| 形变热处理对Al-Zn-Mg-Cu合金板材组织与硬度的影响 |
| 张云崖1,2, 邓运来1,2, 万里1,2,张新明1,2 |
1. 中南大学材料科学与工程学院, 长沙 410083
2. 中南大学有色金属材料科学与工程教育部重点实验室, 长沙 410083 |
|
| EFFECTS OF THERMAL MECHANICAL TREATMENT ON THE MICROSTRUCTURES AND HARDNESS OF AN Al–Zn–Mg–Cu ALLOY PLATE |
| ZHANG Yunya 1,2, DENG Yunlai 1,2, WAN Li 1,2, ZHANG Xinming 1,2 |
1. School of Materials Science and Engineering, Central South University, Changsha 410083
2. Key Laboratory of Nonferrous Metal Materials Science and Engineering, Ministry of Education, Central South University, Changsha 410083 |
引用本文:
张云崖 邓运来 万里 张新明. 形变热处理对Al-Zn-Mg-Cu合金板材组织与硬度的影响[J]. 金属学报, 2011, 47(10): 1270-1276.
,
,
,
.
EFFECTS OF THERMAL MECHANICAL TREATMENT ON THE MICROSTRUCTURES AND HARDNESS OF AN Al–Zn–Mg–Cu ALLOY PLATE[J]. Acta Metall Sin, 2011, 47(10): 1270-1276.
| [1] Williams J C, Starke E A. Acta Mater, 2003; 51: 5775[2] Chakrabarti D J, Liu J, Sawtell R R, Venema G B. Mater Forum, 2004; 28: 969[3] Liu J. Mater Sci Forum, 2006; 519: 1233[4] Senkov O N, Bhat R B, Senkova S V, Schloz J D. Metall Mater Trans, 2004; 36: 2115[5] Hideo Y, Yoshio B. Trans Jpn Inst Met, 1982; 23: 620[6] Robson J D. Mater Sci Eng, 2002; A338: 219[7] Robson J D, Prangnel P B. Acta Mater, 2001; 49: 599[8] Morere B, Maurice C, Driver J, Shahani R. Mater Sci Forum, 1996; 217–222: 517[9] Deng Y L, Wan L, Zhang Y, Zhang X M. J Alloys Compd, 2010; 498: 88[10] Xiong C X, Wan L, Deng Y L, Zhang X M. J Cent China Univ (Sci Technol), 2010; 41: 465(熊创贤, 万里, 邓运来, 张新明. 中南大学学报(自然科学版), 2010; 41: 465)[11] Bunge H J. Texture Analysis in Materials Science. London: Butterworths, 1982: 44[12] L¨ucke K, Pospiech J, Virnich K H, Jura J. Acta Metall, 1981; 29: 167[13] Hu H E, Zhen L, Yang L, Shao W Z, Zhang B Y. Mater Sci Eng, 2008; A488: 64[14] Zhen L, Hua H E, Wang X Y, Zhang B Y, Shao W Z. J Mater Process Technol, 2009; 209: 754[15] Li X Z, Hansen V, Gjonnes J, Wallenberg L R. Acta Metall, 1999; 47: 2651[16] Komura Y, Tokunaga K. Acta Crystallogr, 1980; B36: 1548[17] Stiller K, Warren P J, Hansen V, Angenete J, Gjonnes J. Mater Sci Eng, 1999; A270: 55[18] Engler O, Sachot E, Ehrstrom J C, Reeves A, Shahani R. Mater Sci Technol, 1996; 12: 717[19] Doherty R D, Hughes D A, Humphreys F J, Jonas J J, Juul Jensen D, Kassner M E, King W E, McNelley T R, McQueen H J, Rollett A D. Mater Sci Eng, 1997; A238: 219[20] Humphreys F J, Hatherly M. Recrystallization and Related Phenomena. 2nd Ed., Oxford, London: Pergamon Press, 2004: 86[21] Zhang X M, Deng Y L, Liu Y, Tang J G, Zhou Z P. Acta Metall Sin, 2005; 41: 947(张新明, 邓运来, 刘瑛, 唐建国, 周卓平.金属学报, 2005; 41: 947)[22] Deng Y L, Zhang X M, Liang X, Zhang Y. Adv Mater Res, 2007; 15–17: 929[23] Humphreys F J. Met Sci, 1979; 13: 136[24] Ørsund R, Nes E. Scr Metall, 1988; 22: 665 |
|