25Cr2Ni4MoV钢锻造过程孔洞缺陷愈合规律研究 |
李世键, 孙明月, 刘宏伟, 李殿中 |
中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016 |
|
STUDY ON VOID HEALING BEHAVIOR DURING FORGING PROCESS FOR 25Cr2Ni4MoV STEEL |
LI Shijian, SUN Mingyue, LIU Hongwei, LI Dianzhong |
Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
李世键 孙明月 刘宏伟 李殿中. 25Cr2Ni4MoV钢锻造过程孔洞缺陷愈合规律研究[J]. 金属学报, 2011, 47(7): 946-953.
.
STUDY ON VOID HEALING BEHAVIOR DURING FORGING PROCESS FOR 25Cr2Ni4MoV STEEL[J]. Acta Metall Sin, 2011, 47(7): 946-953.
[1] National Development and Reform Commission. Nuclear Power Medium– and Long–term Development Program 2005—2020, May, 2007
(国家发展和改革委员会. 核电中长期发展规划(2005-2020年). 2007年5月)
[2] Sigworth G K, Wang C M. Metall Trans, 1993; 24B: 349
[3] Lu Y. The Theory and Process of Forging. Beijing: China Machine Press, 1991: 321
(吕炎. 锻压成形理论与工艺. 北京: 机械工业出版社, 1991: 321)
[4] Kallstrom R. Scand J Metall, 1983; 12: 121
[5] Cook P M. J Iron Steel Inst Jpn, 1959; 4: 250
[6] Wang L G, Huang Y, Liu Z B. J Plast Eng, 2002; 9(2): 28
(王雷刚, 黄瑶, 刘助柏. 塑性工程学报, 2002; 9(2): 28)
[7] Park C Y, Yang D Y. J Mater Process Technol, 1996; 57: 129
[8] Wang A, Thomson P F, Hodgson P D. J Mater Process Technol, 1996; 60: 95
[9] Chen K, Yang Y T, Liu K J, Shao G J. Adv Mater Res, 2010; 11: 3079
[10] Zhang X X, Cui Z S. Appl Math Mech (Engl Ed), 2009; 30: 631
[11] Zhu M. J Beijing Inst Technol, 1990; 10(2): 58
(朱明. 北京理工大学学报, 1990; 10(2): 58)
[12] Cui Z S, Ren G S, Xu B Y, Xu C G, Liu G H. J Tsinghua Univ (Sci Technol), 2003; 43: 227
(崔振山, 任广升, 徐秉业, 徐春国, 刘桂华. 清华大学学报(自然科学版), 2003; 43: 227)
[13] Lee Y S, Kwon Y C, Kwon Y N, Lee J H, Lee S W, Kim N S. Adv Mater Res, 2007; 26: 69
[14] Yuan C L, Zhong Y X, Ma Q X. Sci China, 2002; 45E: 531
[15] Petrov A I, Razuvaeva M V. Phys Solid State, 2005; 47: 880
[16] Schleisiek K, Lechler T, Schafer L, Weimar P. J Nucl Mater, 2000; 283: 1196
[17] Huang H G, Du F S, Xu Z Q. J Iron Steel Res, 2007; 19(11): 55
(黄华贵, 杜凤山, 许志强. 钢铁研究学报, 2007; 19(11): 55)
[18] Liu L J, Cui Z S. J Plast Eng, 2010; 17(1): 1
(刘丽娟, 崔振山. 塑性工程学报, 2010; 17(1): 1)
[19] Park C Y, Yang D Y. J Mater Process Technol, 1997; 72: 32
[20] Tanaka M, Ono S, Tsuneno M, Iwadate T. Adv Technol Plast, 1987; 2: 1035
[21] Morihiko N, Ichiro T, Hirosh U. J Mater Process Technol, 2006; 177: 521
[22] Kakimoto H, Arikawa T, Takahashi Y, Tanaka T, Imaida Y. J Mater Process Technol, 2010; 210: 415 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|