| 变形合金的亚晶组织演化的相场模型 |
| 高英俊1,2,3,罗志荣1,2,黄礼琳1,2,胡项英2 |
1. 广西大学教育部工程防灾与结构安全重点实验室, 南宁 530004
2. 广西大学物理科学与工程技术学院, 南宁 530004
3. 中国科学院国际材料物理中心, 沈阳 110016 |
|
| PHASE FIELD MODEL FOR MICROSTRUCTURE EVOLUTION OF SUBGRAIN IN DEFORMATION ALLOY |
| GAO Yingjun 1,2,3, LUO Zhirong 1,2, HUANG Lilin 1,2, HU Xiangying 2 |
1. Key Lab of Engineering Disaster Prevention and Structural Safety of China Ministry of Education, Guangxi University, Nanning 530004
2. College of Physics Science and Engineering, Guangxi University, Nanning 530004
3. International Center for Materials Physics, Chinese Academy of Science, Shenyang 110016 |
引用本文:
高英俊 罗志荣 黄礼琳 胡项英. 变形合金的亚晶组织演化的相场模型[J]. 金属学报, 2012, 48(10): 1215-1222.
GAO Yingjun LUO Zhirong HUANG Lilin HU Xiangying.
PHASE FIELD MODEL FOR MICROSTRUCTURE EVOLUTION OF SUBGRAIN IN DEFORMATION ALLOY[J]. Acta Metall Sin, 2012, 48(10): 1215-1222.
| [1] Yang X Y, Zhu Y K, Zhang L. Chin J Mater Res, 2010; 24: 169(杨续跃, 朱亚坤, 张 雷. 材料研究学报, 2010; 24: 169)[2] Yang X Y, Jiang Y P. Acta Metall Sin, 2010; 46: 451(杨续跃, 姜育培. 金属学报, 2010; 46: 451)[3] Humphreys F J, HatherlyM. Recrystallization and Related Annealing Phenomena. Oxford: Elsevier Science, 1995: 1[4] Wu X X, Yang X Y, Zhang L, Zhang Z L. Acta Metall Sin, 2011; 47: 140(吴新星, 杨续跃, 张雷, 张之岭. 金属学报, 2011; 47: 140)[5] Kim K H, Suh B C, Bac J H. Scr Mater, 2010; 63: 716[6] Chun Y B, Hwang S K. Acta Mater, 2008; 56: 369[7] Huang M X, Pedro E J, Castillo R D, Bouaziz O, Zwaag S. Acta Mater, 2009; 57: 3431[8] Baudin T, Julliard F, Paillard P, Penelle R. Scr Mater, 2000; 43: 63[9] Choi S H, Cho J H. Mater Sci Eng, 2005; A405: 86[10] Sepehrband P, Esmaeli S. Scr Mater, 2010; 63: 4[11] Zheng C W, Lan Y J, Xiao N M, Li D Z, Li Y Y. Acta Metall Sin, 2006; 42: 474(郑成武, 兰勇军, 肖纳敏, 李殿中, 李依依. 金属学报, 2006; 42: 474)[12] Raabe D, Hautchrli L. Comput Mater Sci, 2005; 34: 299[13] Raabe D. Annu Rev Mater Res, 2002; 32: 53[14] Radhakrishnan B, Sarma G. Philos Mag, 2004; 84: 2341[15] Takaki T, Yamanaka A, Higa Y, Tomita Y. Mater Trans, 2008; 49: 2559[16] Gao Y J, Luo Z R, Hu X Y, Huang C G. Acta Metall Sin, 2010; 46: 1161(高英俊, 罗志荣, 胡项英, 黄创高. 金属学报, 2010; 46: 1161)[17] Takaki T, Tomita Y. Int J Mech Sci, 2010; 52: 320[18] Fan D, Chen L Q. Acta Mater, 1997; 45: 3297[19] Wang M T, Zong B Y, Wang G. Comput Mater Sci, 2009; 45: 217[20] Gao Y J, Luo Z R, Zhang S Y, Huang C G. Acta Metall Sin, 2010; 46: 1473(高英俊, 罗志荣, 张少义, 黄创高. 金属学报, 2010; 46: 1473)[21] Zhao P. Fundamental Course of Materials Science. Harbin: Harbin Institute of Technology Press, 1998: 148(赵品. 材料科学基础教程. 哈尔滨: 哈尔滨工业大学出版社, 1998: 148)[22] Oono Y, Pori S. Phys Rev Lett, 1987; 58: 836[23] Sitdikov O, Sakai T, Avtokratova E, Kaibyshev R, Tsuzaki K, Watanabe Y. Acta Mater, 2008; 56: 821[24] Pennock G M, Drury M R, Spiers C J. J Struct Geology, 2005; 27: 2159[25] Xu S W. Master Thesis, Harbin Institute of Technology, 2006(徐世伟. 哈尔滨工业大学硕士学位论文, 2006) |
|