| 基于内聚力模型的AISI4135高强钢氢致滞后断裂数值模拟 |
| 王艳飞1), 巩建鸣1), 蒋文春2), 姜勇1), 唐建群1) |
1) 南京工业大学机械与动力工程学院, 南京 210009
2) 中国石油大学(华东)机电工程学院, 东营 257061 |
|
| NUMERICAL SIMULATION OF HYDROGEN INDUCED DELAYED FRACTURE OF AISI4135 HIGH STRENGTH STEEL USING COHESIVE ZONE MODELING |
| WANG Yanfei1), GONG Jianming1), JIANG Wenchun2), JIANG Yong1), TANG Jianqun1) |
1) College of Mechanical and Power Engineering, Nanjing University of Technology, Nanjing 210009
2) College of Mechanical and Electronic Engineering, China University of Petroleum, Dongying 257061 |
引用本文:
王艳飞 巩建鸣 蒋文春 姜勇 唐建群. 基于内聚力模型的AISI4135高强钢氢致滞后断裂数值模拟[J]. 金属学报, 2011, 47(5): 594-600.
,
,
,
,
.
NUMERICAL SIMULATION OF HYDROGEN INDUCED DELAYED FRACTURE OF AISI4135 HIGH STRENGTH STEEL USING COHESIVE ZONE MODELING[J]. Acta Metall Sin, 2011, 47(5): 594-600.
| [1] Chu W Y, Qiao L J, Chen Q Z, Gao K W. Fracture and Environment Fracture. Beijing: Science Press, 2000: 126(褚武扬, 乔利杰, 陈奇志, 高克玮. 断裂与环境断裂. 北京: 科学出版社, 2000: 126)[2] Serebrinsky S, Carter E A, Ortiz M. J Mech Phys Solids, 2004; 52: 2403[3] Liang Y, Sofronis P. J Mech Phys Solids, 2003; 51: 1509[4] Olden V, Thaulow C, Johnsen R, Φstby E, Berstad T. Eng Fract Mech, 2008; 75: 2333[5] Olden V, Thaulow C, Johnsen R, Φstby E. Scr Mater, 2007; 57: 615[6] Scheider I, Pfuff M, Dietzel W. Eng Fract Mech, 2008; 75: 4283[7] Wang M Q, Akiyama E, Tsuzaki K. Corros Sci, 2006; 48: 2189[8] Dugdale D S. J Mech Phys Solids, 1960; 8: 100[9] Barrenblatt G I. Adv Appl Mech, 1962; 7: 55[10] Hillerborg A, Modeer M, Petersson P. Cement Concrete Res, 1976; 6: 773[11] Needleman A. J Appl Mech, 1987; 54: 525[12] Nguyen O, Ortiz M. J Mech Phys Solids, 2002; 50: 1727[13] Jiang D E, Carter E A. Acta Mater, 2004; 52:4801[14] Hondros E D, Seah M P. Metall Trans, 1977; 8A: 1363[15] Van der Ven A, Ceder G. Phys Rev, 2003; 67B: 060101[16] Tvergaard V, Hutchinson J W. J Mech Phys Solids, 1992; 40: 1377[17] Wang M Q, Akiyama E, Tsuzaki K. Mater Sci Eng, 2005; A398: 37[18] GerberichWW, Livne T, Chen X F, Kaczorowski M. Metall Trans, 1988; 19A: 1319[19] Williams D P, Nelson H G. Metall Trans, 1970; 1: 63 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|