| 高Nb-TiAl合金高温塑性变形行为及微观组织演化 |
| 王刚, 徐磊, 王永, 郑卓, 崔玉友, 杨锐 |
| 中国科学院金属研究所, 沈阳 110016 |
|
| HOT DEFORMATION BEHAVIOR AND MICROSTRUCTURE EVOLUTION OF A HIGH-Nb-CONTAINING TiAl BASED ALLOY |
| WANG Gang, XU Lei, WANG Yong, ZHENG Zhuo, CUI Yuyou, YANG Rui |
| Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
王刚 徐磊 王永 郑卓 崔玉友 杨锐. 高Nb-TiAl合金高温塑性变形行为及微观组织演化[J]. 金属学报, 2011, 47(5): 587-593.
.
HOT DEFORMATION BEHAVIOR AND MICROSTRUCTURE EVOLUTION OF A HIGH-Nb-CONTAINING TiAl BASED ALLOY[J]. Acta Metall Sin, 2011, 47(5): 587-593.
| [1] Bystrzanowski S, Bartels A, Clemens H, Gerling R. Intermetallics, 2008; 16: 717[2] Wang Y H, Lin J P, Xu X J, He Y H, Wang Y L, Chen G L. J Alloys Compd, 2008; 458: 313[3] Wang Y H, Lin J P, He Y H, Wang Y L, Chen G L. Mater Sci Eng, 2007; A471: 82[4] Yan Y Q, Wang W S, Zhang Z Q, Luo G Z, Zhou L. Mater Rev, 2000; 14: 15(闰蕴琪, 王文生, 张振棋, 罗国珍, 周廉. 材料导报, 2000; 14: 15)[5] Lu X, Zhao L M, Qu X H. Mater Rev, 2006; 20: 69(路 新, 赵丽明, 曲选辉. 材料导报, 2006; 20: 69)[6] Prasad Y V R K. J Mater Eng Perform, 2003; 12: 638[7] Srinivasan N, Prasad Y V R K. Rao P R. Mater Sci Eng, 2008; A476: 146[8] Srinivasan N, Prasad Y V R K. J Mater Process Technol, 1995; 51: 171[9] Huang G S, Wang L Y, Chen H, Huang G J, Zhang S Q. Chin J Nonferrous Met, 2005; 15: 763(黄光胜, 汪凌云, 陈华, 黄光杰, 张所全. 中国有色金属学报, 2005; 15: 763)[10] Prasad Y V R K, Seshacharyulu T. Mater Sci Eng, 1998; A243: 82[11] Ramanathan S, Karthikeyan R, Gupta M. J Mater Process Technol, 2007; 183: 104[12] Sivakesavam O, Prasad Y V R K. Mater Sci Eng, 2002; A323: 270[13] Tang W N, Chen R S, Han E H. Acta Metall Sin, 2006; 42: 1096(唐伟能, 陈荣石, 韩恩厚. 金属学报, 2006; 42: 1096)[14] Ju Q, Li D G, Liu G Q. Acta Metall Sin, 2006; 42: 218(鞠泉, 李殿国, 刘国权. 金属学报, 2006; 42: 218)[15] Weiss I, Semiatin S L. Mater Sci Eng, 1999; A263: 243[16] Prasad, Y V R K, Seshacharyulu T. Int Mater Rev, 1998; 43: 243[17] He J S, Wang Y W. Metal Superplasticity. Beijing: Science Press, 1986: 26(何景素, 王燕文. 金属的超塑性. 北京: 科学出版社, 1986: 26)[18] LeeWB, Yang H S, Kim YW, Mukherjee A K. Scr Metall Mater, 1993; 29: 1403[19] Zhang C P, Zhang K F. J Alloys Compd, 2010; 492: 236[20] Ashby M F, Verrall R A. Acta Metall, 1973; 21: 149 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|