金属学报  2009, Vol. 45 Issue (11): 1390-1395    
  论文 本期目录 | 过刊浏览 |
含Fe和Mn的Ni30Cu70固溶体团簇模型与耐蚀性研究
张杰;王清;王英敏;董闯
大连理工大学三束材料改性教育部重点实验室; 大连 116024
STUDY ON THE CLUSTER--BASED MODEL OF Ni30Cu70 SOLID SOLUTION WITH Fe AND Mn AND ITS CORROSION RESISTANCE
ZHANG Jie; WANG Qing; WANG Yingmin; DONG Chuang
Key Lab of Materials Modification by Laser; Ion and Electron Beams of Ministry of Education;
School of Materials Science & Engineering; Dalian University of Technology; Dalian 116024
引用本文:

张杰 王清 王英敏 董闯. 含Fe和Mn的Ni30Cu70固溶体团簇模型与耐蚀性研究[J]. 金属学报, 2009, 45(11): 1390-1395.
, , , . STUDY ON THE CLUSTER--BASED MODEL OF Ni30Cu70 SOLID SOLUTION WITH Fe AND Mn AND ITS CORROSION RESISTANCE[J]. Acta Metall Sin, 2009, 45(11): 1390-1395.

全文: PDF(1007 KB)  
摘要: 

提出了一个极限固溶体合金的团簇模型, 在此基础上优化设计了添加Fe和Mn的Ni30Cu70 (原子分数,\%)固溶体合金成分. 在该模型中, 固溶的Fe和Mn以Ni为第一近邻形成12配位立方八面体原子团簇(Fe1-xMnx)Ni12而分散到Cu基体中, 因此极限固溶体合金成分为 [M1/13Ni12/13]30Cu70=[(Fe1-xMnx)Ni12]Cu30.3, M=(Fe1-xMnx). 采用X射线衍射和电化学腐蚀测试等方法, 研究了[(Fe1-xMnx)Ni12]Cu30.3合金的微观组织与耐腐蚀性能的关系. 实验结果表明, 对应于极限固溶体状态的[(Fe0.75Mn0.25)Ni12]Cu30.3合金, 在3.5%NaCl溶液中具有相对好的耐腐蚀性能.

关键词 Cu-Ni合金Fe(Mn)添加固溶体模型团簇结构耐腐蚀性能    
Abstract

Minor Fe and Mn additions are necessary to enhance the corrosion resistance of commercial Cu-Ni alloys. The present paper aims at optimizing the addition amounts of Fe and Mn in Cu70Ni30 (atomic fraction, %) alloy using a cluster-based solid solution model. In this model it assumed that one Fe(Mn) atom and twelve Ni atoms formed a cluster consisted of Fe(Mn)-centered and Ni-surrounded cube-octahedron and the limit solid solution would be composed of isolated Fe(Mn)Ni12 clusters embedded in the Cu matrix. The ratio of the Fe(Mn) atoms and its surrounding Ni atoms is 1∶12, and the limit solid solution composition of Fe(Mn)-modified Cu70Ni30 alloy is [M1/13Ni12/13]30Cu70=[(Fe1-xMnx)Ni12]Cu30.3, M=(Fe1-xMnx). The OM, XRD and electrochemical corrosion measurements were used to characterize the microstructure and corrosion resistance performance of [(Fe1-xMnx)Ni12]Cu30.3. The results indicated that the solid solubility limitative alloys [(Fe0.75Mn0.25)Ni12]Cu30.3 has the best corrosion resistance in 3.5%NaCl aqueous solution.

Key wordsCu-Ni alloy    addition of Fe(Mn)    solid solution model    cluster structure    corrosion-resistance
收稿日期: 2009-04-29     
ZTFLH: 

TG111

 
基金资助:

国家自然科学基金项目50671018和50631010, 国家重点基础研究发展计划项目2007CB613902及国家高技术研究发展计划项目2007AA05Z102资助

