| 辐照与He协同作用对低活度铁素体/马氏体钢F82H微观结构的影响 |
| 佟振峰, 戴勇, 杨文, 杨启法 |
1) 中国原子能科学研究院, 北京 102413
2) Paul Scherrer Institut, 5232 Villigen PSI, Switzerland |
|
| EFFECTS OF RADIATION AND He ON MICROSTRUCTURES OF LOW ACTIVE FERRITIC/MARTENSITIC STEEL F82H |
| TONG Zhenfeng, DAI Yong, YANG Wen, YANG Qifa |
1) China Insitute of Atomic Energy, Beijing 102413
2) Paul Scherrer Institut, 5232 Villigen PSI, Switzerland |
引用本文:
佟振峰 戴勇 杨文 杨启法. 辐照与He协同作用对低活度铁素体/马氏体钢F82H微观结构的影响[J]. 金属学报, 2011, 47(7): 965-970.
,
.
EFFECTS OF RADIATION AND He ON MICROSTRUCTURES OF LOW ACTIVE FERRITIC/MARTENSITIC STEEL F82H[J]. Acta Metall Sin, 2011, 47(7): 965-970.
| [1] Klueh R L, Harries D R. High–Chromium Ferritic and Martensitic Steels for Nuclear Applications. West Conshohocken, PA: ASTM, 2001: 19[2] Kohyama A, Hishinuma A, Gelles D S, Klueh R L, Dietz W, Ehrlich K. J Nucl Mater, 1996; 233–237: 138[3] Miwa Y, Wakai E, Shiba K, Hashimoto N, Robertson J P, Rowcli A F, Hishinuma A. J Nucl Mater, 2000; 283–287: 334[4] Schaublin R, Spatig P, Victoria M. J Nucl Mater, 1998; 258–263: 1178[5] Sawai T,Wakai E, TomitaT, NaitoA, Jitsukawa S. J Nucl Mater, 2002; 307–311: 312[6] Spatig P, Schaublin R, Gyger S, Victoria M. J NuclMater, 1998; 258–263: 1345[7] Shiba K, Suzuki M, Hishinuma A. J Nucl Mater, 1996; 233–237: 309[8] Jitsukawa S, Tamura M, vander Schaaf B, Klueh R L, Alamo A, Petersen C, Schirra M, Spaetig P, Odette G R, Tavassoli A A, Shiba K, Kohyama A, Kimura A. J Nucl Mater, 2002; 307–311: 179[9] Stamm U, Schroeder H. J Nucl Mater, 1988; 155–157: 1059[10] Ullmaier H. Radiat Eff, 1983; 78: 1[11] Klueh R L, Hashimoto N, Sokolov M A, Shiba K, Jitsukawa S. J Nucl Mater, 2006; 357: 156[12] Malaplate J, Vincent L, Averty X, Henry J, Marini B. Eng Fract Mech, 2008; 75: 3570[13] Henry J, Vincent L, Averty X, Marini B, Jung P. J Nucl Mater, 2007; 367–370: 411[14] Tong Z, Dai Y. J Nucl Mater, 2010; 398: 43[15] Gupta G, Jiao Z, Ham A N, Busby J T, Was G S. J Nucl Mater, 2006; 351: 162[16] Dai Y, Foucher Y, James M R, Oliver B M. J Nucl Mater, 2003; 318: 167[17] Jiao Z, Ham N, Was G S. J Nucl Mater, 2007; 367–370: 440[18] Trinkaus H, Singh B N. J Nucl Mater, 2003; 323: 229[19] Jia X, Dai Y. J Nucl Mater, 2006; 356: 105 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|