| TWIP钢中晶粒尺寸对TWIP效应的影响 |
| 王书晗 ; 刘振宇; 王国栋 |
| 东北大学轧制技术与连轧自动化国家重点实验室; 沈阳 110004 |
|
| INFLUENCE OF GRAIN SIZE ON TWIP EFFECT IN A TWIP STEEL |
| WANG Shuhan; LIU Zhenyu; WANG Guodong |
| State Key Laboratory of Rolling and Automation; Northeastern University; Shenyang 110004 |
引用本文:
王书晗 刘振宇 王国栋. TWIP钢中晶粒尺寸对TWIP效应的影响[J]. 金属学报, 2009, 45(9): 1083-1090.
,
,
.
INFLUENCE OF GRAIN SIZE ON TWIP EFFECT IN A TWIP STEEL[J]. Acta Metall Sin, 2009, 45(9): 1083-1090.
| [1] Frommeyer G, Br¨ux U, Neumann P. ISIJ Int, 2003; 43: 438
[2] Gr¨assel O, Kr¨uger L, Frommeyer G, Meyer L W. Int J Plast, 2000; 16: 1391
[3] Vercammen S, Blanpai B, Cooman B C D, Wollants P. Acta Mater, 2004; 52: 2005
[4] Bouaziz O, Guelton N. Mater Sci Eng, 2001; A319–321: 246
[5] Shiekhelsouk M N, Favier V, Inal K, Cherkaoui M. Int J Plast, 2009; 25: 105
[6] Christian J W, Mahajan S. Pro Mater Sci, 1995; 39: 1
[7] Ueji R, Tsuchida N, Terada D, Tsuji N, Tanaka Y, Takemura A, Kunishige K. Scr Mater, 2008; 59: 963
[8] Danaf E E, Kalidindi S R, Doherty R D. Int J Plast, 2001; 17: 1245
[9] Lu L, Shen Y, Chen X, Qian L, Lu K. Science, 2004; 304: 422
[10] Kalidindi S R. Int J Plast, 1998; 14: 1265
[11] Danaf E E, Kalidindi S R, Doherty R D. Metall Mater Trans, 1999; 30A: 1223
[12] Xiong R G, Fu R Y, Li Q, ZhangM, Li L. Iron Steel, 2007; 42: 61
(熊荣刚, 符仁钰, 黎倩, 张 梅, 李 麟. 钢铁, 2007; 42: 61)
[13] Barbier D, Gey N, Allain S, Bozzolo N, Humbert M. Mater Sci Eng, 2009; A500: 196
[14] Sevillano J G. Scr Mater, 2008; 59: 135
[15] Meyers M A, V¨ohringer O, Lubarda V A. Acta Mater, 2001; 49: 4025
[16] Barnett M R. Scr Mater, 2008; 59: 696
[17] Allain S, Chateau J–P, Kahmoun K, Bouaziz O. Mater Sci Eng, 2004; A387–389: 272
[18] Allain S, Chateau J–P, Bouaziz O, Migot S, Guelton N. Mater Sci Eng, 2004; A387–389: 158 |
|