| Fe-Cu合金基体损伤的分子动力学模拟研究 |
| 贺新福, 杨鹏, 杨文 |
| 中国原子能科学研究院, 北京 102413 |
|
| MOLECULAR DYNAMICS SIMULATION OF MATRIX RADIATION DAMAGE IN Fe-Cu ALLOY |
| HE Xinfu, YANG Peng, YANG Wen |
| China Institute of Atomic Energy, Beijing 102413 |
引用本文:
贺新福 杨鹏 杨文. Fe-Cu合金基体损伤的分子动力学模拟研究[J]. 金属学报, 2011, 47(7): 954-957.
,
.
MOLECULAR DYNAMICS SIMULATION OF MATRIX RADIATION DAMAGE IN Fe-Cu ALLOY[J]. Acta Metall Sin, 2011, 47(7): 954-957.
| [1] Soneda N. In: Ghetta V ed., Materials Issues for Generation IV Systems. Corsica: Springer Science, 2008: 245[2] Odette G R, Wirth B D, Bacon D J, Ghoniem N M. MRS Bull, 2001; 26: 176[3] Becquart C S. Nucl Instrum Methods, 2005; 228B: 111[4] Bacon D J, Gao F, Osetsky Y N. J Comput Aided Mater Des, 1999; 6: 225[5] Calder A F, Bacon D J. MRS Proc, 1997; 439: 521.[6] Becquart C S, Domain C, Van Duysen J C. J Nucl Mater, 2001; 294: 274[7] Golubov S I, Osetsky Y N, Serra A, Barashev A V. J Nucl Mater, 1995; 226: 252[8] He X F, Yang W, Fan S. Acta Phys Sin, 2009; 58: 8657(贺新福, 杨文, 樊胜. 物理学报, 2009; 58: 8657)[9] Ackland G J, Bacon D J, Calder A F, Harry T. Philos Mag, 1997; 73A: 249[10] Ludwig M, Farkas D, Pedraza D, Schmauder S. Modelling Simul Mater Sci Eng, 1998; 6: 19[11] Pasianot R C, Malerba L. J Nucl Mater, 2007; 360: 118[12] Becquart C S, Domain C, Legris A. J Nucl Mater, 2000; 280: 73[13] Ashcroft N W. Solid State Physics. Philadelphia: Saunders, 1976: 4[14] Bjorkas C, Nordlund K, Malerba L, Terentyev D, Olsson P. J Nucl Mater, 2008; 372: 312[15] Ackland G J, Mendelev M I, Srolovitz D J, Han S, Barashev A V. J Phys: Condens Matter, 2004; 16: 1[16] Becquart C S, Domain C. Nucl Instrum Methods, 2003; 202B: 44 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|