时效处理和La含量对AZ91合金组织和力学性能的影响 |
王社斌1, 2, 祁小叶1, 张金玲1, 2,刘 璐1, 许并社1, 2 |
1.太原理工大学材料科学与工程学院, 太原 030024
2.太原理工大学教育部新材料界面与工程重点实验室, 太原 030024 |
|
EFFECT OF AGING TREATMENT AND La CONTENT ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF AZ91 ALLOY |
WANG Shebin 1,2, QI Xiaoye 1, ZHANG Jinling 1,2, LIU Lu 1, XU Bingshe 1,2 |
1. College of Materials Science and Engineering, Taiyuan University of Technology, Taiyuan 030024
2. Key Laboratory of Interface Science and Engineering in Advanced Materials Taiyuan University of Technology, Ministry of Education, Taiyuan 030024 |
引用本文:
王社斌 祁小叶 张金玲 刘璐 许并社. 时效处理和La含量对AZ91合金组织和力学性能的影响[J]. 金属学报, 2011, 47(6): 743-750.
,
,
,
.
EFFECT OF AGING TREATMENT AND La CONTENT ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF AZ91 ALLOY[J]. Acta Metall Sin, 2011, 47(6): 743-750.
[1] Aghion E, Bronfin B, Eliezer D. J Mater Process Technol, 2001; 117: 381[2] Mordike B L, Ebert T. Mater Sci Eng, 2001; A302: 37[3] Wang S B, Li X B, Fan J P, Wang S, Xu B S. Chin J Nonfer Met, 200919: 831(王社斌, 李晓斌, 范晋平, 王 帅, 许并社. 中国有色金属学报, 2009; 19: 831)[4] Cizek L, Greger M, Pawlica L, Dobrzanski L A, Tanski T. J Mater Process Technol, 2004; 157–158: 466[5] Li P J, Tang B, Kandal ova E G. Mater Lett, 2005; 59: 671[6] Zeng X Q, Wu Y J, Peng L M, Lin D, Ding W J, Peng Y H. Acta Metall Sin, 2010; 46: 1043(曾小勤, 吴玉娟, 彭立明, 林栋樑, 丁文江, 彭赢红. 金属学报, 2010; 46: 1043)[7] Wang K Q, Wang G J, Zhang J L, Wang S B, Xu B S. J Taiyuan Univ Technol, 2011; 1: 67(王克勤, 王国军, 张金玲, 王社斌, 许并社. 太原理工大学学报, 2011; 1: 67)[8] Wang S B, Zhang J L, Qi X Y, Xu B S. J Mater Eng, 2009; (Suppl. 1): 304(王社斌, 张金玲, 祁小叶, 许并社. 材料工程, 2009; (增刊1): 304)[9] Zhao Y H, Chen Y G, Tang Y B, Xiao S F, Wei S H, Zhang X P, Wang Q, Tu M J. Rare Met Mater Eng, 2010; 39: 844(赵源华, 陈云贵, 唐永柏, 肖素芬, 魏尚海, 章晓萍, 王卿, 涂铭旌. 稀有金属材料与工程, 2010; 39: 844)[10] Ma Y, Pan Z F, Zhang H F, Hao Y. J Lanzhou Univ Technol, 2009; 5: 9(马 颖, 潘振峰, 张洪锋, 郝 远. 兰州理工大学学报, 2009; 5: 9)[11] Ma Y L, Peng H D, Pan C C, Qin X, Du Y. Hot Work Technol, 2008; 37(10): 51(麻彦龙, 彭华东, 潘承聪, 秦旭, 杜勇. 热加工工艺, 2008;37(10): 51)[12] Xiao X L, Luo C P. Acta Metall Sin, 2001; 37: 2(肖晓玲, 罗承萍. 金属学报, 2001; 37: 2 )[13] Luo C P, Xiao X L, Liu J W. Acta Metall Sin, 2002; 38: 709(罗承萍, 肖晓玲, 刘江文. 金属学报, 2002; 38: 709)[14] Tang W, Han E H, Xu Y B, Liu L. Acta Metall Sin, 2005; 41: 1204(唐 伟, 韩恩厚, 许永波, 刘 路. 金属学报, 2005; 41: 1204)[15] Zhang J M, Jang B L, WanZ H, Yuan S, Xia P J. Heat Treat Met, 2007; 32: 7(张菊梅, 蒋百灵, 王志虎, 袁 森, 夏鹏举. 金属热处理, 2007; 32: 7)[16] Duly D, Cheynet M C, Brechet Y. Acta Metall Mater, 1994; 42: 3855[17] Ren Z Y. Master Dissertation, Southwest University of Science and Technology, Mianyang, 2007(任志远. 西南科技大学硕士学位论文, 绵阳, 2007)[18] Xu B S, Wang S B, Zhang J L, Zhang J Y, Li M Z, Yao X H, Chen J, Wei Y H. Chin Pat, 0102168.9, 2008(许并社, 王社斌, 张金玲, 张俊远, 李明照, 姚宪华, 陈 津, 卫英慧.中国专利, 0102168.9, 2008)[19] Zhang J L. Master Dissertation, Taiyuan University of Technology, 2007(张金玲. 太原理工大学硕士学位论文, 2007)[20] Li Z J, Jin Q L, Jiang Y H, Zhou R. Acta Metall Sin, 2009; 45: 928(李再久, 金青林, 蒋业华, 周荣. 金属学报, 2009; 45: 928) |
|