| 两种铸造镍基高温合金在长期时效期间的微观组织和力学性能演变 |
| 秦学智;郭建亭; 袁 超; 侯介山; 周兰章; 叶恒强 |
| 中国科学院金属研究所; 沈阳 110016 |
|
| EVOLUTIONS OF MICROSTRUCTURES AND MECHANICAL PROPERTIES OF TWO CAST Ni–BASED SUPERALLOYS DURING LONG–TERM THERMAL EXPOSURE |
| QIN Xuezhi; GUO Jianting; YUAN Chao; HOU Jieshan; ZHOU Lanzhang; YE Hengqiang |
| Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
秦学智 郭建亭 袁超 侯介山 叶恒强. 两种铸造镍基高温合金在长期时效期间的微观组织和力学性能演变[J]. 金属学报, 2010, 46(2): 213-220.
.
EVOLUTIONS OF MICROSTRUCTURES AND MECHANICAL PROPERTIES OF TWO CAST Ni–BASED SUPERALLOYS DURING LONG–TERM THERMAL EXPOSURE[J]. Acta Metall Sin, 2010, 46(2): 213-220.
| [1] Ross E W, Sims C T. In: Sims C T, Stoloff N S, Hagel W C eds., Superalloys II, New York, NY: Wiley, 1987: 97
[2] Koul A K, Castillo R. Metall Trans, 1988; 19A: 2049
[3] Qin X Z, Guo J T, Yuan C, Chen C L, Ye H Q. Metall Mater Trans, 2007; 38A: 3014
[4] Qin X Z, Guo J T, Yuan C, Hou J S, Ye H Q. Mater Lett, 2008; 62: 258
[5] Qin X Z, Guo J T, Yuan C, Hou J S, Ye H Q. Mater Lett, 2008; 62: 2275
[6] Qin X Z, Guo J T, Yuan C, Yang G X, Zhou L Z, Ye H Q. J Mater Sci, 2009; 44: 4840
[7] Stevens R A, Flewitt P E J. Mater Sci Eng, 1979; A37: 237
[8] Sha W. Scr Mater, 2000; 42: 549
[9] Rae C M F, Reed R C. Acta Metall, 2001; 49: 4113
[10] Chen Q Z, Jones N, Knowles D M. Acta Metall, 2002; 50: 1095
[11] Guo J T. Materials Science and Engineering for Superalloys . Vol.1, Beijing: Science Press, 2008: 126
(郭建亭. 高温合金材料学(上册). 北京: 科学出版社, 2008: 126)
[12] Lvov G, Levit V I, Kaufman M J, Metall Mater Trans, 2004; 35A: 1669
[13] Choi B G, Kom I S, Kim D H, Jo C Y. Mater Sci Eng, 2008; A478: 329
[14] Qin X Z, Guo J T, Yuan C, Chen C L, Hou J S, Ye H Q. Mater Sci Eng, 2008; A485: 74
[15] Furillo F T, Davidson J M, Tien J K. Mater Sci Eng, 1979; A39: 267
[16] Chen Q Z, Jones C N, Knowles D M. Mater Sci Eng, 2004; A385: 402
[17] Volek A, Singer R F, Buergel R, Grossmann J, Wang Y. Metall Mater Trans, 2006; 37A: 405
[18] Simonetti M, Caron P. Mater Sci Eng, 1998; A254: 1
[19] Pessah M, Caron P, Khan T. In: Antolovich S D, Strusrud R W, MacKay R A, Anton D L, Khan T, Kissinger R D, Klarstrom D L eds., Superalloys 1992, Warrendale PA: TMS, 1992: 567 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|