作者简介: 张杰, 男, 1979年生, 博士生

[1] Marsden D D. Mater Performance, 1978; 17: 9
[2] Pearson C. Br Corros J. 1972; 7: 61
[3] Wang J H, Jiang X X, Li S Z. Acta Metall Sin, 1995; 6A: 266
(王吉会, 姜晓霞, 李诗卓. 金属学报, 1995; 6A: 266)
[4] Efird K D. Corrosion, 1977; 33: 347
[5] Drolenga L J P, Ijsseling F P, Kolster B H. Mater Corros, 1983; 34: 167
[6] Popplewell J M, Hart R J. Corros Sci, 1973; 13: 295
[7] Bailey G L. J Inst Metals, 1951; 79: 243
[8] Stewart W C, La Que F L. Corrosion, 1952; 8: 259
[9] Zhu X L, Lin L Y, Lei T Q. Acta Metall Sin, 1997; 7: 1256
(朱小龙, 林乐耘, 雷廷权. 金属学报, 1997; 7: 1256)
[10] Dong C, Wang Q, Qiang J B, Wang Y M, Jiang N, Han G, Li Y H, Wu J, Xia J H. J Phys, 2007; 40D: R273
[11] Dong C, Chen W R, Wang Y G, Qiang J B, Wang Q, Lei Y, Monique C D, Dubois J M. J Non–Cryst Solids, 2007; 353: 3405
[12] Miracle D B. Acta Mater, 2006; 54: 4317
[13] BraggWL,Williams E J. Proc R Soc London, 1934; 145A: 699
[14] Chakrabarti D J, Laughlin D E. Chen S W, Chang Y A. Binary Alloy Phase Diagrams. Materials Park, OH, ASM International, 1991: 1442
[15] Swartzendruber L J. Phase Diagrams of Binary Iron Alloys. Materials Park, OH, ASM International, 1993: 131
[16] Gupta K P. Indian Inst Metals, 1990; 1: 290
[17] Takeuchi A, Inoue A. Mater Trans JIM, 2000; 41: 1372
[18] Zhang J, Wang Q, Wang Y M, Li C Y, Wen L S, Dong C. J Mater Res, in press

[1] 司永礼, 薛金涛, 王幸福, 梁驹华, 史子木, 韩福生. Cr添加对孪生诱发塑性钢腐蚀行为的影响[J]. 金属学报, 2023, 59(7): 905-914.
[2] 朱雯婷, 崔君军, 陈振业, 冯阳, 赵阳, 陈礼清. 690 MPa级高强韧低碳微合金建筑结构钢设计及性能[J]. 金属学报, 2021, 57(3): 340-352.
[3] 蒋一,程满浪,姜海洪,周庆龙,姜美雪,江来珠,蒋益明. 高强度含NNi奥氏体不锈钢08Cr19Mn6Ni3Cu2N (QN1803)的显微组织及性能[J]. 金属学报, 2020, 56(4): 642-652.
[4] 王垚,李春福,林元华. Cr对Fe-Cr合金耐蚀性能影响的电子理论研究[J]. 金属学报, 2017, 53(5): 622-630.
[5] 徐伟,路新,杜艳霞,孟庆宇,黎鸣,曲选辉. 粉末冶金制备Ti-Fe二元合金的耐腐蚀性能[J]. 金属学报, 2017, 53(1): 38-46.
[6] 王波阳,周邦新,王桢,黄娇,姚美意,周军. Zr-0.72Sn-0.32Fe-0.14Cr-xNb合金在500 ℃过热蒸汽中的耐腐蚀性能*[J]. 金属学报, 2015, 51(12): 1545-1552.
[7] 刘永康, 黄海友, 谢建新. 连续柱状晶组织CuNi10Fe1Mn合金变形行为的各向异性[J]. 金属学报, 2015, 51(1): 40-48.
[8] 韦天国,龙冲生,苗志,刘云明,栾佰峰. Zr-0.4Fe-1.0Cr-x Mo合金在500℃和10.3 MPa水蒸汽中的腐蚀行为[J]. 金属学报, 2013, 49(6): 717-724.
[9] 张金龙,谢兴飞,姚美意,周邦新,彭剑超,梁雪. Zr-1Nb-0.7Sn-0.03Fe-xGe合金在360 ℃ LiOH水溶液中耐腐蚀性能的研究[J]. 金属学报, 2013, 29(4): 443-450.
[10] 牛云松,魏杰,赵健,胡家秀,于志明. 超声辅助电镀法纳米叠层Ni镀膜的制备与性能[J]. 金属学报, 2013, 49(12): 1617-1622.
[11] 朱莉,姚美意,孙国成,陈文觉,张金龙,周邦新. 添加Bi对Zr-1Nb合金在360 ℃和18.6 MPa去离子水中耐腐蚀性能的影响[J]. 金属学报, 2013, 49(1): 51-57.
[12] 姚美意 邹玲红 谢兴飞 张金龙 彭剑超 周邦新. 添加Bi对Zr-4合金在400 ℃/10.3 MPa过热蒸汽中耐腐蚀性能的影响[J]. 金属学报, 2012, 48(9): 1097-1102.
[13] 孙国成 周邦新 姚美意 谢世敬 李强. 锆合金在LiOH水溶液中腐蚀的各向异性研究[J]. 金属学报, 2012, 48(9): 1103-1108.
[14] 莫云飞 刘让苏 梁永超 郑乃超 周丽丽 田泽安 彭平. ZnxAl100-x合金快凝过程中微结构演变特性的分子动力学模拟[J]. 金属学报, 2012, 48(8): 907-914.
[15] 王艳秋,邵亚薇,孟国哲,张涛,王福会. Cu-Ni合金BTA复配体系钝化处理工艺研究[J]. 金属学报, 2012, 48(6): 744-748.