| 定向凝固镍基高温合金DZ125平界面生长的微观组织演化 |
| 闵志先, 沈军, 王灵水, 冯周荣, 刘林, 傅恒志 |
| 西北工业大学凝固技术国家重点实验室, 西安 710072 |
|
| MICROSTRUCTURAL EVOLUTION OF DIRECTIONALLY SOLIDIFIED Ni-BASED SUPERALLOY DZ125 UNDER PLANAR GROWTH |
| MIN Zhixian, SHEN Jun, WANG Lingshui, FENG Zhourong, LIU Lin, FU Hengzhi |
| State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072 |
引用本文:
闵志先 沈军 王灵水 冯周荣 刘林 傅恒志. 定向凝固镍基高温合金DZ125平界面生长的微观组织演化[J]. 金属学报, 2010, 46(9): 1075-1080.
,
,
,
,
,
.
MICROSTRUCTURAL EVOLUTION OF DIRECTIONALLY SOLIDIFIED Ni-BASED SUPERALLOY DZ125 UNDER PLANAR GROWTH[J]. Acta Metall Sin, 2010, 46(9): 1075-1080.
| [1] Fu H Z. J Aeronaut Mater, 1998; 18(4): 52
(傅恒志. 航空材料学报, 1998; 18(4): 52)
[2] McLean M. Directionally Solidified Materials for High Temperature Service. UK: The Metals Society, 1983: 11
[3] Liu L, Huang T W, Zhang J, Fu H Z. Mater Lett, 2007; 61: 227
[4] Versnyder F I, Shank M E. Mater Sci Eng, 1970; A6: 213
[5] Tien J K, Gamble R P. Mater Sci Eng, 1971; A8: 152
[6] Bae J S, Lee J H, Kim S S, Jo C Y. Scr Mater, 2001; 45: 50
[7] Sellamuthu R, Giamei A F. Metall Mater Trans, 1986; 16A: 419
[8] Seo S M, Lee J H, Yoo Y S, Jo C Y, Miyahara H, Ogi K. In: Reed R C, Green K A, Caron P, Gabb T P, Fahrmann M G, Huron E S, Woodard S A. eds, Superalloys 2008, Warrendale, PA: TMS, 2008: 2773
[9] Stefanescu D M. Science and Engineering of Casting Solidification. New York: Kluwer Academic/Plenum Publishers, 2002: 33
[10] Trivedi R, Minyahara H, Mazumder P, Simsek E, Tewari S N. J Cryst Growth, 2001; 222: 365
[11] Tiller W A. Trans TMS–AIME, 1959; 215: 555
[12] Liu L, Sommer F, Fu H Z. Scr Metall Mater, 1994; 30: 584
[13] ZhangWG. PhD Thesis, Northwestern Polytechnical University, Xi’an, 2009
(张卫国. 西北工业大学博士论文, 西安, 2009)
[14] Li R J. Ceramic–Metal Composites. Beijing: Metallurgical Industry Press, 2004: 39
(李荣久. 陶瓷-金属复合材料, 北京: 冶金工业出版社, 2004: 39)
[15] Bhambri A K, Kattamis T Z, Morral J E. Metall Mater Trans, 1986; 6B: 523
[16] Chen J, Lee J H, Jo C Y, Choe S J, Lee Y T. Mater Sci Eng, 1998; A247: 113 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|