| 冷轧Cu板动态压缩力学性能各向异性的研究 |
| 陈志永 1;才鸿年2;王富耻2;谭成文2;詹从堃1;刘楚明1 |
1. 中南大学材料科学与工程学院; 长沙410083
2. 北京理工大学材料科学与工程学院; 北京 100081 |
|
| INVESTIGATION ON ANISOTROPY OF DYNAMIC COMPRESSIVE MECHANICAL PROPERTIES OF COLD--ROLLED Cu SHEET |
| CHEN Zhiyong1; CAI Hongnian2; WANG Fuchi2; TAN Chengwen2; ZHAN Congkun1; LIU Chuming1 |
1. School of Materials Science and Engineering; Central South University; Changsha 410083
2. School of Materials Science and Engineering; Beijing Institute of Technology; Beijing 100081 |
引用本文:
陈志永 才鸿年 王富耻 谭成文 詹从堃 刘楚明. 冷轧Cu板动态压缩力学性能各向异性的研究[J]. 金属学报, 2009, 45(2): 143-150.
,
,
,
,
,
.
INVESTIGATION ON ANISOTROPY OF DYNAMIC COMPRESSIVE MECHANICAL PROPERTIES OF COLD--ROLLED Cu SHEET[J]. Acta Metall Sin, 2009, 45(2): 143-150.
| [1] Glenn T, Bradley W. Metall Trans, 1973; 4A: 2343
[2] Tang N Y, Niessen P, Pick R J, Worswick M J. Mater Sci Eng, 1991; A131: 153
[3] Andrade U R, Meyers M A, Chokshi A H. Scr Metall Mater, 1994; 30: 933
[4] Sanchez J C, Murr L E, Staudhammer K P. Acta Mater, 1997; 45: 3223
[5] Kiritani M, Satoh Y, Kizuka Y, Arakawa K, Ogasawara Y, Arai S, Shimomura Y. Philos Mag Lett, 1999; 79: 797
[6] Jia D, Ramesh K T, Ma E, Lu L, Lu K. Scr Mater, 2001; 45: 613
[7] Stevenson M E, Jones S E, Bradt R C. Mater Sci Res Int, 2003; 9: 187
[8] Gourdin W H, Lassila D H. Acta Metall Mater, 1991; 39: 2337
[9] Gourdin W H, Lassila D H. Mater Sci Eng, 1992; A151: 11
[10] Meyers M A, Andrade U R, Chokshi A R. Metall Mater Trans, 1995; 26A: 2881
[11] Nemat–Nasser S, Li Y L. Acta Mater, 1998; 46: 565
[12] Wang L L. Foundation of Stress Waves. Beijing: National Defense Industry Press, 2005: 52
(王礼立. 应力波基础. 北京: 国防工业出版社, 2005: 52)
[13] Bunge H J. Texture Analysis in Materials Science—Mathematical Methods. London: Butterworths, 1982: 47
[14] Klepaczko J R. J Phys Colloque, 1988; 49: 553
[15] Follansbee P S, Kocks U F. Acta Metall, 1988; 36: 81
[16] Tong W, Clifton R J, Huang S. J Mech Phys Solids, 1992;40: 1251
[17] Chin G Y, Mendorf D R, Hosford W F. Proc Roy Soc,1969; 309A: 433
[18] Hirsch J, LÜcke K, Hatherly M. Acta Metall, 1988; 36:2905
[19] El–Danaf E, Kalidindi S R, Doherty R D. Int J Plast,2001; 17: 1245
[20] Szczerba M S, Bajor T, Tokarski T. Philos Mag, 2004; 84:481
[21] Chen Z Y, Zhang X M, Liu C M, Zhou Z P, Li S Y. J Mater Sci, 2002; 37: 2843
[22] Sachs E. Z Ver Deut Ing, 1928; 72: 734
[23] Taylor G I. J Inst Met, 1938; 62: 307
[24] Van Houtte P. In: Nagashima S ed., Proc 6th Int Conf on Textures of Materials. Tokyo: Iron and Steel Institute of Japan, 1981: 428
[25] Fortunier R, Driver J H. Acta Metall, 1987; 35: 509
[26] Mao W M. Mater Sci Eng, 1998; A257: 171
[27] Bishop J F W, Hill R. Philos Mag, 1951; 42: 414
[28] Bishop J F W, Hill R. Philos Mag, 1951; 42: 1298
[29] Chen Z Y, Cai H N, Zhang X M, Wang F C, Tan C W. Sci China, 2006; 49E: 521 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|