen J, Wu C S. Acta Metall Sin, 2009; 45: 1070(陈姬, 武传松. 金属学报, 2009; 45: 1445)[8] Wu C S, Hu Z K, Zhang Y M. Proc Inst Mech Eng, 2009; 233B: 751[9] Ueyama T, Ohnawa T, Tanaka M, Nakata K. Sci Technol Weld Join, 2005; 10: 750[10] Soderstrom E, Mendez P. Sci Technol Weld Join, 2006; 11: 572[11] Cho M H, Farson D F. Metall Mater Trans, 2007; 38B: 305[12] Fabbro R. J Phys, 2010; 43D: 445501[13] Katayama S, Yoheia A, Mizutania M, Kawahitoa Y. In:Elsevier P O ed., Lasers in Manufacturing 2011–Proc 6th Int WLT Conference on Lasers in Manufacturing, Netherlands:Physics Procedia, 2011: 75[14] Kawahito Y, Mizutani M, Katayama S. J Phys, 2007; 40D: 5854[15] Wei P S, Chuang K C, Ku J S, Debory T. IEEE Trans Comp Packag Manufact Technol, 2012; 2: 383[16] Kawahito Y, Mizutani M, Katayama S. Sci Technol Weld Join, 2009; 14: 588[17] Zhang L J, Zhang J X, Wang R, Gong S L. Rare Met Mater Eng, 2006; S2: 39(张林杰, 张建勋, 王蕊, 巩水利. 稀有金属材料与工程, 2006; S2: 39)[18] Berger P, H¨ugel H, Hess A, Weber R, Graf T. In: Elsevier P O ed., Lasers in Manufacturing 2011 – Proc 6th Int WLT Conferenceon Lasers in Manufacturing, Netherlands: Physics Procedia, 2011: 232[19] Eriksson I, Powell J, Kaplan A F H. Sci Technol Weld Join, 2011; 16: 636[20] Chen J. PhD Thesis, Shandong University, Jinan, 2009(陈姬. 山东大学博士学位论文, 济南, 2009)[21] Amara E H, Fabbro R. Appl Phys, 2010; 101A: 111[22] Mendez P F, Eagar T W. Weld J, 2003; 82: 296[23] Bradstreet B J. Weld J, 1968; 47: 314[24] Gratzke U, Kapadia P D, Dowden J, Kroos J, Simon G. J Phys, 1992; 25D: 1640[25] Kumar A, Debroy T. Weld J, 2006; 85: 292 |
|