| Ce对热轧AZ31镁合金动态再结晶及织构的影响 |
| 李再久; 金青林; 蒋业华; 周荣 |
| 昆明理工大学机电工程学院; 昆明 650093 |
|
| EFFECT OF Ce ON THE DYNAMIC RECRYSTALLIZATION AND TEXTURE OF AZ31 MAGNESIUM ALLOY DURING HOT ROLLING |
| LI Zaijiu; JIN Qinglin; JIANG Yehua; ZHOU Rong |
| Faculty of Mechanical and Electrical Engineering; KunMing University of Science and Technology; KunMing 650093 |
引用本文:
李再久 金青林 蒋业华 周荣. Ce对热轧AZ31镁合金动态再结晶及织构的影响[J]. 金属学报, 2009, 45(8): 924-929.
,
.
EFFECT OF Ce ON THE DYNAMIC RECRYSTALLIZATION AND TEXTURE OF AZ31 MAGNESIUM ALLOY DURING HOT ROLLING[J]. Acta Metall Sin, 2009, 45(8): 924-929.
| [1] Wang Z X, Xie J X, Liu X F, Li J Y, Zhang D F, Pan F S. Acta Metall Sin, 2007; 43: 920
(王智祥, 谢建新, 刘雪峰, 李静媛, 张丁非, 潘复生. 金属学报, 2007; 43: 920)
[2] Chen Z H. Wrought Magnesium Alloy. Beijing: Chemical Industry Press, 2005: 1
(陈振华. 变形镁合金. 北京: 化学工业出版社, 2005: 1)
[3] Wang Q D, Lin J B, Peng L M, Chen Y J. Acta Metall Sin, 2008; 44: 55
(王渠东, 林金保, 彭立明, 陈永军. 金属学报, 2008; 44: 55)
[4] Chen Z H, Xia W J, Cheng Y Q, Fu D F. Chin J Nonferrous Met, 2005; 15: 1
(陈振华, 夏伟军, 程永奇, 傅定发. 中国有色金属学报, 2005; 15: 1)
[5] Guo Q, Yan H G, Chen Z H, Wu Y Z, Chen J. Acta Metall Sin, 2007; 43: 619
(郭强, 严红革, 陈振华, 吴远志, 陈婕. 金属学报, 2007; 43: 619)
[6] Agnew S R, Yoo M H, Tome C N. Acta Mater, 2001; 49: 4277
[7] Chino Y, Kado M, Mabuchi M. Mater Sci Eng, 2008; A494: 343
[8] Chino Y, Kado M, Mabuchi M. Acta Mater, 2008; 56: 387
[9] Liu S F, Huang S Y, Peng L M, Xu P. Acta Metall Sin, 2006; 42: 443
(刘生发, 黄尚宇, 徐萍. 金属学报, 2006; 42: 443)
[10] Yu W B, Liu Z Y, Cheng N P, He H. Acta Metall Sin, 2007; 43: 612
(于文斌, 刘志义, 程南璞, 何洪. 金属学报, 2007; 43: 612)
[11] Wang M X, Zhou H, ang L. J Rare Earths, 2007; 25: 233
[12] Yu F, Wu G H, Zhai C Q. Mater Sci Eng, 2006; A433: 208
[13] Zhen W C, Li S S, Tang B, Zeng D B. Acta Metall Sin, 2006; 42: 835
(郑伟超, 李双寿, 汤彬, 曾大本. 金属学报, 2006; 42: 835)
[14] Mao W M, Zhao X B. Recrystallization and Grain Growth of Metals. Beijing: Metallurgical Industry Press, 1994: 47
(毛卫民, 赵新兵. 金属的再结晶与晶粒长大. 北京: 冶金业出版社, 1994: 47)
[15] Galiyev A, Kaibyshev R, Gottstein G. Acta Mater, 2001; 49: 1199
[16] Liu C M, Liu Z J, Zhu X R, Zhou H T. Chin J Nonferrous Met, 2006; 16: 1
(刘楚明, 刘子娟, 朱秀荣, 周海涛. 中国有色金属学报, 2006; 16: 1)
[17] Stanford N, Barnett M. Scr Mater, 2008; 58: 179
[18] Mwembela A, Konopleva E B, Mcqueen H J. Scr Mater, 1997; 11: 1789
[19] Jin Q L, Shim S Y, Lim S G. Scr Mater, 2006; 55: 843
[20] Park J S, Chang Y W. Adv Mater Res, 2007; 26–28: 95 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|