李萧 杨平 孟利 崔凤娥. AZ31镁合金中拉伸孪晶静态再结晶的分析[J]. 金属学报, 2010, 46(2): 147-154.
,
.
ANALYSIS OF THE STATIC RECRYSTALLIZATION AT TENSION TWINS IN AZ31 MAGNESIUM ALLOY[J]. Acta Metall Sin, 2010, 46(2): 147-154.
| [1] Gehrmann R, Frommert M M, Gottstein G. Mater Sci Eng, 2005; A395: 338
[2] Agnew S R, Duygulu O. Int J Plast, 2005; 21: 1161
[3] Tucker M T, Horstemeyer M F, Gullett P M, Kadiri H E, Whittington W R. Scr Mater, 2009; 60: 182
[4] Kelley E W, Hosford Jr. W F. Trans AIME, 1968; 242: 5
[5] Wonsiewicz B C, Backofen W A. Trans AIME, 1967; 239: 1422
[6] Hartt WH, Reed–Hill R E. Trans Metall Soc AIME, 1968; 242: 1127
[7] Al–Samman T, Gottstein G. Mater Sci Eng, 2008; A490: 411
[8] P´erez–Prado M T, del Valle J A, Contreras J M, Ruano O A. Scr Mater, 2004; 50: 661
[9] Yin D L, Zhang K F, Wang G F, Han W B. Mater Sci Eng, 2005; A392: 320
[10] Prasad Y V R K, Rao K P. Mater Sci Eng, 2006; A432: 170
[11] del Valle J A, Ruano O A. Mater Sci Eng, 2008; A487: 473
[12] Nave M D, Barnett M R. Scr Mater, 2004; 51: 881
[13] Cottam R, Robson J, Lorimer G, Davis B. Ceram Trans, 2008; 200: 501
[14] Jager A, Luk´ac P, Gartnerov´a V, Haloda J, Dopita M. Mater Sci Eng, 2006; A432: 20
[15] Mackenzie L W F, Pekguleryuz M O. Scr Mater, 2008; 59: 665
[16] Yi S B, Zaefferer S, Brokmeier H G. Mater Sci Eng, 2006; A424: 275
[17] Yang X Y, Miura H, Sakai T. Trans Nonferrous Met Soc China, 2007; 17: 1139
[18] Beer A G, Barnett M R. Mater Sci Eng, 2008; A485: 318
[19] Cottam R, Robson J, Lorimer G, Davis B. Mater Sci Eng, 2008; A485: 375
[20] Li X, Yang P, Wang L N, Meng L, Cui F E. Mater Sci Eng, 2009; A517: 160 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|