| 3种锆合金的高温氧化行为 |
| 邱军, 赵文金, Thomas Guilbert, Jean-Luc Bechade |
1) 中国核动力研究设计院反应堆燃料及材料重点实验室, 成都 610041
2) 法国原子能委员会Scalay研究中心, Gif-sur-Yvette cedex 91191, 法国 |
|
| HIGH TEMPERATURE OXIDATION BEHAVIOURS OF THREE ZIRCONIUM ALLOYS |
| QIU Jun, ZHAO Wenjin Thomas Guilbert Jean-Luc Bechade |
1) Science and Technology on Reactor Fuel and Materials Laboratory, Nuclear Power Institute of China, Chengdu 610041
2) French Atomic Energy and Alternative Energies Commission, Gif-sur-Yvette cedex 91191, France |
引用本文:
邱军 赵文金 Thomas Guilbert Jean-Luc Bechade. 3种锆合金的高温氧化行为[J]. 金属学报, 2011, 47(9): 1216-1220.
,
.
HIGH TEMPERATURE OXIDATION BEHAVIOURS OF THREE ZIRCONIUM ALLOYS[J]. Acta Metall Sin, 2011, 47(9): 1216-1220.
| [1] Baker L, Just L C. ANL–6548, AEC Research and Development Report, Argonne National Laboratory, 1962[2] Pawel K E, Cathcart J V, Mckee R A. Electrochem Sci Techol, 1979; 126: 1105[3] Leistikow S, Schanze G. Nucl Eng Des, 1987; 103: 65[4] Nagase F. Otomo T, Uetsuka H. Nucl Sci Technol, 2003; 40: 213[5] Sabol G P, Comstock R J, Weiner R, Larouere A P, Stanutz R N. In: Bradly E R, Sabol G P eds., Zirconium in the Nuclear Industry Tenth International Symposiu. ASTM STP 1245, Philadelphia: ASTM International, 1994: 724[6] Etoh Y, Shimada S, Yasuda T, Ikeda T, Adamson R B, Chen J F, Ishii Y, Takai K. In: Paul D B, Davidson R R eds., Zirconium in the Nuclear Industry Nineth International Symposium, ASTM STP 1129, West Conshohocken, PA: ASTM International, 1992,: 825[7] Choo K N, Kim Y S. J Nucl Mater, 2001; 297: 5247[8] Kim J M, Jeong Y H. J Nucl Mater, 1999; 275: 74[9] Billone M, Yan C, Burtseva Y, Chung H M. In: Fuketa T ed., Summary of Fuel Safety Research Meeting 2005, Tokyo: Japan Atomic Energy Agency, 2006: 168[10] Asmolov V, Yegorova L, Lioutov K, Konoveyev A, Smirnov V, Goryachev A, Chesanov V, Prokhorov V. In: Monteleone S, Nesmith S eds., Proceeding of the 2002 NuclearSafety Research Conference, Washingdon D. C.: Nuclear Regulation Commission, 2003: 109[11] Baek J H, Park K B, Jeong Y H. J Nucl Mater, 2004; 335: 443[12] Zhao W J. Rare Met Lett, 2004; 23(5): 15(赵文金. 稀有金属快报, 2004; 23(5): 15)[13] Li C, Zhou B X, Zhao W J, Li P, Peng Q, Ying S H, Shen B L. J Nucl Mater, 2002; 304: 134[14] Peng J H, Li W F, Bechade J L, Maury R. Chin J Rare Met, 2008; 32(1): 1(彭继华, 李文芳, Bechade J L, Maury R. 稀有金属, 2008; 32(1): 1)[15] Xue X Y, Bai X D, Tan Z Y, Zhou Q S, Liu J Z. Rare Met Mater Eng, 2004; 33(9): 902(薛祥义, 白新德, 田振业, 周青山, 刘建章. 稀有金属材料与工程, 2004; 33(9): 902)[16] American Society for Metals, Metals Handbook Vol.8. 8th Ed., Materials Park: ASM International, 1971: 327 |
|