| 固溶处理对Ni-Co基高温合金反常动态应变时效的影响 |
| 田成刚1,崔传勇1,谷月峰2,孙晓峰1 |
1. 中国科学院金属研究所, 沈阳 110016
2. 日本国立材料研究所, 筑波 305--0047 |
|
| EFFECT OF SOLUTION TREATMENT ON THE INVERSE DYNAMIC STRAIN AGING OF A Ni–Co BASE SUPERALLOY |
| TIAN Chenggang 1, CUI Chuanyong 1, GU Yuefeng 2, SUN Xiaofeng 1 |
1. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
2. National Institute for Materials Science, Tsukuba 305–0047, Japan |
引用本文:
田成刚 崔传勇 谷月峰 孙晓峰. 固溶处理对Ni-Co基高温合金反常动态应变时效的影响[J]. 金属学报, 2012, 48(10): 1223-1228.
TIAN Chenggang CUI Chuanyong GU Yuefeng SUN Xiaofeng.
EFFECT OF SOLUTION TREATMENT ON THE INVERSE DYNAMIC STRAIN AGING OF A Ni–Co BASE SUPERALLOY[J]. Acta Metall Sin, 2012, 48(10): 1223-1228.
| [1] Portevin A, Le Chatelier F. Comp Rend Acad Sci (Paris), 1923; 176: 50[2] Brehet Y, Estrin Y. Acta Metall Mater, 1995; 43: 955[3] Cottrell A H. Philos Mag, 1953; 44: 829[4] McCormick P G. Acta Metall, 1972; 20: 351[5] Beukel Den Van A. Phys Stat Sol, 1975; 30: 197[6] Hayes R W, Hayes W C. Acta Metall, 1982; 30: 1295[7] Nalawade S A, Sundararaman M, Kishore R, Shah J G. Scr Mater, 2008; 59: 991[8] Hale C L, Rollings W S, Weaver M L. Mater Sci Eng, 2001; A300: 153[9] Chen W, Chaturvedi M C. Mater Sci Eng, 1997; A229: 163[10] Hayes R W. Acta Metall, 1982; 30: 1295[11] Shankar V, Valsan M, Rao K B S, Mannan S L. Metall Mater Trans, 2004; 35A: 3129[12] Sharghi–Mashtaghin R, Asgari S. Mater Sci Eng, 2008; A486: 376[13] Roy A K, Pal J, Mukhopadhyay C. Mater Sci Eng, 2008; A474: 363[14] Gopinath K, Gogia A K, Kamat S V, Ramamurty U. Acta Mater, 2009; 57: 1243[15] Hollomon H. Trans AIME, 1945; 162: 268[16] Samuel K G. J Phys, 2006; 39D: 203[17] Qian K W, Reed–Hill R E. Acta Metall, 1983; 31: 87[18] Venkadesan S, Phaniraj C, Sivaprassad P V, Rodriguez P. Acta Metall Mater, 1992; 40: 569[19] Pink E. Scr Metall, 1983; 17: 847[20] Gale W F, Totemeier T C. Smithells Metals Reference Book. London: Butterworth–Heinemann, 2004: 3[21] Nakada Y, Keh A S. Acta Metall, 1970; 18: 437[22] Srinivasan R, Banerjee R, Hwang J Y, Viswanathan G B, Tiley J, Dimiduk D M, Fraser H L. Phys Rev Lett, 2009; 102: 086101[23] Hwang J Y, Nag S, Singh A R P, Srinivasan R, Tiley J, Viswanathan G B, Fraser H L, Banerjee R. Metall Mater Trans, 2009; 40A: 3059[24] Hwang J Y, Nag S, Singh A R P, Srinivasan R, Tiley J, Fraser H L, Banerjee R. Scr Mater, 2009; 61: 92[25] Hwang J Y, Banerjee R, Tiley J, Srinivasan R, Viswanathan G B, Fraser H L. Metall Mater Trans, 2009; 40A: 24[26] Sleewyk A W. Acta Metall, 1958; 6: 598[27] Lloyd D J, Chung D W, Chaturvedi M C. Acta Metall, 1975; 23: 93[28] Xiao L G, Li X Q, Qian K W. Sci China, 1990; 4A: 423(萧林刚, 李效琦, 钱匡武. 中国科学, 1990; 4A: 423)[29] Xiao L G, Li X Q, Qian K W. Sci China, 1990; 33A: 1386[30] Qian K W, Li X Q, Xiao L G. J Fuzhou Univ, 2001; 6: 8(钱匡武, 李效琦, 萧林刚. 福州大学学报, 2001; 6: 8) |
|