| 激光焊接参数对TiNi合金相变温度的影响 |
| 杨成功1,单际国1,2,温鹏1,2,任家烈1 |
1. 清华大学机械工程系, 北京 100084
2. 清华大学先进成形制造教育部重点实验室, 北京 100084 |
|
| EFFECT OF LASER WELDING PARAMETERS ON THE TRANSFORMATION TEMPERATURE OF TiNi ALLOY |
| YANG Chenggong 1, SHAN Jiguo 1,2, WEN Peng 1,2, REN Jialie 1 |
1. Department of Mechanical Engineering, Tsinghua University, Beijing 100084
2. Key Laboratory for Advanced Materials Processing Technology, Ministry of Education, Tsinghua University,Beijing 100084 |
引用本文:
杨成功 单际国 温鹏 任家烈. 激光焊接参数对TiNi合金相变温度的影响[J]. 金属学报, 2011, 47(10): 1277-1284.
,
,
,
.
EFFECT OF LASER WELDING PARAMETERS ON THE TRANSFORMATION TEMPERATURE OF TiNi ALLOY[J]. Acta Metall Sin, 2011, 47(10): 1277-1284.
| [1] Zhao L C, Cai W, Zheng Y F. Shape Memory Effect and Superelasticity in Alloys. Beijing: National Defense Industry Press, 2002: 5(赵连成, 蔡伟, 郑玉峰. 合金的形状记忆效应和超弹性. 北京: 国防工业出版社, 2002: 5)[2] Xu Z Y. Shape Memory Materials. Shanghai: Shanghai Jiaotong University Press, 2002: 18(徐祖耀. 形状记忆材料. 上海: 上海交通大学出版社, 2002: 18)[3] Funakubo H, translate by Qian D F. Shape Memory Alloy. Beijing: China Machine Press, 1984: 85(Funakubo H 著, 千东范 译. 形状记忆合金. 北京: 机械工业出版社, 1984: 85)[4] Ren J L, Wu A P. Joining of Advanced Materials. Beijing: China Machine Press, 2000: 335(任家烈, 吴爱萍. 先进材料的连接. 北京: 机械工业出版社, 2000: 335)[5] Falvo A, Furgiuele F M, Maletta C. Mater Sci Eng, 2005; A412: 235[6] Hsu Y T, Wang Y R, Chen C. Metall Mater Trans, 2001; 32A: 569[7] Falvo A, Furgiuele F M, Maletta C. Mater Sci Eng, 2008; A481–482: 647[8] Gugel H, Schuermann A, TheisenW. Mater Sci Eng, 2008; A481–482: 668[9] Wang W, Chen G, Chen L, Zhao X K, Huang J H. Appl Laser, 2008; 28: 199(王蔚, 陈庚, 陈俐, 赵兴科, 黄继华. 应用激光. 2008; 28: 199)[10] Tang W, Sundmann B, Sandstrom R, Quiu C. Acta Mater, 1999; 47: 3457[11] Frenzel J, George E P, Dlouhy A, Somsen Ch, Wagner M F X, Eggeler G. Acta Mater, 2010; 58: 3444[12] Khalil–Allafi J, Dlouhy A, Eggeler G. Acta Mater, 2002; 50: 4255[13] Fan G, Chen W, Yang S, Zhu J H, Ren X B, Otsuka K. Acta Mater, 2004; 52: 4351[14] Krishna V B, Bose S, Bandyopadhyay A. Metall Mater Trans, 2007; 38A: 1097[15] Otsuka K, Mayman C M. Shape Memory Materials. Cambridge: Cambridge University Press, 1998: 49 |
|